Effects of mechanical and chemical pre-treatments on the morphology and composition of surfaces of aluminium alloys 7075-T6 and 2024-T3
Source abstract
Abstract
Abstract The effects of mechanical and chemical pre-treatments of AA7075-T6 and AA2024-T3 aluminium alloys were studied in terms of changes of morphology, composition and wettability of the surface, and of the related corrosion properties in sodium chloride solution. The mechanical treatments tested include grinding under water and polishing under non-aqueous liquid. The latter preserved the content of Mg at the AA7075-T6 surface. The effect of mechanical treatment was less pronounced on AA2024-T3. The chemical treatments included etching with sodium hydroxide and with a commercial cleaner and desmutting in nitric acid. The sample pre-treatment affects the polarization curves in sodium chloride.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Vargel · 2004
2. Davis · 1999
3. Kufman · 2000
4. Corrosion inhibition of aluminum and aluminum alloys by soluble chromates, chromate coatings, and chromate-free coatings10.5006/1.3277570 ↗
5. An overview of nonhexavalent chromium conversion coatings—Part I: aluminum and its alloys10.1016/S0026-0576(01)81711-6 ↗
6. Review of surface pretreatments for aluminium alloys10.1016/S0143-7496(96)00014-0 ↗
7. Sheasby · 2001
8. Effect of Cu content on corrosion behavior of 7xxx series aluminum alloys10.1149/1.1695385 ↗
9. Corrosion behaviour of mechanically polished AA7075-T6 aluminium alloy10.1002/sia.3136 ↗
10. Transitions between pitting and intergranular corrosion in AA202410.1016/S0013-4686(02)00828-9 ↗
11. Understanding localized corrosion10.1016/S1369-7021(08)70206-2 ↗
12. On the first breakdown in AA7075-T610.1016/j.corsci.2007.02.001 ↗
13. Influence of heat treatment and surface conditioning on filiform corrosion of aluminium alloys AA3005 and AA575410.1016/S0010-938X(01)00019-1 ↗
14. Effect of thermo-mechanical processing on filiform corrosion of aluminium alloy AA300510.1016/S0010-938X(02)00036-7 ↗
15. In situ monitoring of corrosion processes within the bulk of AlMgSi alloys using X-ray microtomography10.1016/j.corsci.2008.09.015 ↗
16. Effect of alkaline cleaning and activation on aluminum alloy 7075-T610.1016/j.apsusc.2010.08.126 ↗
17. Influence of nitric acid pre-treatment on Al–Cu alloys10.1016/j.electacta.2008.01.026 ↗
18. Grilli · 2010
19. Formation of a cerium-based conversion coating on AA2024: relationship with the microstructure10.1016/S0257-8972(03)00743-6 ↗
20. An XPS study of the elemental enrichment on aluminum alloy surfaces from chemical cleaning10.1016/S0257-8972(00)01121-X ↗
21. Behaviour of copper during alkaline corrosion of Al–Cu alloys10.1016/j.corsci.2008.01.021 ↗
22. Influence of pre-treatments in cerium conversion treatment of AA2024-T3 and 7075-T6 alloys10.1016/j.surfcoat.2008.01.027 ↗
23. Effects of different surface cleaning procedures on the superficial morphology and the adhesive strength of epoxy coating on aluminium alloy 105010.1016/j.porgcoat.2015.05.005 ↗
24. Characterization of an effective cleaning procedure for aluminum alloys: surface enhanced Raman spectroscopy and zeta potential analysis10.1016/j.jcis.2004.08.064 ↗
25. Effect of chemical cleaning on the corrosion behaviour of painted aluminium alloys10.1016/S0013-4686(02)00092-0 ↗
26. Characterization of localized surface states of Al 7075-T6 during deposition of cerium-based conversion coatings10.1149/1.3454236 ↗
27. Characterization of cerium-based conversion coatings for corrosion protection of aluminum alloys10.1016/S0257-8972(02)00062-2 ↗
28. Development of cerium-based conversion coatings on 2024-T3 Al alloy after rare-earth desmutting10.1002/sia.1652 ↗
29. Alkaline activation of Al 7075-T6 for deposition of cerium-based conversion coatings10.1016/j.surfcoat.2011.03.073 ↗
30. Effects of acid and alkaline based surface preparations on spray deposited cerium based conversion coatings on Al 2024-T310.1016/j.apsusc.2008.10.110 ↗
31. Surface pretreatments of aluminium for electroplating10.1016/0257-8972(88)90045-X ↗
32. Cerium-based conversion coatings on aluminium alloys: a process review10.1179/1743278213Y.0000000089 ↗
33. Pretreatments of improve the adhesion of electrodeposits on aluminium10.1002/sia.740170720 ↗
34. Characterisation of surface preparation of 2024 aluminium alloy for conversion coating10.1179/mst.1996.12.11.928 ↗
35. Study of deoxidation of 2024-T3 with various acids10.1179/026708301101509728 ↗
36. Corrosion inhibition of pure aluminium and alloys AA2024-T3 and AA7075-T6 by cerium(III) and cerium(IV) salts10.1149/2.0431603jes ↗
37. Cerium chloride and acetate salts as corrosion inhibitors for aluminum alloy AA7075-T6 in sodium chloride solution10.5006/1956 ↗
38. B. Volarič, I. Milošev, Rare eath chloride and nitrate salts as individual and mixed inhibitors for aluminium alloy 7075-T6 in chloride solution, Corr Eng Sci Technol. (n.d.).
39. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
40. An analytical electron microscopy study of constituent particles in commercial 7075-T6 and 2024-T3 alloys10.1007/s11661-998-0240-9 ↗
41. A consistent description of intermetallic particle composition: an analysis of ten batches of AA2024-T310.1002/sia.5207 ↗
42. Sheet AA2024-T3: a new investigation of microstructure and composition10.1002/sia.3163 ↗
43. NIST X-ray Photoelectron Spectroscopy (XPS) Database, Version 3.5, (n.d.). https://srdata.nist.gov/xps/ (Accessed 7 November 2016).
44. Dealloying of Al2CuMg in alkaline media10.1149/1.1393896 ↗
45. Electrochemical behavior of Cu-xZn alloys in borate buffer solution at pH 9.210.1149/1.1615997 ↗
46. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
47. In-situ monitoring of alloy dissolution and residual film formation during the pretreatment of Al-alloy AA2024-T310.1149/2.1121605jes ↗
48. Evidence for Cu ion formation by dissolution and dealloying the Al2CuMg intermetallic compound in rotating ring-disk collection experiments10.1149/1.1393164 ↗