Effect of rare earth elements on high temperature oxidation behaviour of austenitic steel
Source abstract
Abstract
Abstract The oxidation behaviour of K-52 austenitic steel with rare earth elements investigated at 1000 °C for up to 150 h. The oxidation kinetics indicated that the addition of the rare earth elements Y or Ce improved the oxidation resistance of steel. However, the simultaneous addition of Y and Ce decreased the oxidation resistance. The oxidation films forming at different stages were evaluated in detail using surface analysis methods. The improved oxidation resistance primarily resulted from the formation of a complete spinel structure, the inner oxidation of silicon and the existence of MnO2 in the Mn-rich zone.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Semiconductor materials and devices · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Improvement of high-temperature oxidation resistance and strength in alumina-forming austenitic stainless steels10.1016/j.matlet.2011.07.021 ↗
2. Failure analysis of radiant tube burners in continuous annealing line (CAL) of an integrated steel plant10.1007/s11668-010-9426-8 ↗
3. Hot deformation behavior and microstructural evolution of alumina-forming austenitic heat-resistant steels during hot compression10.1016/j.matchar.2016.11.038 ↗
4. High-temperature creep behavior and microstructural evolution of an 18Cr9Ni3CuNbVN austenitic stainless steel10.1016/j.matchar.2014.03.012 ↗
5. Oxidation behavior of RE-modified nickel-based superalloy between 952℃ and 1150℃ in air10.1016/S1003-6326(16)64215-2 ↗
6. Oxidation kinetics and oxide scale characterization of nickel-based superalloy IN738LC at 900°C10.1007/s11665-017-2954-6 ↗
7. Early oxidation mechanism of austenitic stainless steel TP347H in supercritical water10.1016/j.corsci.2017.09.023 ↗
8. Corrosion of ferritic–martensitic steels in steam and supercritical water10.1016/j.jnucmat.2012.09.037 ↗
9. Oxidation behavior of ferritic-martensitic steel P92 exposed to supercritical water at 600℃/25 MPa
10. Study of the corrosion behavior of a 18Cr-oxide dispersion strengthened steel in supercritical water10.1016/j.corsci.2012.08.021 ↗
11. Cause analysis of the oxide scale formed in furnace for W470 steel
12. Influence of dissolved oxygen concentration on the oxide film formed on 304 stainless steel in high temperature water10.1016/j.corsci.2012.06.007 ↗
13. Improved creep behavior of a high nitrogen Nb-Stabilized 15Cr-15Ni austenitic stainless steel strengthened by multiple nanoprecipitates10.1007/s11661-011-0752-6 ↗
14. Coatings and surface treatments for high temperature oxidation resistance
15. High temperature oxidation resistance of plasma sprayed and surface treated YSZ coating on Hastelloy X10.1016/j.surfcoat.2017.05.002 ↗
16. Microstructure and high temperature oxidation resistance of in-situ synthesized TiN/Ti3Al intermetallic composite coatings on Ti6Al4V alloy by laser cladding process10.1016/j.jallcom.2015.10.168 ↗
17. High temperature oxidation behavior of a high Al-containing ferritic heat-resistant stainless steel10.1016/j.matchar.2017.11.038 ↗
18. High temperature cyclic oxidation behavior of ferritic stainless steel with addition of alloying elements Nb and Ti for use in SOFCs interconnect10.1016/j.ijhydene.2016.01.090 ↗
19. High temperature oxidation resistance of aluminum-containing austenitic heat-resisting steel
20. Improved crack healing and high‐temperature oxidation resistance of Ni/Al2O3 by Y or Si doping10.1111/jace.14252 ↗
21. Effects of rare earth metals addition on the resistance to pitting corrosion of super duplex stainless steel-Part 110.1016/j.corsci.2010.02.043 ↗
22. Effect of the rare earth treatment on pitting corrosion behavior of Mn-V-Ti-steel
23. Effects of water vapor on oxidation behavior of ferritic stainless steels under solid oxide fuel cell interconnect exposure conditions10.1016/j.ssi.2005.03.019 ↗
24. Characteristics of oxide scale formed on ferritic stainless steels in simulated reheating atmosphere10.1016/j.surfcoat.2014.09.019 ↗
25. Aging of a cast 35Cr–45Ni heat resistant alloy10.1016/j.matchemphys.2012.02.010 ↗
26. Research on the oxidation behavior of novel γ/γ’-strengthened Co-9Al-10W alloys combined with chromium and rare earth elements10.1557/jmr.2016.345 ↗
27. Effect of Ce addition on the precipitation of deleterious phases and the associated intergranular corrosion resistance of 27Cr–7Ni hyper duplex stainless steels10.1016/j.corsci.2014.10.018 ↗
28. Thermodynamics of the oxidation of rare earth oxysulfides at high temperatures10.1007/BF02657383 ↗
29. Characterization of Ni-25 wt.% Cr alloys containing reactive elements and the oxide scales grown on them at high temperatures using transmission electron microscopy10.1007/BF01046892 ↗
30. High temperature thermodynamics and applications of rare earth oxides and sulphides in ferrous metallurgy10.1080/08827509208914093 ↗
31. Corrosion of austenitic alloys in supercritical water
32. Oxidation behavior of ferritic-martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
33. Study of the corrosion behavior of a 18Cr-oxide dispersion strengthened steel in supercritical water10.1016/j.corsci.2012.08.021 ↗
34. Corrosion of ferritic-martensitic steels in steam and supercritical water10.1016/j.jnucmat.2012.09.037 ↗
35. Young · 2008 · 16
36. Parabolic laws during high temperature oxidation: relations with the grain size and thickness of the oxide10.1023/A:1006677631548 ↗
37. High temperature oxidation behavior of ferritic stanless ateel containing W and Ce10.1016/j.corsci.2018.07.017 ↗
38. Effects of Mn and Mo addition on high-temperature tensile properties in high-Ni-containing austenitic cast steels used for turbo-charger application
39. Study on high temperature oxidation resistance of RE modified HP40 superalloy
40. High temperature oxidation behavior of Cr-Mn-Fe-Co-Ni high entropy alloy10.1016/j.intermet.2018.04.006 ↗
41. Effect of yttrium on the oxide scale adherence of pre-oxidized silicon-containing heat-resistant alloy10.1016/j.corsci.2011.07.002 ↗
42. Effects of yttrium on the oxidation behavior of low sulfur content Fe-Cr-Al alloys for heat resistant wires10.1007/s11085-013-9403-1 ↗
43. Effect of yttrium on the cyclic oxidation behaviour of HP40 heat-resistant steel at 1373 K10.1016/j.corsci.2010.09.039 ↗
44. Stress corrosion cracking of austenitic alloys in supercritical water
45. Self-diffusion in austenitic Fe-Cr-Ni alloys10.1088/0305-4608/10/3/009 ↗
46. The anodic dissolution and passivation of NiCrFe alloys studied by ESCA10.1016/0010-938X(92)90113-H ↗
47. On the oxide formation on stainless steels AlSi 304 and incoloy 800H investigated with XPS10.1016/0169-4332(87)90062-6 ↗
48. Oxidation of stainless steel 316 and nitronic 50 in supercritical and ultrasupercritical water10.1016/j.apsusc.2015.03.127 ↗
49. Investigation of a passive film on an iron chromium alloy by AES and XPS10.1002/sia.740110403 ↗
50. A study of a number of mixed transition metal oxide spinels using X-ray photoelectron spectroscopy10.1016/0169-4332(89)90977-X ↗
51. Birks · 2006
52. Effect of reactive elements Y and Ce on high temperature oxidation of Fe-25Cr-40Ni alloy
53. Microstructure evolution during service exposure of two cast, heat-resisting stainless steels-HP-Nb modified and 20-32 Nb10.1016/j.matchar.2007.08.029 ↗
54. Microstructure of HK40 alloy after high temperature service in oxidizing/carburizing environment : I. Oxidation phenomena and propagation of a crack10.1016/S1044-5803(02)00249-8 ↗