Influence of microstructure and manganese sulfides on corrosion resistance of selective laser melted 17-4 PH stainless steel in acidic chloride medium
Source abstract
Abstract
The corrosion resistance of 17-4PH stainless steel obtained by Selective Laser Melting was investigated. It was found that the as-built SLM-ed steel was entirely ferritic, not martensitic as expected. Re-austenitized SLM-ed steel recovered the martensitic microstructure. The two SLM-ed steels (as-built and re-austenitized) had the same general corrosion resistance which was correlated with their similar chemical composition. The martensitic re-austenitized SLM-ed steel had superior general corrosion behavior than the wrought martensitic steel. This was due to the nearly absence of MnS inclusions in the re-austenitized SLM-ed steel, while their presence in the wrought steel destabilized the passive film.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (74)
Show source-provided references
1. 1994 · 3
2. Aging reactions in a 17-4 PH stainless steel10.1016/S0254-0584(01)00460-6 ↗
3. Study on the microstructure and mechanical properties of 17-4 PH stainless steel depending on heat treatment and aging time10.4028/www.scientific.net/SSP.118.15 ↗
4. Effects of aging on the microstructure of 17-4 PH stainless steel10.1016/0025-5416(88)90420-X ↗
5. Effect of microstructure on pitting and corrosion fatigue of 17-4 PH turbine blade steel in chloride environments10.5006/1.3577350 ↗
6. Pitting corrosion of cold rolled solution treated 17-4 PH stainless steel10.1016/j.corsci.2013.11.039 ↗
7. Localised corrosion behaviour of 17–4 PH stainless steel
8. Pitting and sulfide inclusion in steel10.1016/S0010-938X(74)80047-8 ↗
9. Studies by auger spectroscopy of pit initiation at the site of inclusions in stainless steel10.1016/0010-938X(90)90047-9 ↗
10. Inclusions in stainless steels − a review10.1002/srin.201700130 ↗
11. The initiation of pitting corrosion at MnS inclusions10.1016/0010-938X(93)90279-P ↗
12. Pit initiation at single sulfide inclusions in stainless steel10.1149/1.1474430 ↗
13. Elucidation of a trigger mechanism for pitting corrosion of stainless steels using submicron resolution scanning electrochemical and photoelectrochemical microscopy10.1149/1.1838697 ↗
14. Surface analysis of corrosion pits initiated at MnS inclusions in 304 stainless steel10.1149/1.2069458 ↗
15. The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions10.1016/0010-938X(92)90074-D ↗
16. Microelectrochemical measurements of the dissolution of single MnS inclusions, and the prediction of the critical conditions for Pit Initiation on stainless steel10.1149/1.1360205 ↗
17. Explanation for initiation of pitting corrosion of stainless steels at sulfide inclusions10.1149/1.1393431 ↗
18. Stainless-steel corrosion and MnS inclusions10.1038/424389b ↗
19. High-resolution characterization of the region around manganese sulfide inclusions in stainless steel alloys10.5006/1.3287741 ↗
20. Cavitation erosion and pitting corrosion of laser surface melted stainless steels10.1016/S0257-8972(97)00624-5 ↗
21. Influence of high power diode laser surface melting on the pitting corrosion resistance of type 316L stainless steel10.1023/A:1016569527098 ↗
22. Additive manufacturing: technology, applications and research needs10.1007/s11465-013-0248-8 ↗
23. Progress in additive manufacturing and rapid prototyping10.1016/S0007-8506(07)63240-5 ↗
24. Fabrication of metal and alloy components by additive manufacturing: examples of 3D materials science10.1016/S2238-7854(12)70009-1 ↗
25. Highly anisotropic steel processed by selective laser melting10.1007/s11663-013-9875-z ↗
26. Texture and anisotropy in selective laser melting of NiTi alloy10.1016/j.msea.2015.10.032 ↗
27. Microstructure and mechanical behavior of 17-4 precipitation hardenable steel processed by selective laser melting10.1007/s11665-014-1226-y ↗
28. Additive manufacturing of 17-4 PH stainless steel: post-processing heat treatment to achieve uniform reproducible microstructure10.1007/s11837-015-1754-4 ↗
29. Evidence of austenite by-passing in a stainless steel obtained from laser melting additive manufacturing
30. On the enhanced corrosion resistance of a selective laser melted austenitic stainless steel10.1016/j.scriptamat.2017.07.037 ↗
31. Corrosion behavior of additively manufactured 316L stainless steel in acidic media
32. Excellent mechanical and corrosion properties of austenitic stainless steel with a unique crystallographic lamellar microstructure via selective laser melting10.1016/j.scriptamat.2018.09.017 ↗
33. Influence of postbuild microstructure on the electrochemical behavior of additively manufactured 17-4 PH stainless steel10.1007/s11837-016-2237-y ↗
34. Corrosion properties of powder bed fusion additively manufactured 17-4 PH stainless steel10.5006/2365 ↗
35. Solid state phase transformations at very high temperature in a martensitic stainless steel
36. Energy of lattice distortion
37. Energy of lattice distortion in cold worked permalloy10.1103/PhysRev.52.613 ↗
38. A method for the monitoring of metal recrystallization based on the in-situ measurement of the elastic energy release using neutron diffraction10.1063/1.4919414 ↗
39. Larson · 1994
40. EXPGUI, a graphical user interface for GSAS10.1107/S0021889801002242 ↗
41. Iterative determination of the orientation relationship between austenite and martensite from a large amount of grain pair misorientations10.1007/s11661-016-3462-2 ↗
42. Effect of heat treatments on microstructural evolution of additively manufactured and wrought 17-4PH stainless steel10.1016/j.matdes.2018.07.015 ↗
43. Effect of powder chemical composition on the as-built microstructure of 17-4 PH stainless steel processed by selective laser melting
44. Neutron diffraction in situ monitoring of the dislocation density during martensitic transformation in a stainless steel10.1016/j.scriptamat.2012.11.031 ↗
45. Neutron-diffraction line broadening in a tempered martensitic steel for fusion reactors10.1016/S0921-4526(97)00841-7 ↗
46. Austenite content and dislocation density in electron-beam welds of a stainless maraging steel10.1016/0921-5093(95)10047-4 ↗
47. Malik · 1993
48. Baroux · 2014
49. Metallography of pitting corrosion10.1016/1044-5803(92)90015-A ↗
50. Influence of the microstructure on the corrosion behaviour of low-carbon martensitic stainless steel after tempering treatment10.1016/j.corsci.2014.03.036 ↗
51. Preparation and electrochemical corrosion behavior of bulk nanocrystalline ingot iron in HCl acid solution10.1021/jp046297v ↗
52. Microstructure and corrosion properties of ultrafine-grained interstitial free steel10.1016/j.msea.2005.11.081 ↗
53. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
54. Effect of hydrostatic extrusion on passivity breakdown on 303 austenitic stainless steel in chloride solution10.1007/s10008-007-0488-9 ↗
55. Effect of surface mechanical attrition treatment on corrosion behavior of 316 stainless steel10.1016/S1006-706X(09)60030-3 ↗
56. SVET, AFM and AES study of pitting corrosion initiated on MnS inclusions by microinjection10.1016/S0010-938X(02)00222-6 ↗
57. Influence of the chemical dissolution of MnS inclusions on the electrochemical behavior of stainless steels10.1149/1.1924172 ↗
58. Effect of sulfur content of copper-containing austenitic stainless steels on corrosion behavior in concentrated sulfuric acid—part 210.5006/1.3278486 ↗
59. The role of molybdenum in the dissolution and the passivation of stainless steels with adsorbed sulphur10.1016/0010-938X(92)90150-2 ↗
60. The influence of sulphur on the dissolution and the passivation of a nickel-iron alloy—I. Electrochemical and radiotracer measurements10.1016/0010-938X(84)90012-X ↗
61. Role of adsorbed sulphur in the dissolution and passivation of nickel and nickel-sulphur alloys10.1016/0378-5963(79)90060-6 ↗
62. Initiation of pitting at sulfide inclusions in stainless steel10.1149/1.2401840 ↗
63. Improvement of pitting corrosion resistance of type 316L stainless steel by potentiostatic removal of surface MnS inclusions10.1155/2012/482730 ↗
64. Improvement of pitting corrosion resistance of type 430 stainless steel by electrochemical treatments in a concentrated nitric acid10.2355/isijinternational.54.199 ↗
65. Correlation between corrosion potential and pitting potential for AISI 304L austenitic stainless steel in 3.5% NaCl aqueous solution10.1590/S1516-14392002000100013 ↗
66. Evaluation of 316L stainless steel corrosion resistance in solution simulating the acid hydrolysis of biomass10.1149/1.3554728 ↗
67. The X-ray photoelectron spectra of MnS, MnSe, and MnTe10.1016/0022-4596(78)90107-X ↗
68. Phase-dependent structural and electrochemical properties of single crystalline MnS thin films deposited by DC reactive sputtering10.1063/1.5053875 ↗
69. The role of thiosulfates in the pitting corrosion of Fe-17Cr alloys in neutral chloride solution: electrochemical and XPS study10.1016/S0010-938X(97)81158-4 ↗
70. EIS and XPS studies on passive film of AISI 304 stainless steel in dilute sulfuric acid solution: passive film of AISI 304 stainless steel10.1002/sia.3819 ↗
71. The antagonistic roles of chromium and sulphur in the passivation of Ni-Cr-Fe alloys studied by XPS and radiochemical techniques10.1016/0010-938X(90)90134-Q ↗
72. Analysis of mineral surface chemistry in flotation separation using imaging XPS10.1016/j.mineng.2006.08.006 ↗
73. SO2 adsorption at room temperature on Ni(111) surface studied by XPS10.1002/sia.1821 ↗
74. Comparative XPS analyses of passive layers composition formed on Duplex 2205 SS after standard and high-current-density electropolishing