Corrosion behaviour and mechanism of new aerospace Al–Zn–Mg alloy friction stir welded joints and the effects of secondary Al 3 Sc x Zr 1− x nanoparticles

Ying Deng, Rui Ye, Guofu Xu, Jidong Yang, Qinglin Pan, Bing Peng, Xiaowu Cao, Yulu Duan, Yingjun Wang, Liying Lu, Zhimin Yin

Corrosion Science· Volume 90
Publisher page

Abstract

Abstract Corrosion behaviour, residual stress, intermetallics and microstructure of friction stir welded aerospace Al–Zn–Mg and Al–Zn–Mg–0.10Sc–0.10Zr (wt.%) alloys were investigated comparatively and in detail. The thermo-mechanically affected zones adjacent to weld nugget are most susceptible to corrosion in two weld joints. In addition to the enrichment of coarse Si and Fe intermetallics, wide precipitate free zones (in Al–Zn–Mg weld joint) and high tensile residual stress are the key factors. Secondary Al3ScxZr1−x nanoparticles can effectively improve stress corrosion cracking resistance and decrease exfoliation corrosion rates of Al–Zn–Mg weld joints by restraining the formation of precipitate free zones and refining grains.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (89)

Show source-provided references
1. W.M. Thomas, E.D. Nicholas, J.C. Needham, M.G. Murch, P. Templesmith, C.J. Dawes, Friction Welding, US 5460317 A, 1991.
2. Corrosion protection of AA7449-T7951 friction stir welds by laser surface melting with an Excimer laser10.1016/j.corsci.2011.07.043 ↗
3. Recent advances in friction-stir welding-process, weldment structure and properties10.1016/j.pmatsci.2008.05.001 ↗
4. Relationship between microstructure, microhardness and corrosion sensitivity of an AA 2024-T3 friction stir welded joint10.1016/j.corsci.2011.05.049 ↗
5. A look in the corrosion of aluminum alloy friction stir welds10.1016/j.scriptamat.2007.10.043 ↗
6. Microstructure, microchemistry and environmental cracking susceptibility of friction stir welded 2219-T8710.1016/j.msea.2006.05.036 ↗
7. In-situ investigation on the pitting corrosion behaviour of friction stir welded joint of AA2024-T3 aluminium alloy10.1016/j.corsci.2009.10.027 ↗
8. Microstructure and pitting corrosion of friction stir welded joints in 2219-O aluminum alloy thick plate10.1016/j.corsci.2009.07.004 ↗
9. Stress corrosion cracking susceptibility of friction stir welded AA7075-AA6056 dissimilar joint10.1016/j.msea.2004.09.065 ↗
10. Corrosion behaviour of friction stir welded10.1016/j.corsci.2005.02.020 ↗
11. Characterisation and understanding of the corrosion behaviour of the nugget in a 2050 aluminum alloy friction stir welding joint10.1016/j.corsci.2013.04.001 ↗
12. The effect of welding parameters on the corrosion behaviour of friction stir welded AA2024-T35110.1016/j.corsci.2006.05.038 ↗
13. Corrosion of friction-stir welded aluminum alloys 2024 and 219510.1023/A:1026710422951 ↗
14. A comparison between FSW and TIG welding techniques: modifications of microstructure and pitting corrosion resistance in AA 2024-T3 butt joints10.1016/j.jmatprotec.2004.03.022 ↗
15. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.electacta.2010.09.023 ↗
16. Effect of grain size on corrosion of high purity aluminium10.1016/j.scriptamat.2010.08.035 ↗
17. Improvement of mechanical properties of 7475 based aluminum alloy sheets by controlled warm rolling10.2320/matertrans.45.69 ↗
18. Effect of grain characteristic on intergranular corrosion resistance of 6061 aluminum alloy extrusion10.1007/s11661-002-0274-3 ↗
19. Grain boundary character distribution and intergranular corrosion behavior in high purity aluminum10.1016/S1359-6462(00)00682-5 ↗
20. Corrosion behaviour of different tempers of AA7075 aluminium alloy10.1016/j.electacta.2004.01.046 ↗
21. Enhanced SCC resistance of AA7005 welds with appropriate filler metal and post-welding heat treatment10.1016/j.tafmec.2010.06.011 ↗
22. Corrosion protection of AA7449-T7951 friction stir welds by laser surface melting with an excimer laser10.1016/j.corsci.2011.07.043 ↗
23. Corrosion susceptibility of peened friction stir welded 7075 aluminum alloy joints10.1016/j.corsci.2008.09.031 ↗
24. Improvement in corrosion resistance of friction stir welded aluminum alloys with micro arc oxidation coatings10.1016/j.scriptamat.2008.01.033 ↗
25. Effects of microstructure and local mechanical fields on intergranular stress corrosion cracking of a friction stir welded10.1016/j.corsci.2014.05.001 ↗
26. Effect of residual stresses on hydrogen permeation in iron10.1016/j.corsci.2010.02.045 ↗
27. Effect of Cr, Yb and Zr additions on localized corrosion of Al–Zn–Mg–Cu alloy10.1016/j.corsci.2009.08.001 ↗
28. Effect of Yb, Cr and Zr additions on recrystallization and corrosion resistance of Al–Zn–Mg–Cu alloys10.1016/j.msea.2008.07.028 ↗
29. Effects of Sc and Zr microalloying additions and ageing time at 120°C on the corrosion behaviour of an Al–Zn–Mg alloy10.1016/j.corsci.2012.08.024 ↗
30. Scientific principles of making an alloying addition of scandium to aluminium alloys10.1016/S0921-5093(99)00652-8 ↗
31. Alloying aluminum alloys with scandium and zirconium additives10.1007/BF01395323 ↗
32. Coarsening resistance at 400°C of precipitation-strengthened Al–Zr–Sc–Er alloys10.1016/j.actamat.2011.07.057 ↗
33. Effects of Yb and Zr microalloying additions on the microstructure and mechanical properties of dilute Al–Sc alloys10.1016/j.actamat.2011.09.019 ↗
34. Ambient- and high-temperature mechanical properties of isochronally aged Al–0.06Sc, Al–0.06Zr and Al–0.06Sc–0.06Zr (at.%) alloys10.1016/j.actamat.2010.10.017 ↗
35. Influence of scandium on the pitting behaviour of Al–Zn–Mg–Cu alloys10.1016/j.actamat.2007.08.021 ↗
36. The corrosion behaviour of scandium alloyed Al 5052 in neutral sodium chloride solution10.1016/S0010-938X(00)00147-5 ↗
37. Investigating localized corrosion susceptibility arising from Sc containing intermetallic Al3Sc in high strength Al-alloys10.1016/j.scriptamat.2007.01.036 ↗
38. Coarsening resistance at 400°C of precipitation-strengthened Al–Zr–Sc–Er alloys10.1016/j.actamat.2011.07.057 ↗
39. Microstructure and properties of TIG/FSW welded joints of a new Al–Zn–Mg–Sc–Zr alloy10.1007/s11665-013-0577-0 ↗
40. A cast 7050 friction stir weld with scandium: microstructure, corrosion and environmental assisted cracking10.1016/j.msea.2006.03.065 ↗
41. Corrosion behaviour of friction stir welded AA7108 T79 aluminium alloy10.1016/j.corsci.2005.02.020 ↗
42. Microstructure and pitting corrosion of friction stir welded joints in 2219-O aluminium alloy thick plate10.1016/j.corsci.2009.07.004 ↗
43. GB 15970.7-2000. National Standard of China, Corrosion of Metals and Alloys-Stress Corrosion Testing – Slow Strain Rate Testing.
44. Characterization of the SCC behaviour of 8090 Al–Li alloy by means of the slow-strain-rate technique10.1016/S0010-938X(97)00117-0 ↗
45. GB/T 22639-2008, National Standard of China. Test Method of Exfoliation Corrosion for Wrought Aluminum and Aluminum Alloys.
46. HREM study and structure modeling of the η′ phase, the hardening precipitates in commercial Al–Zn–Mg alloy10.1016/S1359-6454(99)00138-X ↗
47. Corrosion susceptibility of peened friction stri welded 7075 aluminium alloy joints10.1016/j.corsci.2008.09.031 ↗
48. Microstructure, mechanical properties and residual stresses as a function of welding speed in aluminium AA5083 friction stir welds10.1016/S1359-6454(03)00319-7 ↗
49. Influence of time on residual stresses in friction stir welds in agehardenable 7xxx aluminium alloys10.1016/j.actamat.2008.04.059 ↗
50. An investigation of the residual stress characterization and relaxation in peened friction stir welded aluminum–lithium alloy joints10.1016/j.matdes.2009.03.038 ↗
51. Role of grain size on the stress corrosion cracking of 7475 aluminium alloys10.1016/S0921-5093(96)10840-6 ↗
52. Influence of retrogression and re-aging treatment on corrosion behaviour of an Al–Zn–Mg–Cu alloy10.1016/j.matdes.2010.11.036 ↗
53. Enhancing stress corrosion cracking resistance in Al–Zn–Mg–Cu–Zr alloy through inhibiting recrystallization10.1016/j.engfracmech.2009.06.006 ↗
54. An exploratory study of the corrosion of Mg alloys during interrupted salt spray testing10.1016/j.corsci.2009.03.014 ↗
55. Effect of hot rolling and subsequent annealing on electrochemical discharge behavior of AP65 magnesium alloy as anode for seawater activated battery10.1016/j.corsci.2012.06.024 ↗
56. The effect of specimen size on the measured pitting potential of stainless10.1016/S0010-938X(97)83146-0 ↗
57. A hundred years of Tafel’s equation: 1905–200510.1016/j.corsci.2005.07.002 ↗
58. Influence of high-temperature pre-precipitation on local corrosion behavior of Al–Zn–Mg alloy10.1016/j.scriptamat.2006.09.028 ↗
59. Z.H He, Effects of Sc and Zr microalloying additions on the microstructure and mechanical properties of new Al–Zn–Mg alloys10.1016/j.jallcom.2012.03.108 ↗
60. Precipitation of Al3(Sc, Zr) particles in an Al–Zn–Mg–Cu–Sc–Zr alloy during conventional solution heat treatment and its effect on tensile properties10.1016/j.actamat.2008.04.005 ↗
61. Quantitative investigation of the tensile plastic deformation characteristic and microstructure for friction stir welded 2024 aluminum alloy10.1016/j.matchar.2012.08.007 ↗
62. Characterization of a friction-stir-welded aluminum alloy 601310.1007/s11663-002-0059-5 ↗
63. Experimental study on temperature distributions within the workpiece during friction stir welding of aluminum alloys10.1016/j.ijmachtools.2007.12.003 ↗
64. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
65. Properties of friction stir welded 7075-T651 aluminum10.1007/s11661-998-0021-5 ↗
66. Pitting corrosion of rheocast A356 aluminium alloy in 3.5 wt.% NaCl solution10.1016/j.corsci.2013.04.023 ↗
67. Characterization of cast AlSi(Cu) alloys by scanning Kelvin probe force microscopy10.1016/j.electacta.2006.03.027 ↗
68. Comparison of susceptibility to pitting corrosion of AA2024-T4, AA 7075-T651 and AA7475-T761 aluminium alloys in neutral chloride solutions using electrochemical noise analysis10.1016/j.corsci.2007.05.028 ↗
69. Influence of critical surface defects and localized competition between anodic dissolution and hydrogen effects during stress corrosion cracking of a 7050 aluminium alloy10.1016/S0921-5093(97)00369-9 ↗
70. Microstructure and properties of a new super-high-strength Al–Zn–Mg–Cu alloy C91210.1016/S0261-3069(97)00084-8 ↗
71. Influence of retrogression and reaging on microstructure, mechanical properties and susceptibility to stress corrosion cracking of an Al–Zn–Mg alloy10.1002/maco.200303710 ↗
72. Improvements in mechanical and stress corrosion cracking properties in Al-alloy 7075 via retrogress and reaging10.1016/j.msea.2007.08.025 ↗
73. Wang · 2000
74. Role of drawing-induced residual stresses and strains in the hydrogen embrittlement susceptibility of prestressing steels10.1016/j.corsci.2011.06.012 ↗
75. Effect of stress on electrochemical characteristics of pre-cracked ultrahigh strength stainless steel in acid sodium sulphate solution10.1016/j.corsci.2014.08.023 ↗
76. Effects of grain size on the corrosion resistance of wrought magnesium alloys containing neodymium10.1016/j.corsci.2012.01.021 ↗
77. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
78. Enhanced corrosion resistance of Mg alloy ZK60 after processing by integrated extrusion and equal channel angular pressing10.1016/j.actamat.2011.06.033 ↗
79. Effect of nanocrystalline grain size on the electrochemical and corrosion behavior of nickel10.1016/j.corsci.2004.04.007 ↗
80. Effects of grain size on the electrochemical corrosion behaviour of electrodeposited nanocrystalline Fe coatings in alkaline solution10.1016/j.corsci.2009.05.015 ↗
81. Grain size effects on the corrosion behavior of Ni50.5 Ti49.5 and Ni45.6 Ti49.3 Al5.1 films10.1016/j.jelechem.2008.02.020 ↗
82. Effect of grain size on corrosion of high purity aluminium10.1016/j.electacta.2010.09.023 ↗
83. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
84. Role of grain size on the stress aluminum corrosion cracking of 7475 Alloys10.1016/S0921-5093(96)10840-6 ↗
85. Effect of the number of ECAP pass time on the electrochemical properties of 1050 Al alloys10.1016/j.msea.2003.08.056 ↗
86. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
87. Grain character influences on corrosion of ECAPed pure magnesium10.1179/147842209X12559428167805 ↗
88. Corrosion resistance of ultra fine-grained Ti10.1016/j.scriptamat.2004.04.011 ↗
89. Pilling–Bedworth ratio for oxidation of alloys10.1007/s100190050008 ↗