journal article·2016-10

Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon dioxide environments

Ho Jung Lee, Gokul Obulan Subramanian, Sung Hwan Kim, Changheui Jang

Corrosion Science· Volume 111
Publisher page

Abstract

Abstract Chromia-forming heat-resistant alloys were corroded in atmospheric CO2 (0.1 MPa) and supercritical-CO2 (S-CO2, 10 and 20 MPa) at 550–650 °C for 1000 h. The weight gain and the extent of an amorphous C layer at the oxide/matrix interface increased with increasing CO2 pressure from 0.1 MPa to 20 MPa, but the increase was mostly less than a factor of 2. Despite the huge difference in the test pressure, the depth of the carburized region with Cr-rich carbides was rarely affected for Alloy 800HT, resulting in similar tensile properties after corrosion in CO2 and S-CO2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. V. Dostal, M.J. Driscoll, P. Hejzlar, A supercritical carbon dioxide cycle for next generation nuclear reactors, MIT Annual and Progress Reports MIT-ANP-TR-100, 2004, p. 307.
2. Review of supercritical CO2 power cycle technology and current status of research and development10.1016/j.net.2015.06.009 ↗
3. Tutorial: fundamentals of supercritical CO2
4. R. Moore, T. Conboy, Metal Corrosion in a Supercritical Carbon Dioxide-Liquid Sodium Power, Cycle Sandia National Laboratories Report SAND2012-0184, 2012, p. 49.10.2172/1039408 ↗
5. Wastage and self-plugging by a potential CO2 ingress in a supercritical CO2 power conversion system of an SFR10.1080/18811248.2010.9711667 ↗
6. Corrosion of 9Cr steel in CO2 at intermediate temperature II: mechanism of carburization10.1007/s11085-011-9272-4 ↗
7. Effect of CO2 on the strength and ductility of type 304 stainless steel at elevated temperatures10.5006/0010-9312-19.5.157 ↗
8. Type 304 stainless steel vs flowing CO2 at atmospheric pressure and 1100–1800F10.5006/0010-9312-21.3.84 ↗
9. Factors in the oxidation assessment of AISI type 310 steels in high pressure carbon dioxide10.1016/0010-938X(82)90129-9 ↗
10. Behaviour of carbon during the corrosion of stainless steel by carbon dioxide10.1016/0010-938X(67)80039-8 ↗
11. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
12. Corrosion and carburization behavior of chromia-forming heat resistant alloys in high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
13. H.J. Lee, S.H. Kim, H. Kim, C. Jang, Corrosion and carburization behavior of Al-rich surface layer on Ni-base alloy in supercritical-carbon dioxide environment, Applied Surface Science, 2016, in press.10.1016/j.apsusc.2015.11.162 ↗
14. Initial assessment of Ni-base alloy performance in 0.1MPa and supercritical CO210.1007/s11837-015-1661-8 ↗
15. Compatibility of FBR structural materials with supercritical carbon dioxide10.1016/j.pnucene.2011.04.030 ↗
16. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
17. Corrosion of various engineering alloys in supercritical carbon dioxide
18. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
19. Corrosion of a stainless steel and nickel-based alloys in high temperature supercritical carbon dioxide environment10.1016/j.corsci.2012.11.041 ↗
20. Oxidation of alloys for energy applications in supercritical CO2 and H2O10.1016/j.corsci.2016.03.018 ↗
21. Corrosion of 9–12Cr ferritic-martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
22. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
23. Alloys SS316 and Hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
24. Corrosion resistance of PM2000 ODS steel in high temperature supercritical carbon dioxide10.1002/maco.201307223 ↗
25. The role of aluminum and titanium on the oxidation process of a nickel-base superalloy in steam at 800°C10.1007/BF00656727 ↗
26. High temperature oxidation behaviors of Alloy 617 and Haynes 230 in impure helium environments10.1007/s11085-010-9223-5 ↗
27. K. Sridharan, Corrosion in supercritical carbon dioxide: materials environmental purity, surface treatments, and flow issues, Final report for project of nuclear energy university program, 10–872 2013–872, 2013, p. 300.10.2172/1111547 ↗
28. Technology needs for fossil fuel supercritical CO2 power systems
29. Materials performance in supercritical CO2 in comparison with supercritical steam and atmospheric pressure CO2
30. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
31. Hydrogen effects on oxidation behaviors of Haynes 230 in high temperature steam environments10.1016/j.ssi.2013.04.010 ↗
32. A study on the solubility and distribution of carbon in oxides10.1016/0038-1098(85)91021-X ↗
33. A quantitative demonstration of the grain boundary diffusion mechanism for the oxidation of metals10.1080/01418618208239905 ↗
34. Carbon transport through oxide scales on Fe-Cr alloys10.1007/BF00751801 ↗
35. Non-steady state carburization of martensitic 9–12%Cr steels in CO2 rich gases at 550°C10.1016/j.corsci.2014.07.024 ↗
36. Thermodynamics of the fcc Fe-Ni-C and Ni-C alloys10.1007/BF02917551 ↗
37. Diffusion coefficient of carbon in Fe-Ni austenite in the temperature range 950–1100°C
38. The effect of temperature and pressure on supercritical CO2 compatibility of conventional structural alloys