Abstract The long-term corrosion resistance of reinforcing steel embedded in alkali-activated slag (AAS) mortar and ordinary Portland cement (OPC) mortar, when subjected to aggressive marine environments (chloride exposure and atmospheric exposure) for 54 months, was evaluated by electrochemical impedance spectroscopy. Corrosion morphology at the steel-mortar interface, composition of steel corrosion products and microstructure of mortar substrate were also investigated for AAS mortar in different aggressive environments. After long-term atmospheric exposure, AAS mortar provided unexpectedly lower corrosion resistance for steel compared with that for chloride exposure, which can be further evidenced by interfacial morphology and composition of steel corrosion products.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Recent progress in low-carbon binders10.1016/j.cemconres.2019.05.009 ↗
2. Durability and microstructure properties of low-carbon concrete incorporating ferronickel slag sand and fly ash10.1061/(ASCE)MT.1943-5533.0002797 ↗
3. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
4. Chloride-induced corrosion of steel rebars in simulated pore solutions of alkali-activated concretes10.1016/j.cemconres.2017.08.006 ↗
5. Chloride-initiated corrosion in alkali activated reinforced concrete10.1016/j.cemconcomp.2020.103823 ↗
6. Calcined clay limestone cements (LC3)10.1016/j.cemconres.2017.08.017 ↗
7. The role of limestone and calcined clay on the rheological properties of LC310.1016/j.cemconcomp.2020.103516 ↗
8. Corrosion resistance of steel embedded in sulfoaluminate-based binders10.1016/j.cemconcomp.2018.01.014 ↗
9. Shrinkage and creep of high-performance concrete based on calcium sulfoaluminate cement10.1016/j.cemconcomp.2019.02.006 ↗
10. On the intrinsic passivating ability of Belite-Ye’elimite-Ferrite towards carbon steel: A straightforward comparison with ordinary Portland cement10.1016/j.corsci.2018.11.012 ↗
11. A comparative study of mild steel passivation embedded in Belite-Ye’elimite-Ferrite and Porland cement mortars10.1016/j.electacta.2017.12.128 ↗
12. Geopolymers and other alkali activated materials: why, how, and what?10.1617/s11527-013-0211-5 ↗
13. Characterization of the passive film formed on the reinforcement surface in alkali activated fly ash: surface analysis and electrochemical evaluation10.1016/j.corsci.2019.108393 ↗
14. Electrochemical behaviour of a novel alloy steel in alkali-activated slag mortars10.1016/j.cemconcomp.2018.06.004 ↗
15. Chloride‐induced steel corrosion in alkali‐activated fly ash mortar: increased propensity for corrosion initiation at defects10.1002/maco.202011541 ↗
16. Corrosion resistance of steel reinforcements embedded in alkali activated ground granulated SiMn slag mortars10.1016/j.conbuildmat.2019.116917 ↗
17. Passivity of embedded reinforcement in carbonated low-calcium fly ash-based geopolymer concrete10.1016/j.cemconcomp.2017.10.001 ↗
18. Passivation and chloride-induced corrosion of a duplex alloy steel in alkali-activated slag extract solutions10.1016/j.conbuildmat.2017.08.117 ↗
19. Passivation and corrosion behavior of 2304 duplex stainless steel in alkali-activated slag materials10.1016/j.cemconcomp.2020.103532 ↗
20. Free and bound chloride relationships affecting reinforcement cover in alkali activated concrete10.1016/j.cemconcomp.2020.103692 ↗
21. Chloride diffusion resistance and chloride binding capacity of fly ash-based geopolymer concrete10.1016/j.cemconcomp.2019.04.006 ↗
22. Chloride transport and the resulting corrosion of steel bars in alkali activated slag concretes10.1617/s11527-015-0747-7 ↗
23. Influence of SAP on the chloride penetration and corrosion behavior of steel bar in concrete10.1016/j.corsci.2020.108714 ↗
24. Rebar corrosion in coral aggregate concrete: determination of chloride threshold by LPR10.1016/j.corsci.2019.108238 ↗
25. The mechanism controlling corrosion of steel in carbonated cementitious materials in wetting and drying exposure10.1016/j.cemconcomp.2020.103717 ↗
26. Effect of activator types and concentration of CO2 on the steel corrosion in the carbonated alkali-activated slag concrete10.1016/j.conbuildmat.2020.120044 ↗
27. Carbonation-induced and chloride-induced corrosion in reinforced concrete structures10.1061/(ASCE)MT.1943-5533.0001209 ↗
28. Electrochemical and semiconducting properties of passive films on steel surfaces in alkali-activated slag extraction solution10.1061/(ASCE)MT.1943-5533.0002352 ↗
29. Corrosion behavior of steel bars immersed in simulated pore solutions of alkali-activated slag mortar10.1016/j.conbuildmat.2017.03.132 ↗
30. Electrochemical performance of reinforcing steel in alkali-activated slag extract in the presence of chlorides10.1016/j.corsci.2018.01.043 ↗
31. Alkali activated slag mortars provide high resistance to chloride-induced corrosion of steel10.3389/fmats.2018.00034 ↗
32. The interfacial transition zone in alkali-activated slag mortars10.3389/fmats.2015.00070 ↗
33. Corrosion behaviour of low-carbon steel reinforcement in alkali-activated slag-steel slag and Portland cement-based mortars under simulated marine environment10.1016/j.corsci.2020.108874 ↗
34. A study on the corrosion of reinforcing bars in alkali-activated fly ash mortars under wet and dry exposures to chloride solutions10.1016/j.cemconres.2016.05.010 ↗
35. Steel corrosion behaviour in carbonated alkali-activated slag concrete10.1016/j.corsci.2009.05.033 ↗
36. Corrosion of steel bars induced by accelerated carbonation in low and high calcium fly ash geopolymer concretes10.1016/j.conbuildmat.2014.03.015 ↗
37. Corrosion behaviour of bare and galvanized steel in geopolymer and Ordinary Portland Cement based mortars with the same strength class exposed to chlorides10.1016/j.corsci.2018.02.014 ↗
38. Distinctive microstructural features of aged sodium silicate-activated slag concretes10.1016/j.cemconres.2014.07.008 ↗
39. Influence of slag composition on the stability of steel in alkali-activated cementitious materials10.1007/s10853-017-1919-3 ↗
40. Degradation effect of carbonation on electrochemical behavior of 2304 duplex stainless steel in simulated concrete pore solutions10.1016/j.corsci.2020.109006 ↗
41. Corrosion behavior of low-Cr steel rebars in alkaline solutions with different pH in the presence of chlorides10.1016/j.jelechem.2017.09.016 ↗
42. Improved corrosion resistance of a new 6% Cr steel in simulated concrete pore solution contaminated by chlorides10.1016/j.corsci.2020.108851 ↗
43. Impedance study on calcium nitrite as a penetrating corrosion inhibitor for steel in concrete10.1016/j.electacta.2011.01.069 ↗
44. The electrochemical behaviour of stainless steel AISI 304 in alkaline solutions with different pH in the presence of chlorides10.1016/j.electacta.2011.02.094 ↗
45. Electrochemical polarization and impedance of reinforced concrete and hybrid fiber-reinforced concrete under cracked matrix conditions10.1016/j.electacta.2018.03.134 ↗
46. Distribution of corrosion products at the steel-concrete interface: influence of mill scale properties, reinforcing steel type and corrosion inducing method10.1016/j.conbuildmat.2019.116854 ↗
47. Electrochemical behavior and corrosion products of Cr-modified reinforcing steels in saturated Ca(OH)2 solution with chlorides10.1016/j.cemconcomp.2020.103587 ↗
48. The passive behaviour of AISI 316 in alkaline media and the effect of pH: A combined electrochemical and analytical study10.1016/j.electacta.2009.10.026 ↗
49. Effect of cold deformation on the corrosion behaviour of UNS S31803 duplex stainless steel in simulated concrete pore solution10.1016/j.corsci.2017.05.021 ↗
50. Cr-modified low alloy steel reinforcement embedded in mortar for two years: corrosion result of marine field test10.1016/j.cemconcomp.2018.12.019 ↗
51. Enhanced corrosion resistance of reinforcing steels in simulated concrete pore solution with low molybdate to chloride ratios10.1016/j.cemconcomp.2020.103589 ↗
52. Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in Maldives10.1016/j.corsci.2019.108416 ↗
53. Quantitative characterisation of steel/cement paste interface microstructure and corrosion phenomena in mortars suffering from chloride attack10.1016/j.corsci.2006.03.003 ↗
54. Pore structure of hardened cement paste containing colloidal polymers with varied glass transition temperature and surface charges10.1016/j.cemconcomp.2018.11.001 ↗
55. Mechanistic study on initial passivation and surface chemistry of steel bars in nano-silica cement pastes10.1016/j.cemconcomp.2020.103661 ↗
56. Uptake of chloride and carbonate by Mg-Al and Ca-Al layered double hydroxides in simulated pore solutions of alkali-activated slag cement10.1016/j.cemconres.2017.05.015 ↗
57. Chloride diffusivity, chloride threshold, and corrosion initiation in reinforced alkali-activated mortars: role of calcium, alkali, and silicate content10.1016/j.cemconres.2018.06.009 ↗
58. Influence of defects at the steel-mortar interface on the corrosion behavior of steel10.1016/j.conbuildmat.2017.01.007 ↗
59. The effect of the steel–concrete interface on chloride-induced corrosion initiation in concrete: a critical review by RILEM TC 262-SCI10.1617/s11527-019-1387-0 ↗
60. Corrosion initiation of reinforced concretes based on Portland or GGBS cements: chloride contents and electrochemical characterizations versus time10.1016/j.cemconres.2012.07.004 ↗
61. Influence of nitrate corrosion inhibitors on phase stability of alkali-activated slag against chloride binding and natural carbonation10.1061/(ASCE)MT.1943-5533.0002830 ↗
62. Compressive strength, pore structure and chloride transport properties of alkali-activated slag/fly ash mortars10.1016/j.cemconcomp.2019.103392 ↗
63. Pore solution composition and alkali diffusion in inorganic polymer cement10.1016/j.cemconres.2010.04.008 ↗
64. Reinforcement corrosion in marine concretes - 2. long-term effects
65. Microstructural changes in alkali-activated slag mortars induced by accelerated carbonation10.1016/j.cemconres.2017.07.008 ↗
66. Carbonation of low-alkalinity mortars: Influence on corrosion of steel and on mortar microstructure10.1016/j.cemconres.2017.08.013 ↗
67. Drying shrinkage in alkali-activated binders - A critical review10.1016/j.conbuildmat.2018.09.125 ↗
68. Understanding the drying shrinkage performance of alkali-activated slag mortars10.1016/j.cemconcomp.2016.11.010 ↗
69. Impact of atmospheric marine environment on cementitious materials10.1016/j.corsci.2018.12.021 ↗