journal article·2020-02

Chloride- and sulphate-induced hot corrosion mechanism of super austenitic stainless steel S31254 under dry gas environment

Shucai Zhang, Huabing Li, Zhouhua Jiang, Binbin Zhang, Zhixing Li, Jingxi Wu, Hao Feng, Hongchun Zhu, Fei Duan

Corrosion Science· Volume 163
Publisher page

Abstract

Abstract Chloride- and sulphate-induced hot corrosion mechanisms of super austenitic stainless steel S31254 were investigated at 400–1000 °C under dry gas environment. The mixed salts melted with the temperature increasing, gradually deteriorating the corrosion resistance of the steel. Starting at 600 °C, molten chloride salts accelerated corrosion following a two-stage mechanism “electrochemical corrosion + chlorine-active corrosion”. Above 800 °C, molten sulfates dissolved and destroyed corrosion layer via “basic fluxing” mechanism, causing serious internal and intergranular corrosion. Additionally, numerous precipitates formed and promoted element diffusion, further accelerating molten salt corrosion. Jointly deteriorated by molten salts and precipitates, the samples suffered catastrophic corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration environment10.1016/S0010-938X(01)00058-0 ↗
2. Biomass cofiring: the technology, the experience, the combustion consequences10.1016/S0961-9534(00)00049-0 ↗
3. Evaluation of high temperature corrosion in simulated waste incinerator environments10.1007/s11085-016-9615-2 ↗
4. Corrosion of superheater materials in a waste-to-energy plant10.1016/j.fuproc.2011.06.017 ↗
5. Investigation into high-temperature corrosion in a large-scale municipal waste-to-energy plant10.1016/j.corsci.2010.07.032 ↗
6. Ash deposit characterisation in a large-scale municipal waste-to-energy incineration plant10.1016/j.jhazmat.2010.10.095 ↗
7. Albina · 2005
8. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
9. Corrosion in biomass combustion: a materials selection analysis and its interaction with corrosion mechanisms and mitigation strategies10.1016/j.corsci.2013.07.013 ↗
10. Precipitation behavior and phase transformation mechanism of super austenitic stainless steel S32654 during isothermal aging10.1016/j.matchar.2018.01.040 ↗
11. Detection of susceptibility to intergranular corrosion of aged super austenitic stainless steel S32654 by a modified electrochemical potentiokinetic reactivation method10.1016/j.jallcom.2016.11.342 ↗
12. Microstructure evolution and mechanical properties of friction stir welding super-austenitic stainless steel S3265410.1016/j.matdes.2017.01.034 ↗
13. Investigation of microbiologically influenced corrosion of the high nitrogen nickel-free stainless steel by pseudomonas aeruginosa10.1016/j.corsci.2016.06.017 ↗
14. Precipitated phases of superaustenitic stainless steel 654SMO10.1016/S1006-706X(17)30112-7 ↗
15. Applications and experience with a superaustenitic 7Mo stainless steels in hostile environments10.1002/maco.19970481203 ↗
16. High temperature corrosion of superheater tubes in waste incinerators and coal-fired plants10.4028/www.scientific.net/MSF.461-464.973 ↗
17. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700 °C10.1016/S0010-938X(99)00142-0 ↗
18. High temperature corrosion in a 65 MW waste to energy plant10.1016/j.fuproc.2007.06.031 ↗
19. Accelerated corrosion of five commercial steels under a ZnCl2-KCl deposit in a reducing environment typical of waste gasification at 673–773 K10.1016/j.corsci.2008.03.004 ↗
20. KCl induced corrosion of a 304-type austenitic stainless steel at 600 °C; the role of potassium10.1007/s11085-005-5704-3 ↗
21. Are NaCl and KCl equally corrosive on superheater materials of steam boilers?10.1016/j.fuel.2012.07.020 ↗
22. High temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits10.1016/j.corsci.2003.09.026 ↗
23. A microstructural study of the influence of NaCl vapor on the oxidation of a Ni-Cr-Al alloy at 850 °C10.1007/BF00609972 ↗
24. Analysis of material degradation for uncoated and NiCoCrAlY cold spray coated Superfer 800H in the secondary chamber of medical waste incinerator10.1016/j.engfailanal.2014.09.001 ↗
25. Behaviour and mechanisms of alkali-sulphate-induced hot corrosion on composite coatings at 900 °C10.1016/j.corsci.2012.01.034 ↗
26. The influence of sulfides on the oxidation behavior of nickel-base alloys10.1007/BF03037874 ↗
27. Reversible catastrophic oxidation of a 38Fe-34Ni-25Cr alloy induced by sodium sulphate at low oxygen potential atmospheres10.1016/j.corsci.2011.10.010 ↗
28. Hot corrosion mechanism of steels exposed to heavy metal chlorides and sulphates in SO2 environment10.1007/s11085-016-9634-z ↗
29. 2013 · 377
30. Determination of the corrosivity of Pb-containing salt mixtures10.1016/j.corsci.2012.09.024 ↗
31. A comparative study on the high temperature corrosion of TP347H stainless steel, C22 alloy and laser-cladding C22 coating in molten chloride salts10.1016/j.corsci.2014.03.012 ↗
32. Formation of Si diffusion layer on stainless steels and their high temperature corrosion resistance in molten salt10.1016/j.corsci.2011.11.015 ↗
33. Liu · 2017
34. Salt melt induced corrosion of metallic materials in waste incineration plants10.1002/(SICI)1521-4176(199907)50:7<373::AID-MACO373>3.0.CO;2-T ↗
35. Comparison of the high-temperature chloride-induced corrosion between duplex steel and Ni based alloy in presence of H2S10.1016/j.corsci.2018.04.042 ↗
36. High temperature corrosion behaviors of the superheater materials10.1016/j.proeng.2012.03.033 ↗
37. Corrosion behavior of nickel-based superalloys in thermal storage medium of molten eutectic NaCl-MgCl2 in atmosphere10.1016/j.solmat.2017.02.020 ↗
38. Salt induced corrosion behaviour of superalloy IN718
39. Oxidation behavior of αMo-Mo3Si-Mo5SiB2 (T2) three phase system10.1016/S0966-9795(01)00118-2 ↗
40. A new insight into high-temperature oxidation mechanism of superaustenitic stainless steel S32654 in air10.1016/j.jallcom.2016.06.023 ↗
41. Li · 2003
42. Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings10.1016/j.corsci.2017.12.033 ↗
43. The effect of temperature on mechanical properties of oxide scales formed on a carbon steel in a simulated municipal solid waste incineration environment10.1016/j.surfcoat.2013.10.035 ↗
44. High temperature corrosion of metallic materials in simulated waste incineration environments at 300–600 °C10.1002/maco.200503909 ↗
45. Lu · 2012
46. Influence of nitrogen on corrosion behaviour of high nitrogen martensitic stainless steels manufactured by pressurized metallurgy10.1016/j.corsci.2018.09.002 ↗
47. Thermodynamic and kinetic consideration on the corrosion of Fe, Ni and Cr beneath a molten KCl-ZnCl2 mixture10.1016/j.corsci.2005.02.015 ↗
48. Corrosion behavior of Cr, Fe and Ni based superalloy in molten NaCl10.1016/S1875-5372(14)60044-8 ↗
49. A surface analytical approach to the high temperature chlorination behaviour of inconel 600 at 700 °C10.1016/S0010-938X(96)00112-6 ↗
50. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
51. Experimental and thermodynamic investigations on the chlorine-induced corrosion of HVOF thermal sprayed NiAl coatings and 304 stainless steels at 700 °C10.1016/j.corsci.2018.02.047 ↗
52. A microstructural and kinetic investigation of the KCl-induced corrosion of an FeCrAl alloy at 600 °C10.1007/s11085-015-9546-3 ↗
53. Cyclic corrosion and chlorination of an FeCrAl alloy in the presence of KCl10.1007/s11085-015-9554-3 ↗
54. Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: a review10.1007/s11705-018-1720-0 ↗
55. Broström · 2010
56. Knacke · 1991
57. High-temperature corrosion in waste-to-energy boilers10.1007/s11666-006-9005-4 ↗
58. Fundamental aspects of chlorine induced corrosion in power plants10.1179/mht.2003.018 ↗
59. Hot corrosion behavior of porous nickel-based alloys containing molybdenum in the presence of NaCl at 750 °C10.1016/j.engfailanal.2017.05.009 ↗
60. High temperature corrosion behaviour of superalloys under actual waste incinerator environment10.1016/j.engfailanal.2016.02.016 ↗
61. The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750 °C10.1016/j.matchemphys.2004.10.002 ↗
62. Stability of protective oxide films in waste incineration envioronment solubility measurement of oxides in molten chlorides10.1016/S0010-938X(01)00059-2 ↗
63. Hot corrosion behavior and near-surface microstructure of a “low temperature high-activity Cr-aluminide” coating on inconel 738LC exposed to Na2SO4, Na2SO4 + V2O5 and Na2SO4 + V2O5 + NaCl at 900 °C10.1016/j.corsci.2017.09.004 ↗
64. Effect of intergranular precipitation on the internal oxidation behavior of Cr-Mn-N austenitic stainless steels10.1007/s40195-015-0288-7 ↗
65. Oxidation of a Fe-18Cr-8Ni austenitic stainless steel at 850 °C in O2: microstructure evolution during breakaway oxidation10.1016/j.corsci.2016.10.029 ↗
66. Fourlaris, Phase transformations and mechanical properties in heat treated superaustenitic stainless steels10.1016/j.msea.2012.10.066 ↗
67. Catastrophic oxidation mechanism of hyper duplex stainless steel S32707 at high temperature in air10.1016/j.matchar.2018.08.041 ↗
68. Alipour · 2015
69. The effect of co-firing sewage sludge with used wood on the corrosion of an FeCrAl alloy and a nickel-based alloy in the furnace region10.1016/j.fuproc.2015.07.014 ↗