Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water
Source abstract
Abstract
Abstract Stress corrosion cracking (SCC) in the heat affected zone (HAZ) of a stainless steel 308L-316L weld joint in primary water of pressurized water reactor was investigated. Stress corrosion crack growth in the HAZ was observed in off-normal primary water chemistry with dissolved oxygen, but not in normal primary water chemistry with dissolved hydrogen. This suggests that it is unlikely a stress corrosion crack propagating in the HAZ could reach the fusion boundary and penetrate into the weld metal under normal primary water chemistry conditions. Microstructure analysis of the crack tip suggests that the SCC follows the slip-oxidation mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. PWSCC of austenitic stainless steels of heaters of pressurizers
2. Stress corrosion cracking of austenitic stainless steels in PWR primary water: an update of metallurgical investigations performed on French withdrawn components
3. SCC of stainless steels under PWR primary circuit service conditions
4. Perspective and direction of stress corrosion cracking in hot water
5. Crack growth rate of hardened austenitic stainless steels in BWR and PWR environments
6. SCC growth behaviors of austenitic stainless steels in simulated PWR primary water10.1016/j.jnucmat.2012.03.013 ↗
7. F. Vaillant, T. Couvant, J.M. Boursier, C. Amzallag, Y. Rouillon, O. Raquet, Stress corrosion cracking of cold worked austenitic stainless steels in laboratory primary PWR environment, ASME/JSME, 2004, Pressure Vessels and Piping Conference, American Society of Mechanical Engineers, San Diego, California, July 25–29, 2004, pp. 51–63.10.1115/PVP2004-3057 ↗
8. IGSCC of non–sensitized stainless steels in high temperature water10.1016/j.jnucmat.2008.08.005 ↗
9. Stress corrosion cracking of a low alloy steel to stainless steel transition weld in PWR primary waters at 292°C10.1016/S0010-938X(99)00131-6 ↗
10. Microstructure, microchemistry and stress corrosion crack characteristics in a BWR 316LSS core shroud weld
11. Effect of dissolved oxygen content on stress corrosion cracking of a cold worked 316L stainless steel in simulated pressurized water reactor primary water environment10.1016/j.jnucmat.2013.11.027 ↗
12. Role of water chemistry and microstructure in stress corrosion cracking in the fusion boundary region of an alloy 182-A533B low alloy steel dissimilar weld joint in high temperature water10.1016/j.corsci.2011.08.046 ↗
13. Environmentally-assisted cracking behaviour in the transition region of an alloy182/SA 508Cl.2 dissimilar metal weld joint in simulated boiling water reactor normal water chemistry environment10.1016/j.jnucmat.2008.06.034 ↗
14. Stress corrosion cracking behavior in the transition region of alloy 182/low-alloy reactor pressure vessel steel dissimilar metal weld joints in light water reactor environments10.5006/1400 ↗
15. Effects of K and anion impurity concentration on crack growth kinetics near Alloy 182/A533B weld overlay boundaries in BWRs
16. Effects of PWR primary water chemistry and deaerated water on SCC
17. Effects of temperature and corrosion potential on SCC
18. Stress corrosion crack growth rate behavior of various grades of cold worked stainless steel in high temperature water
19. Effect of strain–hardening on stress corrosion cracking of AISI 304L stainless steel in PWR primary environment at 360°C
20. Effects of cold working degrees on grain boundary characters and strain concentration at grain boundaries in alloy 60010.1016/j.corsci.2010.11.022 ↗
21. Environmentally assisted crack growth in one-dimensionally cold worked alloy 690TT in primary water10.1016/j.corsci.2011.12.031 ↗
22. Effects of cold working path on strain concentration, grain boundary microstructure and stress corrosion cracking in alloy 60010.1016/j.corsci.2011.05.037 ↗
23. Residual strain measurement and grain boundary characterization in the heat–affected zone of a weld joint between alloy 690TT and alloy 5210.1016/j.jnucmat.2009.12.016 ↗
24. Strain and microstructure characterization of austenitic stainless steel weld HAZs
25. SCC of alloy 690 and its weld metals
26. The stress corrosion crack growth rate of Alloy 600 heat affected zones exposed to high purity water
27. Establishment of experimental conditions for the SCC growth rate test of Alloy 600 and Ni base weld metal in high temperature oxygenated water
28. CGR behavior of low carbon stainless steel of hardened heat affected zone in PLR piping weld joints
29. Effect of loading direction on crack growth behavior near fusion line in low carbon stainless steel weld joints
30. Nuclear Industry Safety Agency (NISA), Cracks on the inner surface of the welds at primary water inlet and outlet nozzle to steam generators, NISA, 2008.
31. Kansai electric’s efforts to develop aging management technologies
32. Stress corrosion crack growth in type 316 stainless steel in supercritical water10.5006/1.3278318 ↗
33. Measurement of local plastic strain distribution of stainless steel by electron backscatter diffraction10.1016/j.matchar.2008.07.010 ↗
34. Cold work and temperature dependence of stress corrosion crack growth of austenitic stainless steels in hydrogenated and oxygenated high-temperature water10.5006/1.3278329 ↗
35. Study on SCC growth behavior of BWR core shroud
36. Effects of thermo-mechanical treatments on deformation behavior and IGSCC susceptibility of stainless steels in PWR primary water chemistry
37. Growth testing of cold worked stainless steel in a simulated PWR primary water environment to assess susceptibility to stress corrosion cracking
38. Plastic strain and residual stress distributions in an AISI 304 stainless steel BWR pipe weld
39. Intergranular cracking of AISI 316NG stainless steel in BWR environment
40. Crack growth behavior of irradiated type 316 SS in low dissolved oxygen environment
41. K/Size effects on SCC in irradiated, cold worked and unirradiated stainless steel
42. SCC crack growth of cold–worked type 316SS in simulated BWR oxidizing and hydrogen water chemistry conditions
43. Crack growth behavior of welded and cast stainless steels in hydrogenated and oxygenated high–temperature water
44. Comparison of IGSCC crack–tip characteristics produced in BWR oxidizing water and BWR hydrogen water chemistry conditions
45. Crack-tip characteristics in BWR service components
46. Nanoscale characterization of grain boundary oxidation in cold-worked stainless steels10.1016/j.corsci.2012.06.030 ↗
47. Early stage SCC initiation analysis of FCC Fe-Cr-Ni ternary alloy at 288°C: a quantum chemical molecular dynamics approach10.1016/j.corsci.2009.01.005 ↗
48. Microstructural characterization of SCC crack tip and oxide film for SUS316 stainless steel in simulated PWR water at 320°C10.1080/18811248.2005.9726383 ↗
49. Defining the role of solute diffusion kinetics at crack tips in stainless steel during irradiation in light-water reactors