The effect of artificial ageing heat treatments on the corrosion-induced hydrogen embrittlement of 2024 (Al–Cu) aluminium alloy

Nikolaos D. Alexopoulos, Zaneta Velonaki, Constantinos I. Stergiou, Stavros K. Kourkoulis

Corrosion Science· Volume 102
Publisher page

Abstract

Abstract This work is focused on the role of microstructure ( S -type particles) that are precipitated in the aluminium matrix due to artificial ageing on the tensile ductility decrease of 2024 aluminium alloy when exposed to exfoliation corrosion solution. A common, extremely short corrosion exposure time was selected to corrode the already heat-treated specimens in different conditions, including under-, peak- and over-ageing so as to avoid pitting formation and to concentrate only to hydrogen embrittlement degradation. Corrosion-induced yield stress decrease was less sensitive to the change of microstructure. Corrosion-induced tensile ductility decrease was correlated with the precipitation of S -phase particles, showing that the specimens at the peak-ageing ( S ″ and S ′ precipitates) and over-ageing ( S precipitates) exhibited the lowest decrease (∼11% and ∼22%, respectively) due to corrosion exposure. The highest ductility decrease (∼26%) was noticed for the T3 condition (as received) that limited GPB zones were formed on the grain boundaries. Tensile ductility decrease was also ageing temperature sensitive, as the lowest temperature gave the least ductility decrease, thus giving proof of the role of the precipitates on the corrosion mechanism. The results were explained based on the hydrogen trapping at the interphases of the S -type precipitates.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. How complex is the microstructure of AA2024-T3?10.1016/j.corsci.2009.05.001 ↗
2. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
3. Application of Modern aluminum alloys to aircraft10.1016/0376-0421(95)00004-6 ↗
4. Structural changes on aging Al–Cu–Mg alloys
5. Mondolfo · 1976
6. Nucleation of precipitates in aged Al–Cu–Mg–(Ag) alloys with high Cu:Mg ratios10.1016/1359-6454(95)00314-2 ↗
7. Response to comments on cluster hardening in an aged Al–Cu–Mg alloy10.1016/S1359-6462(98)00364-9 ↗
8. Two types of S precipitates in Al–Cu–Mg alloys10.1016/j.actamat.2006.09.015 ↗
9. Localized corrosion of 2024-T351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
10. In-situ confocal laser scanning microscopy of AA2024-T3 corrosion metrology: 1. localized corrosion of particles10.1149/1.1764780 ↗
11. In-situ confocal laser scanning microscopy of AA2024-T3 corrosion metrology: 2. trench formation around particles10.1149/1.1764781 ↗
12. Statistical study of the corrosion behavior of Al2CuMg intermetallics in AA2024-T35110.1149/1.2799089 ↗
13. Combination of AFM, SKPFM, and SIMS to study the corrosion behavior of S-phase particles in AA2024-T35110.1149/1.2833315 ↗
14. Co-operative corrosion phenomena10.1016/j.corsci.2009.10.021 ↗
15. Cerium tartrate as a corrosion inhibitor for AA 2024-T310.1016/j.corsci.2015.03.010 ↗
16. Simulating corrosion of Al2CuMg phase by measuring ionic currents, chloride concentration and pH10.1016/j.corsci.2014.07.021 ↗
17. Relation between microstructural aspects of AA2024 and its corrosion behaviour investigated using AFM scanning potential technique10.1016/S0010-938X(00)00002-0 ↗
18. The effect of precipitate size on the yield strength-pitting corrosion correlation in Al–Cu–Mg alloys10.1016/j.actamat.2010.07.010 ↗
19. Role of nanostructure in pitting of Al–Cu–Mg alloys10.1016/j.electacta.2010.02.001 ↗
20. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
21. Grain-stored energy and the propagation of intergranular corrosion in AA2xxx aluminium alloys10.1002/sia.5218 ↗
22. In situ X-ray tomography of intergranular corrosion of 2024 and 7050 aluminium alloys10.1016/j.corsci.2010.08.026 ↗
23. The study of intergranular corrosion in aircraft aluminium alloys using X-ray tomography10.1016/j.corsci.2010.11.005 ↗
24. Combined Kelvin probe force microscopy and secondary ion mass spectrometry for hydrogen detection in corroded 2024 aluminium alloy10.1016/j.electacta.2013.02.063 ↗
25. Corrosion-induced hydrogen embrittlement of 2024 and 6013 aluminum alloys10.1016/j.tafmec.2003.11.014 ↗
26. Corrosion-induced hydrogen embrittlement in aluminium alloy 202410.1016/j.corsci.2005.05.015 ↗
27. Experimental and theoretical studies of corrosion-induced mechanical properties degradation of aircraft 2024 aluminum alloy10.1016/j.msea.2008.08.024 ↗
28. On the corrosion-induced mechanical degradation for different artificial aging conditions of 2024 aluminum alloy10.1016/j.msea.2009.05.023 ↗
29. Characterization of trapped hydrogen in exfoliation corroded aluminum alloy 202410.1016/S1359-6462(99)00292-4 ↗
30. The diffusion and trapping of hydrogen in high purity aluminum10.1016/S1359-6454(98)00333-4 ↗
31. Scamans · 1979 · 464
32. Corrosion in artificial defects. I: Development of corrosion10.1016/j.corsci.2005.05.050 ↗
33. Behaviour of hydrogen in pure aluminium, Al-4 mass% Cu and Al-1 mass% Mg2 Si alloys studied by tritium electron microautoradiography10.1007/BF00349974 ↗
34. The contribution of hydrogen to the corrosion of 2024 aluminum alloy exposed to thermal and environmental cycling in chloride media10.1016/j.corsci.2012.12.005 ↗
35. Pit propagation rate on the 2024 and 6056 aluminium alloys10.1016/S0010-938X(97)00147-9 ↗
36. Stable pit formation on 2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
37. Electrochemical aspects of exfoliation corrosion of aluminium alloys: the effects of heat treatment10.1016/j.corsci.2011.01.010 ↗
38. Corrosion behaviour of 2024 Al–Cu–Mg alloy of various tempers10.1016/S1003-6326(13)62856-3 ↗
39. Transitions between pitting and intergranular corrosion in AA202410.1016/S0013-4686(02)00828-9 ↗
40. 1992 · 13
41. Hatch · 1984 · 245
42. N.D. Alexopoulos, Z. Velonaki, C. Stergiou, S.K. Kourkoulis, Artificial ageing and mechanical properties of aluminium alloy 2024, submitted for publication, 2015.
43. Accelerated corrosion exposure in ultra-thin sheets of 2024 aircraft aluminium alloy for glare applications10.1016/j.corsci.2011.10.032 ↗
44. Martin · 1998
45. Polmear · 1995
46. Corrosion of AA2024-T3 Part III: propagation10.1016/j.corsci.2010.09.035 ↗
47. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
48. Hydrogen absorption into aluminum alloy 2024-t3 during exfoliation and alternate immersion testing10.5006/1.3284830 ↗
49. Effect of prior deformation and heat treatment on the corrosion-induced hydrogen trapping in aluminium alloy 202410.1016/j.corsci.2013.11.021 ↗