journal article·2015-05

Low cycle fatigue behavior of a modified 9Cr–1Mo ferritic–martensitic steel in lead–bismuth eutectic at 350°C – Effects of oxygen concentration in the liquid metal and strain rate

Xing Gong, Pierre Marmy, Bert Verlinden, Martine Wevers, Marc Seefeldt

Corrosion Science· Volume 94
Publisher page

Abstract

Abstract The synergistic effects of oxygen concentration and strain rate on the low cycle fatigue behavior of a 9Cr–1Mo steel have been investigated in lead–bismuth eutectic (LBE) at 350 °C. The results showed substantial fatigue life reduction due to liquid metal embrittlement (LME), compared to vacuum. Nevertheless, no evident life degradation was observed under a combination of low strain amplitude, high oxygen concentration in LBE and slow strain rate. This is because fatigue crack initiation was delayed by surface oxide films, rather than because LME disappeared. Fatigue crack propagation remained unaffected by oxygen concentration. A new LME mechanism is proposed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
2. Structural materials for Gen-IV nuclear reactors: challenges and opportunities10.1016/j.jnucmat.2008.08.044 ↗
3. Multi-purpose hYbrid Research Reactor for High-tech Applications a multipurpose fast spectrum research reactor10.1002/er.1891 ↗
4. D. De Bruyn, H. Aït Abderrahim, P. Baeten, R. Fernandez, G. Van den Eynde, Recent design developments of the MYRRHA ADS project in Belgium, in: ICAPP13 – 2013 International Congress on Advances in Nuclear Power Plants, Jeju, Korea, 14–18 April 2013, Korean Nuclear Society.
5. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
6. Long term corrosion on T91 and AISI 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
7. Liquid metal embrittlement susceptibility of T91 steel by lead–bismuth10.1016/j.scriptamat.2005.02.027 ↗
8. Low cycle fatigue behavior of T91 martensitic steel at 300°C in air and in liquid lead bismuth eutectic10.1016/j.ijfatigue.2005.11.003 ↗
9. Investigation of the effect of lead–bismuth eutectic on the fracture properties of T91 and 316L10.1016/j.jnucmat.2009.10.021 ↗
10. On the kinetics of LME for the ferritic–martensitic steel T91 immersed in liquid PbBi eutectic10.1016/j.jnucmat.2011.03.044 ↗
11. Slow strain rate tensile tests on T91 in static lead–bismuth eutectic10.1016/j.jnucmat.2006.05.039 ↗
12. Fracture toughness assessment of ferritic–martensitic steel in liquid lead–bismuth eutectic10.1016/j.jnucmat.2008.11.024 ↗
13. Liquid Pb–Bi embrittlement effects on the T91 steel after different heat treatments10.1016/j.jnucmat.2008.02.050 ↗
14. Liquid metal embrittlement of the T91 steel in lead bismuth eutectic: the role of loading rate and of the oxygen content in the liquid metal10.1016/j.msea.2014.04.082 ↗
15. J. Lim, Thermodynamic Assessment of the Oxygen Control Boundary for the Operation of MYRRHA, 2011, SCK⋅CEN internal report.
16. Influence of PbBi environment on the low-cycle fatigue behavior of SNS target container materials10.1016/S0022-3115(03)00015-1 ↗
17. Low cycle fatigue tests of surface modified T91 steel in 10−6wt% oxygen containing Pb45Bi55 at 550°C10.1016/j.jnucmat.2008.02.075 ↗
18. F. Gnecco, D. Giuranno, E. Ricci, Wettability of T91 steel by Pb and Pb–Bi eutectic alloy, 2002, CNR-IENI report, Genoa.
19. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
20. Oxidation mechanism of an Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy at 470°C (Part II)10.1016/j.corsci.2008.06.051 ↗
21. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
22. LIMETS 3, a novel system for high strain fatigue testing in lead–bismuth eutectic10.1016/j.jnucmat.2013.10.064 ↗
23. Accuracy of potentiometric oxygen sensors with Bi/Bi2O3 reference electrode for use in liquid LBE10.1016/j.jnucmat.2012.06.011 ↗
24. Synergy effect of LBE and hydrogenated helium on resistance to LME of T91 steel grade10.1016/S0022-3115(03)00081-3 ↗
25. The exponential law of endurance tests
26. Fatigue: a complex subject – some simple approximation10.1007/BF02321056 ↗
27. A study of the effect of cyclic thermal stresses on a ductile metal
28. Crack propagation in a liquid metal environment10.1016/0001-6160(63)90180-9 ↗
29. Concerning liquid metal embrittlement, particularly of zinc monocrystals by mercury10.1080/14786436308213836 ↗
30. Effect of liquid metal embrittlement on low cycle fatigue properties and fatigue crack propagation behavior of a modified 9Cr–1Mo ferritic–martensitic steel in an oxygen-controlled lead–bismuth eutectic environment at 350°C10.1016/j.msea.2014.09.003 ↗
31. Influence of liquid lead and lead–bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
32. Multiplication processes for slow moving dislocations10.1103/PhysRev.79.722 ↗
33. Krupp · 2007
34. Plastic strain localization in metals: origins and consequences10.1016/j.pmatsci.2013.06.001 ↗
35. The mechanisms of crack initiation and crack propagation in metal-induced embrittlement of metals10.1007/BF02643354 ↗