Glass coatings on stainless steels for high-temperature oxidation protection: Mechanisms
Source abstract
Abstract
Abstract The oxidation behavior of a martensitic stainless steel with or without glass coating was investigated at 600–800 °C. The glass coating provided effective protection for the stainless steel against high-temperature oxidation. However, it follows different protection mechanisms depending on oxidation temperature. At 800 °C, glass coating acts as a barrier for oxygen diffusion, and oxidation of the glass coated steel follows linear law. At 700 or 600 °C, glass coating induces the formation of a (Cr, Fe)2O3/glass composite interlayer, through which the diffusion of Cr3+ or Fe3+ is dramatically limited. Oxidation follows parabolic law.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Recent developments in the preparation, characterization and applications of glass- and glass-ceramic-to-metal seals and coatings10.1007/s10853-010-5095-y ↗
2. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature10.1016/j.corsci.2007.06.007 ↗
3. A new high temperature resistant glass-ceramic coating for gas turbine engine components10.1007/BF02708539 ↗
4. Electrochemical impedance spectroscopy for studying the degradation of enamel coatings10.1016/S0010-938X(01)00149-4 ↗
5. Microstructure and properties characterization of the double layered glass-ceramic coating on near-α titanium alloy10.1016/j.surfcoat.2010.04.008 ↗
6. Wetting and sealing of interface between 7056 glass and kovar alloy10.1016/j.matchemphys.2007.04.012 ↗
7. Corrosion resistance and mechanism of steel rebar coated with three types of enamel10.1016/j.corsci.2012.02.024 ↗
8. Silicate glass coatings on Ti-based implants10.1016/S1359-6454(98)80039-6 ↗
9. Preparation and thermal shock behavior at 1000°C of a glass-alumina-NiCrAlY tri-composite coating on K38G superalloy10.1016/j.surfcoat.2011.11.015 ↗
10. Metal-glass based composites for novel TBC-systems
11. Glass-ceramic coatings on titanium alloys for high temperature oxidation protection: oxidation kinetics and microstructure10.1016/j.corsci.2013.04.041 ↗
12. SiO2–Al2O3–glass composite coating on Ti–6Al–4V alloy: oxidation and interfacial reaction behavior10.1016/j.corsci.2013.05.010 ↗
13. Effect of sand blasting and glass matrix composite coating on oxidation resistance of a nickel-based superalloy at 1000°C10.1016/j.corsci.2013.04.022 ↗
14. Comparative study of interfacial reaction between superalloy substrate and glass coating with and without alumina particles incorporation10.1016/j.apsusc.2013.01.165 ↗
15. Electrochemical behavior of enamel-coated carbon steel in simulated concrete pore water solution with various chloride concentrations10.1016/j.electacta.2012.12.125 ↗
16. The effects of a nickel oxide precoat on the gas bubble structures and fish-scaling resistance in vitreous enamels10.1016/j.msea.2003.08.003 ↗
17. An analysis of the microstructure and interfacial chemistry of steel–enamel interface10.1016/S0040-6090(03)00973-8 ↗
18. Effect of crystallization on the property of hard enamel coating on steel substrate10.1016/j.apsusc.2008.12.007 ↗
19. Effect of surface pretreatments on the adherence of porcelain enamel to a type 316L stainless steel10.1023/A:1004728416960 ↗
20. Glass and glass-ceramic coatings, versatile materials for industrial and engineering applications10.1007/BF02704843 ↗
21. Microstructure and adherence of cobalt containing and cobalt free enamels to low carbon steel10.1016/j.msea.2006.12.108 ↗
22. Microstructure of the enamel–steel interface: cross-sectional TEM and metallographic studies10.1016/0921-5093(92)90382-B ↗
23. Role of “adherence oxides” in the development of chemical bonding at glass–metal interfaces10.1111/j.1151-2916.1966.tb13135.x ↗
24. Yttrium sol–gel coating effects on the cyclic oxidation behaviour of 304 stainless steel10.1016/S0010-938X(03)00114-8 ↗
25. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
26. The influence of microstructure on the oxidation of duplex stainless steels in simulated propane combustion products at 1000°C10.1016/j.corsci.2008.11.023 ↗
27. Oxidation kinetics of high strength low alloy steels at elevated temperatures10.1016/j.corsci.2008.08.008 ↗
28. Quantitative high-temperature oxidation of porcelain enameled iron10.1111/j.1151-2916.1958.tb13543.x ↗
29. The presence of an iron oxide layer at the enamel/steel interface in one-coat porcelain enamelling10.1007/BF00560649 ↗
30. Kinetics of dissolution and diffusion of the oxides of iron in sodium disilicate glass10.1111/j.1151-2916.1968.tb15674.x ↗
31. Self-diffusion of iron in alkali–magnesia–silica glass melts10.1016/S0022-3093(98)00368-8 ↗
32. Diffusion of oxygen in vitreous silica10.1111/j.1151-2916.1963.tb13763.x ↗
33. Crystallization behavior of SiO2–Al2O3–ZnO–CaO glass system at 1123–1273K10.1111/j.1551-2916.2010.03859.x ↗
34. Effect of NiCrAlY platelets inclusion on the mechanical and thermal shock properties of glass matrix composites10.1016/j.msea.2010.10.015 ↗
35. Liang · 1993
36. Effect of shot-peening on the oxidation behaviour of boiler steels10.1007/s11085-011-9250-x ↗