Mechanical, oxidation and ablation properties of C/(C-SiC)CVI-(ZrC-SiC)PIP composites
Source abstract
Abstract
Abstract A joint chemical vapor infiltration-precursor infiltration and pyrolysis (CVI-PIP) process was used to fabricate C/C-SiC-ZrC composites with different volume ratio of CVI-derived C-SiC. The composite with a C-SiC volume ratio of 0.91 has a higher tensile and flexural strength of 181.7 MPa and 352.8 MPa, respectively, and also exhibits a better anti-oxidation property at 800∼1400 °C for 30 h. After an oxyacetylene ablation for 600 s at ∼2100 °C, the composite with a C-SiC volume ratio of 0.12 possesses a better anti-ablation performance with a linear and mass ablation rates of 0.94 um × s−1 and 0.13 mg × cm-2×s−1, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Carbon fiber reinforced hafnium carbide composite10.1023/B:JMSC.0000041696.64055.8c ↗
2. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
3. Material property requirements for analysis and design of UHTC components in hypersonic applications10.1016/j.jeurceramsoc.2010.01.026 ↗
4. Oxidation-based materials selection for 2000°C + hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
5. Oxidation protection of C/C composites with a multilayer coating of SiC and Si + SiC + SiC nanowires10.1016/j.carbon.2011.10.048 ↗
6. The future of carbon-carbon composites10.1016/0008-6223(87)90116-3 ↗
7. The effect of carbon fabric treatment on delamination of 2D-C/C composites10.1016/j.compscitech.2006.03.025 ↗
8. C/C–SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
9. Development of hot CMC structures for space re-entry vehicles via fight experiments
10. Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC Composites10.1002/adem.200290001 ↗
11. Oxidation of ZrB2–SiC ceramic under atmospheric and reentry conditions
12. The oxidation behavior of SiC–ZrC–SiC coated C/SiC minicomposites at ultrahigh temperatures10.1111/j.1551-2916.2010.04178.x ↗
13. Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration10.1016/S0008-6223(98)00076-1 ↗
14. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
15. The thermal stability in air of hot-pressed diboride matrix composites for uses at ultra-high temperatures10.1016/j.corsci.2004.09.019 ↗
16. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500 °C10.1016/j.jeurceramsoc.2006.10.012 ↗
17. Effect of PyC interphase thickness on mechanical and ablation properties of 3D Cf/ZrC–SiC composite10.1016/j.ceramint.2016.04.187 ↗
18. Fabrication and properties of 3-D Cf/SiC–ZrC composites, using ZrC precursor and polycarbosilane10.1111/j.1551-2916.2012.05116.x ↗
19. Effects of porous C/C density on the densification behavior and ablation property of C/C–ZrC–SiC composites10.1016/j.carbon.2013.01.059 ↗
20. Effects of low-temperature thermal cycling treatment on the microstructures, mechanical properties and oxidation resistance of C/C–ZrC–SiC composites10.1016/j.jallcom.2017.05.263 ↗
21. Effects of high-temperature annealing on the microstructures and mechanical properties of C/C–ZrC–SiC composites prepared by precursor infiltration and pyrolysis10.1016/j.matdes.2015.10.140 ↗
22. C/C–SiC–ZrC composites fabricated by reactive melt infiltration with Si0.87Zr0.13 alloy10.1016/j.ceramint.2012.02.016 ↗
23. Ablation behaviors of ultra-high temperature ceramic composites10.1016/j.msea.2007.02.040 ↗
24. Fabrication and properties of 3-D Cf/ZrC–SiC composites via in-situ reaction10.1016/j.ceramint.2013.07.022 ↗
25. Mechanical and physical behaviors of short pitch-based carbon fiber-reinforced HfB2–SiC matrix composites10.1016/j.ceramint.2012.07.108 ↗
26. Carbon-fiber-reinforced C-SiC binary matrix composites10.1016/0008-6223(94)00169-Z ↗
27. Characterization of interfaces in C fiber-reinforced laminated C–SiC matrix composites10.1016/S0008-6223(99)00177-3 ↗
28. Effect of PyC interphase thickness on mechanical behaviors of SiBC matrix modified C/SiC composites fabricated by reactive melt infiltration10.1016/j.carbon.2014.05.092 ↗
29. Influence of fiber coating thickness on microstructure and mechanical properties of carbon fiber-reinforced zirconium diboride based composites10.1016/j.ceramint.2013.07.040 ↗
30. Zhang · 2001 · 231
31. The thermal expansion of graphite within the layer planes10.1016/0022-3115(64)90139-4 ↗
32. Structure/oxidation behavior relationship in the carbonaceous constituents of 2D–C/PyC/SiC composites10.1016/0008-6223(93)90086-P ↗
33. Dynamic fracture of C/SiC composites under high strain-rate loading: microstructures and mechanisms10.1016/j.carbon.2015.05.015 ↗
34. The effect of heat treatment on the strength and toughness of carbon fiber/silicon carbide composites with different pyrolytic carbon interphase thicknesses10.1016/j.carbon.2013.01.076 ↗
35. Residual stresses in fiber-reinforced ceramics due to thermal expansion mismatch10.1111/j.1151-2916.1993.tb03988.x ↗
36. Microstructures and ablation properties of C/C−SiC−ZrC composites prepared using C/C skeletons with various densities10.1016/j.ceramint.2013.03.093 ↗
37. Effects of ZrC content on microstructure and properties of 2D C/SiC–ZrC composites via precursor infiltration and pyrolysis
38. Effect of pyrolytic carbon interface on the properties of 3D C/ZrC–SiC composites fabricated by reactive melt infiltration10.1016/j.ceramint.2016.03.155 ↗
39. Preparation of 3D Cf/ZrC–SiC composites by joint processes of PIP and RMI10.1016/j.msea.2014.03.071 ↗
40. Fabrication and properties of PIP 3D Cf/ZrC–SiC composites10.1016/j.msea.2013.10.102 ↗
41. Atmospheric corrosion of carbon steel in Colombia10.1016/j.corsci.2009.09.006 ↗
42. Evolution of corrosion of MnCuP weathering steel submitted to wet/dry cyclic tests in a simulated coastal atmosphere10.1016/j.corsci.2012.01.017 ↗
43. Oxidation and ablation of 3D carbon–carbon composite at up to 3000 °C10.1016/0008-6223(94)00172-V ↗
44. Ablation mechanism and properties of SiCf/SiBCN ceramic composites under an oxyacetylene torch environment10.1016/j.corsci.2014.01.006 ↗
45. Ablation behavior and mechanism of SiCf/Cf/SiBCN ceramic composites with improved thermal shock resistance under oxyacetylene combustion flow10.1016/j.ceramint.2015.03.144 ↗
46. Effect of heat flux on ablation behaviour and mechanism of C/C–ZrB2–SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
47. Oxidation–resistant ZrB2–SiC composites at 2200 °C10.1016/j.compscitech.2007.08.017 ↗
48. Spinodal decomposition in amorphous metal–silicate thin films: phase diagram analysis and interface effects on kinetics10.1063/1.1510590 ↗
49. Ablation behavior and mechanism of C/ZrC, C/ZrC–SiC and C/SiC composites fabricated by polymer infiltration and pyrolysis process10.1016/j.corsci.2014.05.005 ↗
50. Ablation behaviour of C/C and C/C–ZrC–SiC composites with cone-shaped holes under an oxyacetylene flame10.1016/j.corsci.2015.09.022 ↗
51. Effect of SiC/ZrC ratio on the mechanical and ablation properties of C/C–SiC–ZrC composites10.1016/j.corsci.2013.12.017 ↗