Unraveling the effects of CO2 and H2S on the corrosion behavior of electroless Ni-P coating in CO2/H2S/Cl– environments at high temperature and high pressure
Source abstract
Abstract
Abstract The effects of CO2 and/or H2S on the corrosion behavior of electroless Ni-P coating were investigated using weight loss method, surface characterization and water chemistry analysis. The results show that Ni-P coating demonstrates good resistance to corrosion in CO2 environment. While in H2S and CO2-H2S environments, corrosion of the coating is aggravated and controlled by H2S. The coexistence of CO2 and H2S causes a CO2-enhanced H2S corrosion effect, synergistically accelerating the coating degradation through increasing the electrolyte aggressiveness and changing the surface film characteristics. Concurrently, H2S facilitates the electrolyte penetration at the coating microdefects, causing the localized corrosion of substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Electrocatalysts for Energy Conversion
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. A study on corrosion behavior of Ni-Cr-Mo laser coating, 316 stainless steel and X70 steel in simulated solutions with H2S and CO210.1016/j.surfcoat.2016.02.017 ↗
2. Initiation and developmental stages of steel corrosion in wet H2S environments10.1016/j.corsci.2015.01.024 ↗
3. The electrochemical behavior of 316L austenitic stainless steel in Cl– containing environment under different H2S partial pressures10.1016/j.apsusc.2013.10.080 ↗
4. Electrochemical corrosion behavior of carbon steel under dynamic high pressure H2S/CO2 environment10.1016/j.corsci.2012.08.007 ↗
5. The experiment research of corrosion behavior about Ni-based alloys in simulant solution containing H2S/CO210.1016/j.electacta.2011.05.116 ↗
6. Application of nickel-coated carbon fibre material in cathodic protection of underground-buried steel structures10.1016/j.corsci.2009.06.054 ↗
7. Corrosion protection with hard coatings on steel: past approaches and current research efforts10.1016/j.surfcoat.2014.08.069 ↗
8. Studies on electrodeposition and characterization of the Ni-W-Fe alloys coatings10.1016/j.jallcom.2014.09.087 ↗
9. Downhole corrosion behavior of Ni-W coated carbon steel in spent acid & formation water and its application in full-scale tubing10.1016/j.engfailanal.2016.05.014 ↗
10. Deposition of electroless Ni-P graded coatings and evaluation of their corrosion resistance10.1016/j.surfcoat.2004.10.014 ↗
11. Effect of coating time and heat treatment on structures and corrosion characteristics of electroless Ni-P alloy deposits10.1016/S0257-8972(03)00746-1 ↗
12. Temperature effects on the chemical composition of nickel-phosphorus alloy thin films10.1016/j.tsf.2009.09.007 ↗
13. High corrosion-resistant Ni-P/Ni/Ni-P multilayer coatings on steel10.1016/j.surfcoat.2004.11.004 ↗
14. Duplex Ni-P-ZrO2/Ni-P electroless coating on stainless steel10.1016/j.jallcom.2015.01.064 ↗
15. Electrochemical studies on electroless ternary and quaternary Ni-P based alloys10.1016/j.electacta.2006.07.001 ↗
16. Evaluation of the corrosion resistance of electroless Ni-P and Ni-P composite coatings by electrochemical impedance spectroscopy10.1007/s100080000159 ↗
17. An XPS investigation into the passivity of an amorphous Ni-20P alloy10.1149/1.2095880 ↗
18. Electrochemical corrosion testing of high phosphorus electroless nickel in 5% NaCl10.5006/1.3585309 ↗
19. Synthesis of a duplex Ni-P-YSZ/Ni-P nanocomposite coating and investigation of its performance10.1016/j.surfcoat.2016.12.075 ↗
20. EIS as a means of evaluating electroless nickel deposits10.1016/0013-4686(93)80345-Z ↗
21. The anodic behavior of amorphous Ni-19P alloys in different amorphous states10.1016/0010-938X(89)90122-4 ↗
22. Characterization and corrosion behavior of electroless Ni-P/nano-SiC coating inside the CO2 containing media in the presence of acetic acid10.1016/j.matdes.2010.07.030 ↗
23. Effect of defect on corrosion behavior of electroless Ni-P coating in CO2-saturated NaCl solution10.1016/j.corsci.2018.01.041 ↗
24. The corrosion behavior of electroless Ni-P coating in Cl–/H2S environment10.1016/j.apsusc.2012.05.094 ↗
25. Corrosion resistance enhancement of electroless Ni-P coating by incorporation of ultrasonically dispersed diamond nanoparticles10.1016/j.corsci.2013.07.046 ↗
26. Quality of electroless Ni-P (nickel-phosphorus) coatings applied in oil production equipment with salinity
27. Development of electroless Ni-P/nano-WC composite coatings and investigation on its properties10.1016/j.surfcoat.2015.07.011 ↗
28. Improvement of the erosion-corrosion resistance of magnesium by electroless Ni-P/Ni(OH)2-ceramic nanoparticle composite coatings10.1016/j.surfcoat.2016.04.063 ↗
29. Characterization and corrosion resistance of duplex electroless Ni-P composite coatings on magnesium alloy10.1016/j.surfcoat.2013.05.047 ↗
30. Corrosion behavior of Ni-P-nano-Al2O3 composite coating in the presence of anionic and cationic surfactants10.1016/j.surfcoat.2016.12.089 ↗
31. Improving surface characteristic and corrosion inhibition of coating on Mg alloy by trace stannous (II) chloride10.1016/j.corsci.2017.04.018 ↗
32. Corrosion of stainless 316 L in simulated formation water environment with CO2-H2S-Cl–10.1016/j.corsci.2009.08.010 ↗
33. Effects of chloride content on CO2 corrosion of carbon steel in simulated oil and gas well environments10.1016/j.corsci.2014.03.025 ↗
34. ASTM Standard G1-03 · 2011
35. Stability of an electrodeposited nanocrystalline Ni-based alloy coating in oil and gas wells with the coexistence of H2S and CO210.3390/ma10060632 ↗
36. ASTM Standard G31-72 · 2004
37. ASTM Standard G46-94 · 2005
38. NACE standard RP0775-2005 · 2005
39. Crystallisation kinetics and phase transformation behaviour of electroless nickel-phosphorus deposits with high phosphorus content10.1016/S0925-8388(01)01798-4 ↗
40. Effect of alloying elements and microstructure on stability of corrosion product in CO2 and/or H2S environments
41. Onsite substitution synthesis of ultrathin Ni nanofilms loading ultrafine Pt nanoparticles for hydrogen evolution, ACS Appl10.1021/acsami.5b07472 ↗
42. Advanced asymmetric supercapacitors based on Ni(OH)2/graphene and porous graphene electrodes with high energy density10.1002/adfm.201102839 ↗
43. Cliff-like NiO/Ni3S2 directly grown on Ni foam for battery-type electrode with high area capacity and long cycle stability10.1016/j.electacta.2017.08.102 ↗
44. Effect of applied potential on passivation and erosion-corrosion of a Fe-based amorphous metallic coating under slurry impingement10.1016/j.corsci.2014.01.004 ↗
45. Preparation and electrochemical characterization of hollow hexagonal NiCo2S4 nanoplates as pesudocapacitor materials10.1021/sc400472z ↗
46. Controllable preparation of nanoporous Ni3S2 films by sulfuration of nickel foam as promising asymmetric supercapacitor electrodes10.1016/j.apsusc.2017.05.206 ↗
47. Electroactive edge site-enriched nickel-cobalt sulfide into graphene frameworks for high-performance asymmetric supercapacitors10.1039/C5EE03633J ↗
48. Studies of nickel-tungsten-alumina catalysts by X-ray photoelectron spectroscopy10.1021/j100560a009 ↗
49. Effect of CO2 and H2S on the composition and stability of passive film on iron alloys in geothermal water10.1016/j.electacta.2007.01.086 ↗
50. Marcus · 2012
51. Key issues related to modelling of internal corrosion of oil and gas pipelines – a review10.1016/j.corsci.2007.06.006 ↗
52. Anderko · 2000
53. Corrosion of low alloy steel and stainless steel in supercritical CO2/H2O/H2S systems10.1016/j.corsci.2016.06.003 ↗
54. Smith · 1994
55. Mesh-capped probe design for direct pH measurements at an actively corroding metal surface10.1007/s10800-009-0043-8 ↗
56. Formation of iron oxide and iron sulfide at high temperature and their effects on corrosion10.1016/j.corsci.2018.02.045 ↗
57. The kinetics and mechanism of the nickel electrode - III. The potentiodynamic response of nickel electrodes in alkaline solutions in the potential region of Ni(OH)2 formation10.1016/S0010-938X(78)80094-8 ↗
58. The characteristics of the potentiodynamic potential/current profiles obtained with the Ni/0.5 N H2SO4 interface. A contribution to the mechanism of the electrode process10.1016/0010-938X(80)90072-4 ↗
59. Dunlop · 1983
60. Dugstad · 2006
61. Chloride role in the surface of nickel electrode10.1016/S0013-4686(98)00199-6 ↗
62. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗
63. Passivity breakdown, pit initiation and propagation of pits in metallic materials - review10.1016/j.corsci.2014.10.006 ↗
64. The effect of H2S on the performance of Ni-YSZ anodes in solid oxide fuel cells10.1016/j.jpowsour.2009.02.001 ↗
65. Smith · 2002
66. Agrawal · 2004
67. The effect of deformation on metastable pitting of 304 stainless steel in chloride contaminated concrete pore solution10.1016/j.corsci.2015.11.022 ↗
68. The effects of anions on the behavior of scratched iron electrodes in aqueous solutions10.1016/0010-938X(80)90145-6 ↗
69. Initial stages of the anodic oxidation of iron in chloride solutions10.5006/1.3585204 ↗