journal article·2019-08

On microstructure and corrosion behaviour of AlSi10Mg alloy with low surface roughness fabricated by direct metal laser sintering

P. Fathi, M. Rafieazad, X. Duan, M. Mohammadi, A.M. Nasiri

Corrosion Science· Volume 157
Publisher page

Abstract

Abstract In this study, in-depth microstructure and electrochemical properties of highly smoothed AlSi10Mg parts fabricated through direct-metal-laser-sintering are reported. The samples with the lowest surface roughness were characterized by having a periodic large and small melt pools (MPs) pattern in their upskin layers. Consequently, a noticeably coarser eutectic-Si network, Al-dendrite and grain size formed along the larger MPs’ borders, rationalized by their slower solidification rate. Such microstructural features were found to control/deteriorate the electrochemical performance of the as-printed samples than their surface roughness. An improved electrochemical stability for the samples that experience the fastest solidification rate along their MP-boundaries was revealed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
2. Additive manufacturing of metals : a brief review of the characteristic microstructures and properties of steels
3. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
4. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
5. Influence of process parameters on surface roughness of aluminum parts produced by DMLS10.1007/s00170-012-4688-9 ↗
6. On the surface quality of additive manufactured parts10.1007/s00170-016-9215-y ↗
7. Comparison of forming manufacturing processes and selective laser melting technology based on the mechanical properties of products10.1080/17452759.2011.613597 ↗
8. Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by Selective Laser Melting (SLM)10.1016/j.matchar.2017.06.029 ↗
9. Achieving low surface roughness AlSi10Mg 200C parts using direct metal laser sintering10.1016/j.addma.2017.12.012 ↗
10. A comparative study on corrosion and microstructure of direct metal laser sintered AlSi10Mg_200C and die cast A360.1 aluminum10.1016/j.jmatprotec.2018.04.013 ↗
11. Surface Roughness and Morphology Customization of Additive Manufactured Open Porous Ti6Al4V Structures10.3390/ma6104737 ↗
12. Influences of processing parameters on surface roughness of Hastelloy X produced by selective laser melting10.1016/j.addma.2016.10.010 ↗
13. Evaluation of corrosion resistance of Al – 10Si – Mg alloy obtained by means of Direct Metal Laser Sintering10.1016/j.jmatprotec.2015.12.033 ↗
14. Corrosion resistance of direct metal laser sintering AlSiMg alloy10.1002/sia.5981 ↗
15. Effects of surface finishing procedure on corrosion behavior of DMLS-AlSi10Mg_200C alloy vs die cast A360.1 aluminum
16. Effect of heat treatment on corrosion resistance of DMLS AlSi10Mg alloy10.1016/j.electacta.2016.04.157 ↗
17. Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by Selective Laser Melting (SLM)10.1016/j.matchar.2017.06.029 ↗
18. Corrosion Behavior of AlSi10Mg Alloy Produced by Additive Manufacturing (AM) vs. Its Counterpart Gravity Cast Alloy10.3390/met6070148 ↗
19. Local Corrosion Behavior of Additive Manufactured AlSiMg Alloy Assessed by SEM and SKPFM10.1149/2.0461702jes ↗
20. Corrosion behavior of heat-treated AlSi10Mg manufactured by laser powder bed fusion10.3390/ma11071051 ↗
21. Correlation between process parameters, microstructure and properties of 316 L stainless steel processed by selective laser melting10.1016/j.msea.2018.01.103 ↗
22. Gamry Instrument, MultiPort Electrochemical Cell Kit Operator’s Manual, (n.d.). https://www.gamry.com/assets/Uploads/MultiPort-Manual-Rev1-4.pdf.
23. Comparison of Methods for Removal of Corrosion Product from AA2024-T310.5006/1.3290336 ↗
24. Modeling of the thermal physical process and study on the reliability of linear energy density for selective laser melting10.1016/j.rinp.2018.03.047 ↗
25. Energy density analysis on single tracks formed by selective laser melting with CoCrMo powder material10.1007/s00170-013-4902-4 ↗
26. On the limitations of Volumetric Energy Density as a design parameter for Selective Laser Melting10.1016/j.matdes.2016.10.037 ↗
27. On the effect of process parameters on properties of AlSi10Mg parts produced by DMLS10.1108/RPJ-03-2013-0028 ↗
28. Microstructure and mechanical properties of AlSi10Mg parts produced by the laser beam additive manufacturing (AM) technology10.1007/s13632-014-0168-y ↗
29. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
30. Columnar to equiaxed transition during direct metal laser sintering of AlSi10Mg alloy: effect of building direction10.1016/j.addma.2018.08.001 ↗
31. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: comparison between virgin and recycled powders10.1016/j.addma.2018.07.014 ↗
32. Microstructural characterization of cellular AlSi10Mg alloy fabricated by selective laser melting10.1016/j.matdes.2018.08.005 ↗
33. On microstructure and mechanical properties of additively manufactured AlSi10Mg_200C using recycled powder10.1016/j.msea.2017.09.041 ↗
34. Image processing with ImageJ
35. Microstructure and mechanical properties of aluminium alloy cellular lattice structures manufactured by direct metal laser sintering10.1016/j.msea.2015.01.063 ↗
36. Kou · 2003
37. Formation of AlSi10Mg surfaces via selective laser melting: scanning electron microscopy and Raman spectroscopy study10.1088/1742-6596/1092/1/012170 ↗
38. Galvanostatic Anodizing of additive manufactured Al-Si10-Mg alloy st ´10.1149/2.1121714jes ↗
39. Quantitative texture prediction of epitaxial columnar grains in additive manufacturing using selective laser melting10.1016/j.addma.2017.05.005 ↗
40. Microstructure, texture and mechanical properties of 6061 aluminum laser beam welded joints10.1016/j.matchar.2018.01.030 ↗
41. Selective laser melting of aluminum die-cast alloy—correlations between process parameters, solidification conditions, and resulting mechanical properties10.2351/1.4906389 ↗
42. Deformation mechanism during dynamic loading of an additively manufactured AlSi10Mg_200C10.1016/j.msea.2018.03.014 ↗
43. Evolution of solidification texture during additive manufacturing10.1038/srep16446 ↗
44. Pitting corrosion of rheocast A356 aluminium alloy in 3.5wt.% NaCl solution10.1016/j.corsci.2013.04.023 ↗
45. Microstructure and corrosion behaviour of A356 aluminium alloy modified with Nd10.1002/maco.201407674 ↗
46. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
47. Pitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗
48. Szklarska-Smialowska · 1986
49. Effect of surface abrasion on pitting corrosion of Al-Li alloy10.1016/j.corsci.2018.04.010 ↗
50. Effect of surface roughness on corrosion resistance of sol-gel coatings on AA2024-T3 alloy10.1149/2.0271514jes ↗
51. Corrosion of aluminium alloy AlSi7Mg0.3 in artificial sea water with added sodium sulphide10.1016/j.corsci.2018.08.038 ↗
52. EIS study on pitting corrosion of AA5083-H321 aluminum-magnesium alloy in stagnant 3.5% NaCl solution
53. Improvement of corrosion behavior of A3xx.x/SiCp composites in 3.5 wt % NaCl solution by Ce surface coatings10.1149/1.2150151 ↗
54. Origins of pitting corrosion
55. Study of nobility of chromium nitrides in isothermally aged duplex stainless steels by using SKPFM and SEM/EDS10.1016/j.corsci.2009.08.057 ↗
56. Size dependence of microstructure of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.matchar.2017.11.052 ↗
57. Ashby · 2000
58. E.G.– E.O. Systems · 2014
59. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
60. Heat transfer and fluid flow of molten pool during selective laser melting of AlSi10Mg powder: simulation and experiment10.1016/j.jmapro.2017.02.009 ↗
61. Microstructure and mechanical properties of stainless steel CX manufactured by Direct Metal Laser Sintering10.1016/j.msea.2017.10.045 ↗