Correlation of surface Volta potential with galvanic corrosion initiation sites in solid-state welded Ti-Cu bimetal using AFM-SKPFM
Source abstract
Abstract
Abstract This study aims to correlate the microstructure and Volta potential distribution of Ti-Cu welded bimetal to its corrosion initiation sites, using AFM-SKPFM, and SEM-EDS. Local melted zones with Ti-Cu intermetallic precipitates in weld interface and in Cu matrix showed different Volta potential values in comparison with those of Ti and Cu regions. SKPFM revealed that Cu region has a higher Volta potential than that of Ti region. AFM and microstructural images after immersion in corrosive media proved the presence of a galvanic cell. Corrosion mainly extends on Cu side due to the increasing growth of Ti passive film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Influence of electron-beam superposition welding on intermetallic layer of Cu/Ti joint10.1016/S1003-6326(11)61479-9 ↗
2. Interfacial characterization and mechanical property of Ti/Cu clad sheet produced by explosive welding and annealing10.1007/s11595-015-1295-2 ↗
3. Microstructural and mechanical properties of Cu–Ti plates bonded through explosive welding process10.1016/j.jmatprotec.2005.02.264 ↗
4. Corrosion and microstructural aspects of dissimilar joints of titanium and type 304L stainless steel10.1016/S0022-3115(03)00194-6 ↗
5. Recent developments in explosive welding10.1016/j.matdes.2010.10.017 ↗
6. Texture transformations near the bonding zones of the three-layer Al/Ti/Al explosively welded clads10.1016/j.matchar.2017.05.007 ↗
7. Microstructure and electrical conductivity of aluminium/steel bimetallic rods processed by severe plastic deformation10.1007/s10853-016-9973-9 ↗
8. A new concept of universal substitutive explosive welding10.1016/j.matdes.2016.11.053 ↗
9. High cooling rates and metastable phases at the interfaces of explosively welded materials10.1016/j.actamat.2017.06.038 ↗
10. Growth kinetics of TiAl 3 phase in annealed Al/Ti/Al explosively welded clads10.1016/j.matlet.2017.04.025 ↗
11. Investigation of cold rolling influence on the mechanical properties of explosive-welded Al/Cu bimetal10.1016/j.msea.2012.07.102 ↗
12. Experimental and numerical analysis of the formation behavior of intermediate layers at explosive welded Al/Fe joint interfaces10.1016/j.jmapro.2016.08.002 ↗
13. Formation of intermetallic compounds during explosive welding10.1007/s11661-016-3729-7 ↗
14. The investigate metallurgical properties of roll bonding titanium clad steel10.7763/IJAPM.2011.V1.34 ↗
15. Evaluation of transient liquid phase bonding between titanium and steel10.1002/adem.200900021 ↗
16. Weldability window and the effect of interface morphology on the properties of Al/Cu/Al laminated composites fabricated by explosive welding10.1016/j.matdes.2015.07.114 ↗
17. Microstructure and property inhomogeneity investigations of bonded Zr/Ti/steel trimetallic sheet fabricated by explosive welding10.1016/j.jallcom.2016.12.213 ↗
18. Effect of alloying elements on interdiffusion phenomena in explosive clads of 304LSS/Ti–5Ta–2Nb alloy10.1007/s10853-016-9832-8 ↗
19. Microstructural and microanalysis investigations of bond titanium grade1/low alloy steel st52-3N obtained by explosive welding10.1016/j.jallcom.2016.02.120 ↗
20. Galvanic corrosion associated with SM 80SS steel and Ni-based alloy G3 couples in NaCl solution10.1016/j.electacta.2008.04.029 ↗
21. Galvanic corrosion of laser weldments of AA6061 aluminium alloy10.1016/j.corsci.2007.04.010 ↗
22. Galvanic corrosion behavior of copper/titanium galvanic couple in artificial seawater10.1016/S1003-6326(14)63097-1 ↗
23. Effect of near-ambient temperature changes on the galvanic corrosion of an AA2024-T3 and mild steel couple10.1149/2.0551501jes ↗
24. The effect of annealing on the interface microstructure and mechanical characteristics of AZ31B/AA6061 composite plates fabricated by explosive welding10.1016/j.matdes.2014.08.025 ↗
25. Effect of explosive mixture on quality of explosive welds of copper to aluminium10.1016/j.matdes.2016.01.116 ↗
26. Simulation of galvanic corrosion of magnesium coupled to a steel fastener in NaCl solution10.1002/maco.200403855 ↗
27. Friction stir welded AM50 and AZ31 Mg alloys: microstructural evolution and improved corrosion resistance10.1016/j.matchar.2017.02.018 ↗
28. Microstructure and corrosion characterization of the interfacial region in dissimilar friction stir welded AA5083 to AA702310.1016/j.corsci.2016.02.027 ↗
29. Microgalvanic corrosion behavior of Cu-Ag active braze alloys investigated with SKPFM10.3390/met6040091 ↗
30. The localised corrosion associated with individual second phase particles in AA7075‐T6: a study by SEM, EDX, AES, SKPFM and FIB‐SEM10.1002/maco.201609312 ↗
31. In situ detection of differences in the electrochemical activity of Al 2 Cu IMPs and investigation of their effect on FFC by scanning Kelvin probe force microscopy10.1016/j.corsci.2012.02.006 ↗
32. High-resolution Kelvin probe microscopy in corrosion science: scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
33. The influence of microstructure on the corrosion behaviour of AZ91D studied by scanning Kelvin probe force microscopy and scanning Kelvin probe10.1016/j.corsci.2005.05.008 ↗
34. Characterization of corrosion interfaces by the scanning Kelvin probe force microscopy technique10.1149/1.1359199 ↗
35. Calibration of the scanning Kelvin probe force microscope under controlled environmental conditions10.1016/j.electacta.2012.01.054 ↗
36. Interfacial hydrogen localization in austenite/martensite dual‐phase steel visualized through optimized silver decoration and scanning Kelvin probe force microscopy10.1002/maco.201609104 ↗
37. Micro-galvanic corrosion effects on patterned copper-zinc samples during exposure in humidified air containing formic acid10.1149/2.113308jes ↗
38. Corrosion inhibition of two brass alloys by octadecanethiol in humidified air with formic acid10.5006/1648 ↗
39. Correlative EBSD and SKPFM characterisation of microstructure development to assist determination of corrosion propensity in grade 2205 duplex stainless steel10.1007/s10853-015-9501-3 ↗
40. The role of intermetallic particles in localized corrosion of an aluminum alloy studied by SKPFM and integrated AFM/SECM10.1149/1.2883737 ↗
41. SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel10.1016/j.corsci.2015.06.035 ↗
42. Local electronic properties of the passive film on nickel studied by scanning tunneling spectroscopy10.1149/2.010208jes ↗
43. Electron work functions of ferrite and austenite phases in a duplex stainless steel and their adhesive forces with AFM silicon probe10.1038/srep20660 ↗
44. Effect of hydrogen on semiconductive properties of passive film on ferrite and austenite phases in a duplex stainless steel10.1038/s41598-017-03480-8 ↗
45. Correlation between the histogram and power spectral density analysis of AFM and SKPFM images in an AA7023/AA5083 FSW joint10.1016/j.jallcom.2018.02.106 ↗
46. Corrosion behavior of TiO2/Cu2O coupled oxides in Cl− ion containing solution: Volta potential and electronic properties characterization by scanning probe microscopy10.1016/j.matchemphys.2018.03.066 ↗
47. Surface potential analysis on initial galvanic corrosion of Ti/Mg-Al dissimilar material10.1016/j.matchemphys.2016.05.031 ↗
48. Establishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM–EDS and AFM–SKPFM10.1016/j.corsci.2013.10.039 ↗
49. Ultra-hydrophobicity through stochastic surface roughness10.1163/156856108X370082 ↗
50. Surface roughness and power spectral density study of SHI irradiated ultra-thin gold films10.1016/j.apsusc.2009.08.046 ↗
51. Correlative microstructure analysis and in situ corrosion study of AISI 420 martensitic stainless steel for plastic molding applications10.1149/2.0531704jes ↗
52. Characterization of 475 °C embrittlement of duplex stainless steel microstructure via scanning kelvin probe force microscopy and magnetic force microscopy10.1149/2.0311706jes ↗
53. Characterization of screw dislocation-driven growth in nickel micro-nanostructure electrodeposition process by AFM10.1016/j.matlet.2017.09.057 ↗
54. The effect of explosive welding parameters on metallurgical and mechanical interfacial features of Inconel 625/plain carbon steel bimetal plate10.1016/j.msea.2012.07.012 ↗
55. Hierarchical microstructure of explosive joints: example of titanium to steel cladding10.1016/j.msea.2010.11.092 ↗
56. Examination of copper/stainless steel joints formed by explosive welding10.1016/j.matdes.2004.07.021 ↗
57. Effect of explosive characteristics on the explosive welding of stainless steel to carbon steel in cylindrical configuration10.1016/j.matdes.2013.03.069 ↗
58. The Cu−Ti (copper-titanium) system10.1007/BF02880329 ↗
59. Influence of metal carbides on dissolution behavior of biomedical CoCrMo alloy: SEM, TEM and AFM studies10.1016/j.electacta.2011.08.028 ↗
60. Depletion effects at phase boundaries in 2205 duplex stainless steel characterized with SKPFM and TEM/EDS10.1016/j.corsci.2009.05.012 ↗
61. Corrosion behaviour and galvanic coupling of titanium and welded titanium in LiBr solutions10.1016/j.corsci.2006.07.007 ↗
62. Corrosion mechanisms in titanium oxide-based films produced by anodic treatment10.1016/j.electacta.2017.03.011 ↗
63. The corrosion behavior of copper alloys, stainless steels and titanium in seawater10.1016/0010-938X(94)90008-6 ↗