journal article·2023-11

Microstructural evolution and corrosion mechanism of micro-alloyed 2024 (Zr, Sc, Ag) aluminum alloys

Pan Deng, Wenfeng Mo, Zuoqiong Ouyang, Kai Ling, Binghui Luo, Zhenhai Bai

Corrosion Science· Volume 224
Publisher page

Abstract

The 2024 aluminum alloy has excellent mechanical and low corrosion due to the existence of the high Cu levels, which shortens its service life. In this paper, we have systematically investigated the mechanism of the influence of three elements (Sc, Zr, and Ag) on the microstructure and corrosion behavior of 2024 aluminum alloy after microalloying. The results showed that microalloying treatment of 2024 aluminum alloy reduced the dendritic spacing of cast aluminum alloy ; decreased the sizes of Cu-rich intermetallic particles (Cu-IMPs) within the peak aging of the T6 alloy to make their distribution more uniform; and changed the grain boundary phases (GBPs) and precipitate-free zones (PFZs) width of the T6 alloy. Microalloying treatment significantly changed the corrosion resistance of the alloy. Both Zr and Ag elements significantly improved the corrosion resistance of the alloy and reduced IGC depth and electrochemical corrosion rate, however, the Sc elements deteriorated the corrosion resistance of the alloy. Moreover, the corrosion mechanism of the alloy was also discussed in detail.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. Structural relationship between one-dimensional crystals of Guinier–Preston–Bagaryatsky zones in Al–Cu–Mg alloys10.1016/j.scriptamat.2011.01.033 ↗
2. Precipitation hardening in Al–Cu–Mg alloys revisited10.1016/j.scriptamat.2005.09.010 ↗
3. The effect of silver on microstructural evolution in two 2xxx series Al-alloys with a high Cu:Mg ratio during ageing to a T8 temper10.1016/j.msea.2008.03.014 ↗
4. Double-atomic-wall-based dynamic precipitates of the early-stage S-phase in AlCuMg alloys10.1016/j.actamat.2012.08.023 ↗
5. Role of vacancy–solute complex in the initial rapid age hardening in an Al–Cu–Mg alloy10.1016/S1359-6454(00)00348-7 ↗
6. The structure and the properties of S-phase in AlCuMg alloys10.1016/j.actamat.2011.08.009 ↗
7. In situ structural characterization of ageing kinetics in aluminum alloy 2024 across Angstrom-to-micrometer length scales10.1016/j.actamat.2016.03.058 ↗
8. The coexistence of two S (Al2CuMg) phases in Al–Cu–Mg alloys10.1016/j.actamat.2012.08.044 ↗
9. Recent advances in the development of aerospace materials10.1016/j.paerosci.2018.01.001 ↗
10. Multiple twins of a decagonal approximant embedded in S-Al2CuMg phase resulting in pitting initiation of a 2024Al alloy10.1016/j.actamat.2014.09.001 ↗
11. Microstructure and corrosion of AA202410.1515/corrrev-2014-0039 ↗
12. Corrosion of AA2024-T3 Part I: localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
13. Effect of Zr on microstructures and mechanical properties of an AlMgSiCuCr alloy prepared by low frequency electromagnetic casting10.1016/j.matchar.2014.02.013 ↗
14. Comparison of microstructure and mechanical properties of Al-Mg-Li-Sc-Zr alloys processed by ingot metallurgy and rapid solidification10.1016/j.jallcom.2021.160937 ↗
15. A novel rheological high pressure die-casting process for preparing large thin-walled Al–Si–Fe–Mg–Sr alloy with high heat conductivity, high plasticity and medium strength10.1016/j.msea.2020.139040 ↗
16. Conventional stir casting versus ultrasonic assisted stir casting process: mechanical and physical characteristics of AMCs10.1016/j.jallcom.2019.07.076 ↗
17. The effect of interrupted aging on the yield strength and uniform elongation of precipitation-hardened Al alloys10.1016/j.actamat.2013.06.036 ↗
18. Effects of retrogression and re-aging treatment on precipitation behavior, mechanical and corrosion properties of a Zr+Er modified Al-Zn-Mg-Cu alloy
19. The effect of stress-aging on dimensional stability behavior of Al-Cu-Mg alloy10.1016/j.jallcom.2017.05.183 ↗
20. Effect of non-isothermal ageing on microstructure and mechanical properties of an Al–Cu–Mg–Ag alloy10.1016/j.msea.2021.142315 ↗
21. Effects of non-isothermal aging on mechanical properties, corrosion behavior and microstructures of Al-Cu-Mg-Si alloy10.1016/j.jallcom.2019.152960 ↗
22. Microstructural evolution and strengthening mechanisms operating during cryogenic rolling of solutionized Al-Cu-Mg alloy10.1016/j.msea.2018.12.103 ↗
23. Effect of equal-channel angular pressing routes on high-strain-rate deformation behavior of ultra-fine-grained aluminum alloy10.1016/j.actamat.2009.12.041 ↗
24. Homogenization of ECAPed Al 2024 alloy through age-hardening10.1016/j.msea.2012.08.148 ↗
25. Application of hot forming cold die quenching for facilitating equal channel angular pressing of AA2024 aluminum alloy10.1016/j.jallcom.2019.03.059 ↗
26. Plastic deformation of 2024-T351 aluminum plate over a wide range of loading conditions10.1016/j.ijsolstr.2013.02.006 ↗
27. Influence of a microalloying addition of Ag on the precipitation kinetics of an Al–Cu–Mg alloy with high Mg:Cu ratio10.1016/j.actamat.2015.07.032 ↗
28. Effects of Cu/Mg ratio on the microstructure, mechanical and corrosion properties of Al-Li-Cu-Mg-X alloys10.1016/j.msea.2018.01.118 ↗
29. Comparison of corrosion resistance of the AA2524-T3 and the AA2024-T310.3390/met11060980 ↗
30. The influence of Sc solute partitioning on the microalloying effect and mechanical properties of Al-Cu alloys with minor Sc addition10.1016/j.actamat.2016.08.013 ↗
31. The effect of Cu and Sc on the localized corrosion resistance of Al-Zn-Mg-X alloys10.1016/j.jallcom.2019.05.189 ↗
32. Effect of minor Sc and Zr on recrystallization behavior and mechanical properties of novel Al–Zn–Mg–Cu alloys10.1016/j.jallcom.2015.10.122 ↗
33. Mechanical properties and corrosion behaviors of (Sc, Zr) modified Al-Cu-Mg alloy10.1016/j.matchar.2022.112619 ↗
34. Effect of V additions on the microstructure and mechanical properties of Al-Cu-Mg-Ag alloy
35. Highly stable coherent nanoprecipitates via diffusion-dominated solute uptake and interstitial ordering
36. Effect of Mn/Mo incorporated oxide layer on the corrosion behavior of AA 2024 alloy10.1016/j.corsci.2011.08.016 ↗
37. Understanding the corrosion behavior by passive film evolution in Zn-containing Al-Si-Cu cast alloy10.1016/j.corsci.2022.110468 ↗
38. Effect of Sc and Zr additions on corrosion behaviour of Al–Zn–Mg–Cu alloys10.1016/j.jallcom.2014.05.128 ↗
39. Effect of Zr content on corrosion behavior and chemically-milled surface roughness of Al-Cu-Mg alloy10.1016/j.jallcom.2023.171364 ↗
40. Effect of minor Ge addition on microstructure and localized corrosion behavior of Al-Zn-Mg alloy sheet10.1016/j.matchar.2019.109837 ↗
41. Isotropy of precipitate distribution in pre-stretched Al-Cu-(Sc)-(Zr) alloys10.1016/j.scriptamat.2021.114452 ↗
42. Improvement of high temperature strength of 2219 alloy by Sc and Zr addition through a novel three-stage heat treatment route10.1016/j.msea.2018.07.003 ↗
43. The influence of Sc and Zr additions on microstructure and corrosion behavior of AA5182 alloy sheet10.1016/j.corsci.2022.110181 ↗
44. Effects of Sc and Zr microalloying additions and aging time at 120°C on the corrosion behaviour of an Al–Zn–Mg alloy10.1016/j.corsci.2012.08.024 ↗
45. Effects of Sc and Zr microalloying additions on the recrystallization texture and mechanism of Al–Zn–Mg alloys10.1016/j.jallcom.2013.06.020 ↗
46. Co-stabilization of θ′-Al2Cu and Al3Sc precipitates in Sc-microalloyed Al–Cu alloy with enhanced creep resistance
47. Precipitation of Al3Zr by two-step homogenization and its effect on the recrystallization and mechanical property in 2195 Al–Cu–Li alloys10.1016/j.msea.2021.141637 ↗
48. Effect of zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
49. Effect of trace amounts of added Sc on microstructure and mechanical properties of 2055 aluminum alloy10.1016/j.matchar.2018.04.041 ↗
50. Experimental and numerical analysis of toughness anisotropy in AA2139 Al-alloy sheet10.1016/j.actamat.2009.04.046 ↗
51. On the role of Ag additions on the initial solute hardening and competitive precipitation of Al-Cu-Mg alloys10.1016/j.jallcom.2023.169339 ↗
52. Effect of Ag additions on the lengthening rate of Ω plates and formation of σ phase in Al-Cu-Mg alloys during thermal exposure10.1016/j.matchar.2016.11.008 ↗
53. Trace element effects on precipitation in Al–Cu–Mg–(Ag, Si) alloys: a computational analysis10.1016/j.actamat.2004.04.021 ↗
54. Electrochemical characteristics of intermetallic phases in aluminum alloys10.1149/1.1869984 ↗
55. Effect of trace Zn addition on microstructure and corrosion behavior of AA2024 under different aging treatments10.1016/j.matchar.2022.112440 ↗
56. Simultaneous improvement in corrosion resistance and hardness of a model 2xxx series Al-Cu alloy with the microstructural variation caused by Sc and Zr additions10.1016/j.corsci.2019.108095 ↗
57. Effects of Sc alloying on the evolution of solidification microstructure and formation of W phase in as-cast 2519 aluminum alloys10.1016/j.jallcom.2021.162764 ↗
58. Quantifying the effects of Sc and Ag on the microstructure and mechanical properties of Al–Cu alloys
59. The nano-structural characterization of Ω and S phases in Al-5.1Cu-1.0 Mg-(0.4Ag) AA2024 aluminum alloys10.1016/j.msea.2023.145361 ↗
60. Effect of Sc and Zr on microstructure and chemical milling surface roughness of 2024-T6 alloy sheets10.1016/j.matchemphys.2022.126815 ↗
61. Effects of precipitates versus solute atoms on the deformation-induced grain refinement in an Al–Cu–Mg alloy10.1016/j.msea.2019.138486 ↗
62. Improving the corrosion resistance of MgZn1.2Gd Zr0.18 (x = 0, 0.8, 1.4, 2.0) alloys via Gd additions10.1016/j.corsci.2020.108962 ↗
63. Corrosion resistance of a two-stage stress-aged Al–Cu–Mg alloy: Effects of external stress10.1016/j.jallcom.2015.11.173 ↗
64. Corrosion resistance of a two-stage stress-aged Al–Cu–Mg alloy: effects of stress-aging temperature10.1016/j.jallcom.2015.10.114 ↗
65. A novel bilayer system comprising LDH conversion layer and sol-gel coating for active corrosion protection of AA202410.1016/j.corsci.2018.08.039 ↗
66. A burnished and Al-alloyed magnesium surface with improved mechanical and corrosion properties10.1016/j.corsci.2021.109395 ↗
67. On the corrosion of a high solute Al-Zn-Mg alloy produced by laser powder bed fusion10.1016/j.corsci.2021.109626 ↗
68. The effect of dry/wet ratios on the corrosion process of the 6061 Al alloy in simulated Nansha marine atmosphere10.1016/j.corsci.2022.110840 ↗
69. Pitting of 2024 alloys prepared by spark plasma sintering using powders with different sizes10.1016/j.corsci.2020.108525 ↗
70. Effect of high-temperature furnace treatment on the microstructure and corrosion behavior of NiCrBSi flame-sprayed coatings10.1016/j.corsci.2014.07.057 ↗
71. Temperature dependent lattice misfit and coherency of Al3X (X = Sc, Zr, Ti and Nb) particles in an Al matrix10.1016/j.actamat.2015.02.004 ↗
72. Effect of Sc addition on the microstructures and age-hardening behavior of an Al Cu Mg Ag alloy10.1016/j.msea.2019.04.045 ↗
73. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
74. The intergranular corrosion susceptibility of 2024 Al alloy during re–ageing after solution treating and cold–rolling10.1016/j.corsci.2016.11.013 ↗
75. Corrosion-induced mechanical properties degradation of Al-Cu-Li (2198-T351) aluminium alloy and the role of side-surface cracks10.1016/j.corsci.2021.109330 ↗