journal article·2016-01

Effect of Mo, Ta, and Re on high-temperature oxidation behavior of minor Hf doped β-NiAl alloy

Baohong Han, Yue Ma, Hui Peng, Lei Zheng, Hongbo Guo

Corrosion Science· Volume 102
Publisher page

Abstract

Abstract The microstructure and cyclic oxidation behavior of minor Hf-doped NiAl alloys with addition of different alloying elements including Mo, Ta, and Re were investigated. Co-precipitation of Ta and Hf as well as Re and Hf occurred during alloy preparation, whereas Mo and Hf precipitated individually into different phases. Over 0.5 at.% addition of Mo, Ta and Re had negative influence on the oxidation behavior of β-NiAlHf alloy, while the effect could be ignorable once the concentration reduced to less than 0.05 at.%. The interaction mechanism between Ta and Hf as well as Re and Hf was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
2. Thermal barrier coatings for enhanced efficiency of gas turbine engines10.1016/j.surfcoat.2006.06.026 ↗
3. High temperature coatings for gas turbine blades: a review10.1016/0257-8972(89)90099-6 ↗
4. NiAl bond coats made by a directed vapour deposition approach10.1016/j.msea.2004.11.017 ↗
5. Cyclic oxidation and interdiffusion behavior of a NiAlDy/RuNiAl coating on a Ni-based single crystal superalloy10.1016/j.corsci.2011.04.025 ↗
6. Improved cyclic oxidation resistance of electron beam physical vapor deposited nano-oxide dispersed β-NiAl coatings for Hf-containing superalloy10.1016/j.corsci.2010.01.009 ↗
7. Comparison of the cyclic oxidation behavior of β-NiAl, β-NiPtAl and γ-γ′NiPtAl coatings on various superalloys10.1016/j.surfcoat.2007.06.039 ↗
8. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
9. Characterization of commercial EB-PVD TBC systems with CVD (Ni, Pt)Al bond coatings10.1016/S0257-8972(01)01483-9 ↗
10. Examination of the platinum effect on the oxidation behavior of nickel–aluminide coatings10.1016/j.surfcoat.2007.06.013 ↗
11. Effect of Hf and Y alloy additions on aluminide coating performance10.1016/j.surfcoat.2010.03.040 ↗
12. High temperature oxidation behavior of hafnium modified NiAl bond coat in EB-PVD thermal barrier coating system10.1016/j.tsf.2007.07.031 ↗
13. Effect of 0.1at.% zirconium on the cyclic oxidation resistance of β-NiAl10.1007/BF00659006 ↗
14. Effect of Dy on oxide scale adhesion of NiAl coatings at 1200°C10.1016/j.corsci.2011.03.003 ↗
15. Effects of Dy on cyclic oxidation resistance of NiAl alloy10.1016/S1003-6326(08)60426-4 ↗
16. The effect of various oxide dispersions on the phase composition and morphology of Al2O3 scales grown on β-NiAl10.1007/BF01682369 ↗
17. The oxidation behavior of oxide-dispersed β-NiAl: I. Short-term performance at 1200°C10.1023/A:1018894711276 ↗
18. Cyclic oxidation of β-NiAl with various reactive element dopants at 1200°C10.1016/j.corsci.2012.09.010 ↗
19. Effect of co-doping of two reactive elements on alumina scale growth of β-NiAl at 1200°C10.1016/j.corsci.2014.07.036 ↗
20. Cyclic oxidation and interdiffusion behavior of Pt modified NiAlHfCrSi coatings on single crystal superalloy containing Mo10.1016/j.surfcoat.2014.10.055 ↗
21. High-temperature diffusion barriers for protective coatings10.1016/j.surfcoat.2004.08.066 ↗
22. NiAlHf/Ru promising bond coat materials in thermal barrier coatings for advanced single crystal superalloys10.1016/j.corsci.2013.10.013 ↗
23. Synthesis and cyclic oxidation behavior of a (Ni,Pt)Al coating on a desulfurized Ni-based superalloy10.1007/s11661-999-0308-1 ↗
24. Effect of diffusion barrier on the high-temperature oxidation behavior of thermal barrier coatings10.1016/j.jallcom.2007.11.083 ↗
25. High temperature oxidation of γ/γ′-strengthened Co-base superalloys10.1016/j.corsci.2011.02.033 ↗
26. High temperature oxidation behavior of directionally solidified NiAl–31Cr–2.9Mo–0.1Hf–0.05Ho eutectic alloy10.1016/S1003-6326(11)61359-9 ↗
27. Formation of multilayered scale during the oxidation of NiAl–Mo alloy10.1016/j.apsusc.2014.01.148 ↗
28. Effect of alloying elements on the oxidation resistance of 4th generation Ni-base single-crystal superalloys10.2320/jinstmet.69.249 ↗
29. Effect of superalloy substrate composition on the performance of a thermal barrier coating system10.1023/A:1025992502450 ↗
30. Effect of Al and Ta on the high temperature oxidation of Ni-based superalloys10.1016/j.corsci.2014.10.025 ↗
31. The role of secondary oxide inclusions (pegs) on the spalling resistance of oxide films10.1016/S1359-6454(00)00081-1 ↗
32. Modelling of composition and phase changes in multiphase alloys due to growth of an oxide layer10.1016/j.actamat.2008.06.010 ↗
33. Beneficial effects of rhenium additions on the cyclic-oxidation resistance of β-NiAl+α-Cr alloys10.1023/A:1018804824847 ↗
34. Effect of quaternary additions on the oxidation behavior of Hf-doped NiAl10.1023/A:1023087926788 ↗
35. Effect of Sm, Gd, Yb, Sc, and Nd as reactive elements on oxidation behavior of β-NiAl at 1200°C10.1016/j.corsci.2013.10.021 ↗
36. The effect of silicon on the oxidation behavior of NiAlHf coating system10.1016/j.apsusc.2013.01.189 ↗
37. Determination of the constitution of the quasi-binary eutectic NiAl-Re system by DTA and microstructural investigations10.1016/S0921-5093(02)00388-X ↗
38. Partition of alloying elements between γ (A1), γ′ (L12), and β (B2) phases in Ni–Al base systems10.1007/BF02651589 ↗
39. Intermetallic NiAl-Ta alloys with strengthening Laves phase for high-temperature applications. I. Basic properties10.1016/S0966-9795(97)00031-9 ↗
40. Al–Ni–Ta (aluminum–nickel–tantalum)
41. The constitution diagram of the rhenium–hafnium system10.1016/0022-5088(63)90041-9 ↗
42. Influence of surface area and additives on the thermal stability of transition alumina catalyst supports. II: kinetic model and interpretation10.1016/S0166-9834(00)82459-8 ↗
43. Improved Cr2O3 adhesion by Ce ion implantation in the presence of interfacial sulfur segregation10.1016/j.actamat.2006.07.047 ↗
44. Experimental observations in support of the dynamic-segregation theory to explain the reactive-element effect10.1007/BF01046818 ↗
45. 18O/SIMS characterization of the growth mechanism of doped and undoped α-Al2O310.1007/BF00665610 ↗
46. Interfacial segregation, pore formation, and scale adhesion on NiAl alloys10.1007/s11085-005-1954-3 ↗
47. A TEM study of sulfur distribution in oxidized Ni40Al and its effect on oxide growth an adherence10.1016/j.msea.2006.11.015 ↗
48. Aero engine test experience with CMSX-4 alloy single-crystal turbine blades10.1115/1.2816600 ↗
49. Oxidation of a La2O3-modified aluminide coating10.1016/S1359-6462(01)00666-2 ↗
50. The oxidation behavior of CoCrAl systems containing active element additions10.1007/BF00609974 ↗