Intergranular erosion corrosion of pure copper tube in flowing NaCl solution

Lei Wu, Aili Ma, Lianmin Zhang, Yugui Zheng

Corrosion Science· Volume 201
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. The corrosion of copper and its alloys: a practical guide for engineers
2. In-situ graphene enhanced copper wire: a novel electrical material with simultaneously high electrical conductivity and high strength10.1016/j.carbon.2021.10.015 ↗
3. Epoxy coating modified with graphene: a promising composite against corrosion behavior of copper surface in marine media10.1016/j.jallcom.2019.153380 ↗
4. Corrosion behavior of copper with minor alloying addition in chloride solution10.1016/j.jallcom.2007.08.008 ↗
5. Interactive effect of ant nest corrosion and stress corrosion on the failure of copper tubes10.1016/j.engfailanal.2017.09.013 ↗
6. Hot-water corrosion failure of a hard-drawn copper tube10.1016/j.engfailanal.2013.04.020 ↗
7. The influence of corrosion product structure on the corrosion rate of Cu-Ni alloys10.1016/S0010-938X(70)80022-1 ↗
8. Electrochemical corrosion of unalloyed copper in chloride media––a critical review10.1016/S0010-938X(02)00257-3 ↗
9. The corrosion of copper-nickel alloys 706 and 715 in flowing sea water. I – Effect of oxygen
10. Effect of fluid dynamics on the corrosion of copper-based alloys in sea water10.5006/0010-9312-33.1.3 ↗
11. Failure analysis of a copper tube in a finned heat exchanger10.1016/j.engfailanal.2015.02.016 ↗
12. Erosion–corrosion of heat exchanger tubes10.1016/j.engfailanal.2009.03.026 ↗
13. A metallographic case study of formicary corrosion in heat exchanger copper tubes10.1016/j.engfailanal.2020.104502 ↗
14. Ant nest corrosion – exploring the labyrinth
15. Ant-nest corrosion digging the tunnels10.1515/CORRREV.2002.20.1-2.51 ↗
16. Investigating the mechanism behind 'Ant Nest' corrosion on copper tube10.3390/ma11040533 ↗
17. Intergranular stress corrosion cracking of copper – a case study10.1016/j.corsci.2007.05.014 ↗
18. Stress corrosion cracking of a copper elbow fitting10.1016/j.engfailanal.2018.03.016 ↗
19. Some aspects of the atmospheric corrosion of copper in the presence of sodium chloride10.1149/1.1838422 ↗
20. Chemical characterization and anticorrosion properties of corrosion products formed on pure copper in synthetic rainwater of Rio de Janeiro and São Paulo10.1016/j.corsci.2009.11.003 ↗
21. Evaluation of corrosion behavior of copper in chloride media using electrochemical Impedance spectroscopy (EIS)10.4152/pea.200502301 ↗
22. Investigating the flow induced corrosion of copper in chloride-containing solution at the atomistic scale10.1016/j.apsusc.2020.147925 ↗
23. Effect of exposure time on the polarization behavior of marine alloys under flowing and quiescent conditions10.5006/1.3583052 ↗
24. Electrochemical impedance spectroscopy study of the passive oxide film on titanium for implant application10.1016/0013-4686(95)00465-3 ↗
25. Corrosion product film formed on the 90/10 copper-nickel tube in natural seawater: Composition/structure and formation mechanism10.1016/j.corsci.2014.11.028 ↗
26. Influence of hydrostatic pressure on the corrosion behavior of 90/10 copper-nickel alloy tube under alternating dry and wet condition10.1016/j.corsci.2018.10.036 ↗
27. Electrochemical impedance spectroscopy (EIS) of corrosion processes on inhomogeneous surfaces10.1016/0013-4686(90)80004-8 ↗
28. Comparison of the corrosion behavior of pure titanium and its alloys in fluoride-containing sulfuric acid10.1016/j.corsci.2015.11.003 ↗
29. Localised instability of titanium during its erosion-corrosion in simulated acidic hydrometallurgical slurries10.1016/j.corsci.2020.108816 ↗
30. Technical note: concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
31. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
32. Constant-phase-element behavior caused by resistivity distributions in films10.1149/1.3499565 ↗
33. Electrochemical impedance spectroscopy (EIS) as a new tool for investigating methods of corrosion protection10.1016/0013-4686(90)80007-B ↗
34. Infrared optical properties of cuprous oxide10.1063/1.1734530 ↗
35. Optical constants of CuO and ZnO particles in the terahertz frequency range10.1016/j.ceramint.2020.06.190 ↗
36. The effect of sulphate-reducing bacteria biofilm on passivity and development of pitting on 2205 duplex stainless steel10.1016/j.electacta.2016.07.043 ↗
37. Significantly enhanced resistance to SRB corrosion via Fe-based amorphous coating designed with high dose corrosion-resistant and antibacterial elements
38. Correlations between the inhibition performances and the inhibitor structures of some azoles on the galvanic corrosion of copper coupled with silver in artificial seawater10.1016/j.corsci.2019.108413 ↗
39. Copper-nickel alloys modified with thin surface films: corrosion behaviour in the presence of chloride ions10.1016/j.corsci.2010.09.041 ↗
40. Surface “roughness” effect on marine immersion corrosion of mild steel
41. Intergranular corrosion of AA6082 Al–Mg–Si alloy extrusion: The influence of trace Cu and grain boundary misorientation10.1016/j.jallcom.2020.157228 ↗
42. Copper (sub)oxide formation: a surface sensitive characterization of model catalysts10.1039/b000253o ↗
43. Oxygen injection during fast vs slow passivation in aqueous solution10.1016/j.actamat.2021.116898 ↗
44. 1D Nb-doped LiNi1/3Co1/3Mn1/3O2 nanostructures as excellent cathodes for Li-ion battery10.1016/j.electacta.2018.11.172 ↗
45. Effect of Ti ion doping on electrochemical performance of Ni-rich LiNi0.8Co0.1Mn0.1O2 cathode material10.1016/j.electacta.2019.135086 ↗
46. Swanson · 1953
47. The electric field gradient at the position of copper in Cu2O and electronic charge density analysis by means of K-factors10.1007/BF00309465 ↗
48. Realizing reversible conversion‐alloying of Sb(V) in polyantimonic acid for fast and durable lithium‐ and potassium‐ion storage
49. Structure of B6O boron-suboxide by Rietveld refinement10.1007/BF00367573 ↗
50. Interstitial oxygen in oxygen-stoichiometric apatites10.1039/b503374h ↗
51. Refinement by the rietveld method and extended X-ray absorption fine structure of a 1,2,3-type ceramic oxide containing cobalt instead of copper10.1039/dt9910000403 ↗
52. ESCA studies of Cu, Cu2O and CuO10.1016/0039-6028(73)90206-9 ↗
53. Characterization of nanostructured CuO–porous silicon matrix formed on copper-coated silicon substrate via electrochemical etching10.1007/s00339-013-8008-5 ↗
54. Anomalous chemical shifts of Cu 2p and Cu LMM Auger spectra of silicate glasses10.1016/S0368-2048(03)00126-9 ↗
55. Near-ambient XPS characterization of interfacial copper species in ceria-supported copper catalysts10.1039/C5CP04354A ↗
56. Critical flow velocity phenomenon in erosion-corrosion of pipelines: determination methods, mechanisms and applications10.1016/j.jpse.2021.01.005 ↗
57. Flow dependent corrosion. I. Current understanding of the mechanisms involved10.1002/maco.19830340906 ↗
58. "Horse shoe" corrosion of copper alloys in flowing sea water: Mechanism, and possibility of cathodic protection of condenser tubes in power stations10.5006/0010-9312-34.11.396 ↗
59. Cavity formation and metallurgical changes induced by growth of oxide scale10.1179/mst.1988.4.12.1089 ↗
60. Electrochemical reduction of the corrosion products formed on copper surface in alkaline-sulphide solutions10.1016/j.jallcom.2006.05.099 ↗
61. Reflections on the history of electrochemical impedance spectroscopy10.1016/j.electacta.2005.02.107 ↗
62. The behaviour of Cu-Ni-x (x=10 to 40 wt%) alloys in alkaline solutions containing chloride ions10.1016/S0013-4686(96)00315-5 ↗
63. Corrosion behavior of the filmed copper surface in saline water under static and jet impingement conditions10.5006/1.3683224 ↗
64. K.D. Efird, Flow accelerated corrosion testing basics, in: Proceedings of the CORROSION 2006, San Diego, California, OnePetro, 2006.10.5006/C2006-06689 ↗