Isothermal experiments on steam oxidation of magnetron-sputtered chromium-coated zirconium alloy cladding at 1200 ℃
Source abstract
Abstract
The isothermal steam oxidation behavior of chromium-coated zirconium alloy cladding at 1200 ℃ is studied. The cladding substrate is Zr-1 Nb alloy with outer diameter of 9.5 mm and thickness of 0.57 mm. The Cr coating is prepared by magnetron sputtering method with thickness of about 11 µm. The oxidation durations are 300 s~14,400 s. After oxidation, blisters are formed on the surface due to the compressive stress in coating, and the coating surfaces are porous or exhibit a morphology with ravines and granular crystals. A four-layer structure (Cr 2O 3, Cr, Zr(Cr,Fe) 2 and Zr from outside to inside) is formed in the early stage of oxidation. However, Zr 4+ can migrate into Cr coating through grain boundaries and reacts with Cr 2O 3 . The redox reaction between Zr and Cr 2O 3 leads to the coating failure, resulting in the oxidation of Zr alloy substrate. Due to selective oxidation, a certain thickness of Cr coating is retained during the thickening of outer ZrO 2. The emergence of outer ZrO 2 layer is significantly delayed by Cr coating, and Cr coating is able to reduce the growth rate of outer ZrO 2 layer. Therefore, Cr coating has a protective effect in 1,200 ℃ steam environment and can improve the oxidation resistance of Zr alloy cladding.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Insights from review and analysis of the Fukushima Dai-ichi accident10.1080/18811248.2011.636538 ↗
2. A review on analysis of LWR severe accident10.1115/1.4030364 ↗
3. Primary radiation damage characteristics in displacement cascades of FeCrAl alloys10.1016/j.jnucmat.2021.152909 ↗
4. Preliminary evaluation of U3Si2-FeCrAl fuel performance in light water reactors through a multi-physics coupled way10.1016/j.nucengdes.2017.12.019 ↗
5. Oxidation kinetics of Cr-coated zirconium alloy: effect of coating thickness and microstructure10.1016/j.corsci.2020.108883 ↗
6. Design and characterization of zirconium-based multilayer coating for carbon/carbon composites against oxyacetylene ablation10.1016/j.corsci.2021.109785 ↗
7. Influence of Al content on the oxidation behavior of CrAl coating on Zry-4 alloys in 1200°C steam
8. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
9. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
10. A comparative study on preliminary performance evaluation of ATFs under normal and accident conditions with FRAP-ATF code10.1016/j.pnucene.2017.12.010 ↗
11. A systematic study of the oxidation behavior of Cr coatings on Zry4 substrates in high temperature steam environment10.1016/j.corsci.2020.108826 ↗
12. Protective coatings on zirconium-based alloys as accident-Tolerant fuel (ATF) claddings10.1515/corrrev-2017-0010 ↗
13. Microstructure and tensile behavior of powder metallurgy FeCrAl accident tolerant fuel cladding10.1016/j.jnucmat.2022.153524 ↗
14. Exploring the high-temperature steam oxidation behaviors of the lean-Cr (7–10 wt%) FeCrAl alloys10.1016/j.corsci.2021.109927 ↗
15. Development of low-Cr wrought FeCrAl cladding alloys and its irradiation tolerance and steam oxidation resistance at 1200 °C10.1016/j.corsci.2021.109998 ↗
16. Development of accident tolerant FeCrAl-ODS fuel cladding for BWRs in Japan10.1016/j.jnucmat.2021.153276 ↗
17. Degradation mechanism of SiCf/SiC composites after long-time water vapor and oxygen corrosion at 1300 °C10.1016/j.corsci.2022.110099 ↗
18. Development and testing of multicomponent fuel cladding with enhanced accidental performance10.1016/j.net.2019.08.015 ↗
19. J.C. Brachet, M. Dumerval, V. Lezaud-Chailioux, M. Le Saux, E. Rouesne, D. Hamon, S. Urvoy, T. Guilbert, Q. Houmaire, C. Cobac, Behavior of chromium coated M5TM claddings under LOCA conditions, in: WRFPM 2017, WRFPM 2017 Water Reactor Fuel Performance Meeting, 2017.
20. S.K. Arifin, M. Hamid, A.N. Berahim, M.H. Ani, Effects of water vapor on protectiveness of Cr2O3 scale at 1073 K, in: IOP Conf. Ser. Mater. Sci. Eng., Institute of Physics Publishing, 2018: p. 012085. https://doi.org/10.1088/1757–899X/290/1/012085.10.1088/1757-899X/290/1/012085 ↗
21. Review on chromium coated zirconium alloy accident tolerant fuel cladding
22. Steam oxidation of Cr-coated Sn-containing zircaloy solid rod at 1000 °C10.1016/j.corsci.2021.109682 ↗
23. A thermodynamic database for zirconium alloys10.1016/S0022-3115(99)00125-7 ↗
24. High temperature steam oxidation of chromium-coated zirconium-based alloys: kinetics and process10.1016/j.corsci.2020.108537 ↗
25. Development of cold spray chromium coatings for improved accident tolerant zirconium-alloy cladding10.1016/j.jnucmat.2019.03.039 ↗
26. High temperature oxidation and microstructural evolution of cold spray chromium coatings on Zircaloy-4 in steam environments10.1016/j.jnucmat.2019.151737 ↗
27. High temperature Cr-Zr interaction of two types of Cr-coated Zr alloys in inert gas environment10.1016/j.jnucmat.2021.152806 ↗
28. High-temperature oxidation and quenching of chromium-coated zirconium alloy ATF cladding tubes with and w/o pre-damage10.1016/j.jnucmat.2021.153470 ↗
29. Microstructure, corrosion resistance and oxidation behavior of Cr-coatings on Zircaloy-4 prepared by vacuum arc plasma deposition10.1016/j.corsci.2019.06.029 ↗
30. High-temperature oxidation of thick Cr coating prepared by arc deposition for accident tolerant fuel claddings10.1016/j.jnucmat.2019.01.039 ↗
31. Behavior of plasma sprayed Cr coatings and FeCrAl coatings on Zr fuel cladding under loss-of-coolant accident conditions10.1016/j.surfcoat.2018.03.016 ↗
32. Oxidation behavior of Cr-coated zirconium alloy cladding in high-temperature steam above 1200 °C10.1038/s41529-021-00155-8 ↗
33. Transient experiments on oxidation and degradation of Cr-coated Zircaloy in steam up to 1600 ℃10.1016/j.corsci.2021.109805 ↗
34. Early studies on Cr-Coated Zircaloy-4 as enhanced accident tolerant nuclear fuel claddings for light water reactors10.1016/j.jnucmat.2019.02.018 ↗
35. Evaluation of equivalent cladding reacted parameters of Cr-coated claddings oxidized in steam at 1200 °C in relation with oxygen diffusion/partitioning and post-quench ductility10.1016/j.jnucmat.2020.152106 ↗
36. Systematic investigations on the coating degradation mechanism during the steam oxidation of Cr-coated Zry-4 at 1200 °C10.1016/j.corsci.2022.110310 ↗
37. An interesting oxidation phenomenon of Cr coatings on Zry-4 substrates in high temperature steam environment10.1016/j.corsci.2019.05.017 ↗
38. Assessment of the severe accident code MIDAC based on FROMA, QUENCH-06&16 experiments
39. Numerical simulation of zircaloy-water reaction based on the moving particle semi-implicit method and combined analysis with the MIDAC code for the nuclear-reactor core melting process10.1016/j.pnucene.2019.103083 ↗
40. H. Georges, A state-of-the-art review of past programs devoted to fuel behaviour under LOCA conditions - part3 Cladding Oxidation. Resistance to Quench and Post-Quench Loads., (n.d.).
41. Advanced treatment of zircaloy cladding high-temperature oxidation in severe accident code calculations: Part I. Experimental database and basic modeling10.1016/j.nucengdes.2004.02.013 ↗
42. Stresses in NiO, Cr2O3 and Al2O3 oxide scales10.1016/0921-5093(94)09747-X ↗
43. Effects of water vapor on protectiveness of Cr2O3 scale at 1073 K10.1088/1757-899X/290/1/012085 ↗
44. Predicting oxide stability in high-temperature water vapor10.1007/s11837-006-0063-3 ↗
45. Effect of water vapour on growth and adherence of chromia scales formed on Cr in high and low pO2-environments at 1000 and 1050°C10.3184/096034005782744443 ↗
46. Role of water vapor in chromia-scale growth at low oxygen partial pressure10.1023/A:1023040010859 ↗
47. Development of oxidation model for zirconium alloy cladding and application in the analysis of cladding behavior under loss of coolant accident10.1016/j.jnucmat.2022.153564 ↗
48. Oxidation kinetics and oxygen diffusion in low-tin Zircaloy-4 up to 1523 K10.1016/j.jnucmat.2008.03.012 ↗
49. J. Stuckert, M.S. Veščunov, Behaviour of oxide layer of zirconium-based fuel rod cladding under steam starvation conditions, FZKA-7373, Forschungszentrum Karlsruhe, 2008.
50. Cladding oxidation model development based on diffusion equations and a simulation of the monoclinic-tetragonal phase transformation of zirconia during transient oxidation10.1016/j.jnucmat.2014.03.035 ↗