Corrosion behaviour of AA6082 Al-Mg-Si alloy extrusion: Recrystallized and non-recrystallized structures
Source abstract
Abstract
• Recrystallized region in AA6082 alloy extrusion is susceptible to intergranular corrosion. • Non-recrystallized region is susceptible to both intergranular and intragranular corrosion. • Corrosion morphology is related to crystallographic defect density. • Corrosion penetration rate and propagation path are related to grain structure. • Heavily deformed non-recrystallized region is more susceptible to corrosion. In the present study, the corrosion behaviour of AA6082 Al-Mg-Si alloy extrusion, consisting of a recrystallized surface region and non-recrystallized fibre structure core, is investigated. It is found that the corrosion penetration rate and propagation path are closely related to grain structure and local plastic deformation. Corrosion morphology changes from intergranular corrosion in recrystallized region to both intergranular and intragranular corrosion of the heavily deformed subgrains in non-recrystallized region. Further, local plastic deformation is quantified by electron backscatter diffraction and transmission Kikuchi diffraction and correlated to corrosion propagation path.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Effect of thermomechanical history on intergranular corrosion of extruded AlMgSi(Cu) model alloy10.1016/j.corsci.2006.03.018 ↗
2. Effect of artificial aging on intergranular corrosion of extruded AlMgSi alloy with small Cu content10.1016/j.corsci.2005.05.045 ↗
3. Effect of high temperature heat treatment on intergranular corrosion of AlMgSi(Cu) model alloy10.1016/j.corsci.2004.12.003 ↗
4. Effect of low copper content and heat treatment on intergranular corrosion of model AlMgSi alloys10.1016/j.corsci.2004.11.025 ↗
5. Improving the intergranular corrosion resistance of Al-Mg-Si-Cu alloys without strength loss by a two-step aging treatment10.1016/j.msea.2013.10.001 ↗
6. The influence of MgSi particle reactivity and dissolution processes on corrosion in Al-Mg-Si alloys10.1016/j.electacta.2008.05.078 ↗
7. Investigation of the exfoliation-like attack mechanism in relation to Al-Mg-Si alloy microstructure10.1016/j.corsci.2008.04.003 ↗
8. Influence of overaging treatment on localized corrosion of Al 605610.5006/1.3280517 ↗
9. The role of grain boundary regions in the localized corrosion of a copper-free 6111-like aluminum alloy10.5006/1.3278189 ↗
10. Localized corrosion of 6056 T6 aluminium alloy in chloride media10.1016/S0010-938X(99)00053-0 ↗
11. Intergranular corrosion of copper-containing AA6xxx AlMgSi aluminum alloys10.1149/1.2976774 ↗
12. Grain boundary precipitation induced by grain crystallographic misorientations in an extruded Al–Mg–Si–Cu alloy10.1016/j.jallcom.2014.10.206 ↗
13. General aspects related to the corrosion of 6xxx series aluminium alloys: exploring the influence of Mg/Si ratio and Cu10.1016/j.corsci.2013.06.035 ↗
14. Understanding the origins of intergranular corrosion in copper-containing Al-Mg-Si alloys10.1007/s11661-015-3296-3 ↗
15. Corrosion mechanism associated with Mg2Si and Si particles in Al-Mg-Si alloys10.1016/S1003-6326(11)61092-3 ↗
16. Microstructural studies on the effect of Si and Cr on the intergranular corrosion in Al-Mg-Si alloys10.1016/S0261-3069(97)00027-7 ↗
17. Significance of low copper content on grain boundary nanostructure and intergranular corrosion of AlMgSi(Cu) model alloys10.4028/www.scientific.net/MSF.519-521.667 ↗
18. Davis · 1999
19. Electrochemical behavior and localized corrosion associated with Mg2Si particles in Al and Mg alloys10.1149/2.002201eel ↗
20. Effect of excess silicon and small copper content on intergranular corrosion of 6000-Series aluminum alloys10.1149/1.3261804 ↗
21. Effect of grain boundary characteristics on intergranular corrosion resistance of 6061 aluminum alloy extrusion10.1007/s11661-002-0274-3 ↗
22. Precipitation in an AA6111 aluminium alloy and cosmetic corrosion10.1016/j.actamat.2006.08.025 ↗
23. Precipitation and corrosion behaviour of nano-structured near-surface layers on an AA6111 aluminium alloy10.1088/1742-6596/26/1/024 ↗
24. The origin of the grain boundary precipitate free zone10.1016/0001-6160(69)90154-0 ↗
25. The influence of grain structure on the corrosion behaviour of 2A97-T3 Al-Cu-Li alloy10.1016/j.corsci.2016.12.005 ↗
26. The propagation of localized corrosion in Al-Cu-Li alloy10.1002/sia.5890 ↗
27. Localized corrosion in AA 2099-T83 aluminium-lithium alloy: the role of grain orientation10.1016/j.corsci.2016.02.018 ↗
28. Grain-stored energy and the propagation of intergranular corrosion in AA2xxx aluminium alloys10.1002/sia.5218 ↗
29. Corrosion behaviour of 2A97-T6 Al-Cu-Li alloy: the influence of non-uniform precipitation10.1016/j.corsci.2017.12.010 ↗
30. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
31. Effects of strain localization on the corrosion behavior of ultra-fine grained aluminum alloy AA606110.1016/j.corsci.2018.04.023 ↗
32. Identification of the metallurgical parameters explaining the corrosion susceptibility in a 2050 aluminium alloy10.1016/j.corsci.2015.10.020 ↗
33. The precipitation sequence in Al-Mg-Si alloys10.1016/S1359-6454(98)00059-7 ↗
34. Precipitation hardening in Al-Mg-Si alloys with and without excess Si10.1016/S0921-5093(01)01247-3 ↗
35. The influence of prolonged natural aging on the subsequent artificial aging response of the AA6111 automotive alloy10.1007/s11661-015-3043-9 ↗
36. Phase relations and precipitation in Al–Mg–Si alloys with Cu additions10.1016/S0079-6425(03)00031-8 ↗
37. Localized corrosion in AA2024-T351 aluminium alloy: transition from intergranular corrosion to crystallographic pitting10.1016/j.matchar.2017.06.022 ↗