Cyclic oxidation and rumpling behaviour of single phase β-(Ni,Pt)Al coatings with different thickness of initial Pt plating

Y.F. Yang, C.Y. Jiang, H.R. Yao, Z.B. Bao, S.L. Zhu, F.H. Wang

Corrosion Science· Volume 111
Publisher page

Abstract

Abstract Cyclic oxidation behaviour of single phase β-(Ni,Pt)Al coatings with different thickness of initial Pt plating was evaluated at 1100 °C in air. The coating sample of 5 μm Pt showed the best oxidation resistance, and after oxidation a dual-layered structure of alumina scale was formed on this coating with precipitation of Pt-rich particles at both boundary and interior of columnar α-Al2O3 grains. Comparatively, the coating sample with 8 μm Pt was prone to rumpling due to its lower hardness and Young⿿s modulus, while the severer rumpling behaviour in turn increased the scale spallation tendency and Al depletion rate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Martensite in NiAl oxidation-resistant coatings10.1007/BF02662758 ↗
2. A study of hot corrosion behaviour of NiAl coatings in an aggressive environment10.4028/www.scientific.net/SSP.226.177 ↗
3. Surface and interface segregation in β-NiAl with and without Pt addition10.1016/j.scriptamat.2005.10.065 ↗
4. Progress in coatings for gas turbine airfoils10.1016/S0257-8972(98)00667-7 ↗
5. Materials design for the next generation thermal barrier coatings10.1146/annurev.matsci.33.011403.113718 ↗
6. The role of Cr and Si in affecting high-temperature oxidation behaviour of minor Dy doped NiAl alloys10.1016/j.corsci.2013.08.020 ↗
7. Improved oxide scale adherence of low-Pt/Hf co-doped β-NiAlCrSi coating on superalloy IC21 at 1200°C10.1016/j.corsci.2016.01.005 ↗
8. Effect of Si content on cyclic hot corrosion of NiAl in fused Na2SO4-NaCl mixture10.2320/jinstmet1952.57.5_533 ↗
9. Effect of Pt on the High temperature stability of NiCoCrAlY or NiAl bond coat in the thermal barrier coating system10.3740/MRSK.2005.15.6.375 ↗
10. Effect of Mo Ta, and Re on high-temperature oxidation behavior of minor Hf doped β-NiAl alloy10.1016/j.corsci.2015.10.011 ↗
11. Pt and Hf additions to NiAl bond coats and their effect on the lifetime of thermal barrier coatings10.4028/www.scientific.net/MSF.426-432.209 ↗
12. The oxidation and rumpling behavior of overlay B2 bond coats containing Pt, Pd Cr and Hf10.1016/j.surfcoat.2013.01.021 ↗
13. Synthesis and cyclic oxidation behavior of a (Ni,Pt)Al coating on a desulfurized Ni-base superalloy10.1007/s11661-999-0308-1 ↗
14. Examination of the platinum effect on the oxidation behavior of nickel⿿aluminide coatings10.1016/j.surfcoat.2007.06.013 ↗
15. Influence of Pt on the metal⿿oxide interface during high temperature oxidation of NiAl bulk materials10.1016/j.corsci.2008.12.016 ↗
16. Oxidation behavior of platinum⿿aluminum alloys and the effect of Zr doping10.1557/JMR.1999.0615 ↗
17. Thermal cycling behaviour of EB-PVD TBCs on CVD platinum modified aluminide coatings10.1016/j.jallcom.2015.02.177 ↗
18. Microstructure and high temperature oxidation behavior of Pt-modified aluminide bond coats on Ni-base superalloys10.1016/j.pmatsci.2012.08.002 ↗
19. α-NiPt(Al) and phase equilibria in the Ni⿿Al⿿Pt system at 1150°C10.1016/j.actamat.2005.03.046 ↗
20. A combined first-principles and experimental study of the lattice site preference of Pt in B2 NiAl10.1016/j.actamat.2004.12.038 ↗
21. Investigation of the microstructure of platinum-modified aluminide coatings10.1016/j.surfcoat.2004.12.019 ↗
22. Effect of composition on the oxidation and hot corrosion resistance of NiAl doped with precious metals10.1016/S0257-8972(00)00878-1 ↗
23. Effects of platinum on the hot corrosion behavior of Hf-modified γ'-Ni3Al+γ-Ni-based alloys10.1007/s11085-011-9251-9 ↗
24. Effect of aluminisation characteristics on the microstructure of single phase β-(Ni,Pt)Al coating and the isothermal oxidation behaviour10.1016/j.corsci.2016.01.024 ↗
25. Temperature and cycle-time dependence of rumpling in platinum-modified diffusion aluminide coatings10.1016/j.scriptamat.2007.06.031 ↗
26. Rumpling induced by thermal cycling of an overlay coating: the effect of coating thickness10.1016/j.actamat.2003.10.001 ↗
27. Influence of bond coat thickness on the cyclic rumpling of thermally grown oxides10.1016/j.actamat.2005.12.008 ↗
28. Martensitic transformation in CVD NiAl and (Ni,Pt)Al bond coatings10.1016/S0257-8972(02)00585-6 ↗
29. Preparation and hot corrosion behaviour of an Al-gradient NiCoCrAlYSiB coating on a Ni-base superalloy10.1016/j.corsci.2009.01.003 ↗
30. Microstructures and cyclic oxidation behaviour of Pt-free and low-Pt NiAl coatings on the Ni-base superalloy Rene-8010.1016/j.corsci.2011.10.037 ↗
31. Mechanistic aspects of Pt-modified β-NiAl alloy oxidation10.3184/096034009X463907 ↗
32. Oxidation behavior of simple and Pt-modified aluminide coatings on IN738 at 1100°C
33. Influence of sulfur platinum, and hafnium on the oxidation behavior of CVD NiAl bond coatings10.1023/A:1020525123056 ↗
34. Rumpling of platinum modified aluminide coatings during thermomechanical testing10.4028/www.scientific.net/MSF.595-598.51 ↗
35. Experimental investigation of the bond-coat rumpling instability under isothermal and cyclic thermal histories in thermal barrier systems10.1098/rspa.2003.1262 ↗
36. Effect of temperature on rumpling and thermally grown oxide stress in an EB-PVD thermal barrier coating10.1016/j.surfcoat.2006.07.212 ↗
37. An analytical model of rumpling in thermal barrier coatings10.1016/j.jmps.2004.11.002 ↗
38. Bond coat surface rumpling in thermal barrier coatings10.1016/S1359-6454(02)00395-6 ↗
39. Microstructural and microchemical development of simple and Pt-modified aluminide diffusion coatings during long term oxidation at 1050°C10.1016/S0257-8972(03)00767-9 ↗
40. Oxide adhesion and growth characteristics on platinum-modified aluminide coatings10.1016/0257-8972(87)90098-3 ↗
41. Effect of Dy on oxide scale adhesion of NiAl coatings at 1200°C10.1016/j.corsci.2011.03.003 ↗
42. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
43. Characterization of alumina scales grown on a 2nd generation single crystal Ni superalloy during isothermal oxidation at 1050, 1100 and 1150°C10.1007/s11085-014-9487-2 ↗
44. Characterization of alumina scales formed during isothermal and cyclic oxidation of plasma-sprayed TBC systems at 1150°C10.1023/A:1018870923397 ↗
45. 18O/SIMS Characterization of the growth mechanism of doped and undoped α-Al2O310.1007/BF00665610 ↗
46. Effect of co-doping of two reactive elements on alumina scale growth of β-NiAl at 1200°C10.1016/j.corsci.2014.07.036 ↗
47. Ta effect on oxidation of a nickel-based single-crystal superalloy and its sputtered nanocrystalline coating at 900⿿1100°C10.1016/j.apsusc.2015.03.157 ↗
48. Improved Cr2O3 adhesion by Ce ion implantation in the presence of interfacial sulfur segregation10.1016/j.actamat.2006.07.047 ↗
49. On the kinetics of the pack⿿aluminization process10.1007/BF02656589 ↗
50. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
51. Grain-boundary nickel diffusion in NiAl intermetallic compound
52. Short-circuit diffusion in NiAl alloys10.1016/S0966-9795(97)00049-6 ↗
53. Direct molecular dynamics observations of bulk and grain boundary diffusion in NiAl10.4028/www.scientific.net/DDF.213-215.83 ↗
54. Atomistic theory and computer simulation of grain boundary structure and diffusion
55. On the rumpling mechanism in nickel-aluminide coatings: part II: characterization of surface undulations and bond coat swelling
56. On the initiation of cyclic oxidation-induced rumpling of platinum-modified nickel aluminide coatings10.1016/j.actamat.2008.12.015 ↗
57. Pilling-bedworth ratio for oxidation of alloys10.1007/s100190050008 ↗
58. Thermal barrier coating adherence to Hf-modified B2 NiAl bond coatings10.1016/j.actamat.2014.07.033 ↗
59. Plastic deformation of fine-grained alumina (Al2O3): II, Basal slip and nonaccommodated grain-boundary sliding10.1111/j.1151-2916.1980.tb10649.x ↗
60. Deformation of fine-grained alumina by grain boundary sliding accommodated by slip10.1016/S1359-6454(03)00180-0 ↗