Effect of chloride and sulfate ions in simulated boiler water on pitting corrosion behavior of 13Cr steel
Source abstract
Abstract
Abstract The pitting corrosion behavior of 13Cr steel was investigated in simulated boiler waters containing chloride ions (Cl − ) and sulfate ions (SO 4 2− ) using potentiodynamic and potentiostatic polarization tests in addition to pit morphology analysis. The presence of 100 ppm Cl − in the water caused pitting corrosion of the steel. Pit initiation was inhibited by the addition of 50 ppm or 100 ppm SO 4 2− into the water containing 100 ppm Cl − . Pit growth was also suppressed by the presence of 50 ppm SO 4 2− in the water with 100 ppm Cl − ; however, it was conversely promoted in the presence of 100 ppm SO 4 2− .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Report of Central Research Institute of Electric Power Industry, T97801, Steam Chemistry and Corrosion in Steam Turbine, Tokyo, 1998, pp. 29–47.
2. Chemical processes in steam turbines
3. Recent developments in understanding of the phase transition zone in the low pressure steam turbine
4. Steam turbine corrosion
5. O. Jonas, L. Machemer, Steam turbine corrosion and deposits problems and solutions, in: Proc. 37th Turbomachinery Symposium, Houston, USA, 2008, pp. 211–228.
6. Geothermal steam turbines with high efficiency, high reliability blades
7. Pit to crack transition in stress corrosion cracking of a steam turbine disc steel10.1016/j.corsci.2003.09.017 ↗
8. SCC behavior of low-pressure steam turbine materials for fossil power plants under conditions coexisted with oxygen and corrosive chemicals10.3323/jcorr1991.53.568 ↗
9. Accelerated corrosion behavior due to alternating dry–wet conditions for LP steam turbine materials of fossil power plants10.2355/isijinternational.45.373 ↗
10. Effect of Cl− and SO42− on pitting corrosion susceptibility for materials of low-pressure steam turbines in power plants10.2320/jinstmet.74.635 ↗
11. Environmental factors affecting the critical potential for pitting in 18–8 stainless steel10.1149/1.2423801 ↗
12. Japanese Standards Association, Water Conditioning for Boiler Feed Water and Boiler Water; JIS B 8223, Japanese Standards Association, Tokyo, 2006.
13. The effects of some anions on metastable pitting of 316L stainless steel10.1016/S0010-938X(01)00031-2 ↗
14. The metastable pitting potential and its relation to the pitting potential for four materials in chloride solutions10.1016/j.corsci.2013.11.015 ↗
15. Japan Society of Corrosion Engineering, Corrosion Handbook, Maruzen, Tokyo, 2000, pp. 573–576.
16. Metastable pitting of stainless steel10.5006/1.3583880 ↗
17. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗
18. The nucleation and growth of corrosion pits on stainless steel10.1016/0010-938X(93)90133-2 ↗
19. Pit growth studies in stainless steel foils. I. Introduction and pit growth kinetics10.1016/S0010-938X(01)00133-0 ↗
20. Electrochemical crevice corrosion behavior of low-pressure steam turbine materials in the simulated boiler water added chloride and sulfate ions10.2320/matertrans.M2013202 ↗
21. Studies on accumulation of chloride ions in pits growing during anodic polarization10.1016/0010-938X(75)90015-3 ↗
22. The corrosion of single pits on stainless steel in acidic chloride solution10.1016/0010-938X(88)90060-1 ↗
23. Pit growth studies in stainless steel foils. II. Effect of temperature, chloride concentration and sulphatr addition10.1016/S0010-938X(01)00134-2 ↗
24. The mechanism of lacy cover formation in pitting10.1016/S0010-938X(97)00043-7 ↗