Experimental and thermodynamic investigations on the chlorine-induced corrosion of HVOF thermal sprayed NiAl coatings and 304 stainless steels at 700 °C

Mingwen Bai, Liam Reddy, Tanvir Hussain

Corrosion Science· Volume 135

Abstract

Alumina-forming β-NiAl coatings were deposited by high velocity oxy-fuel (HVOF) thermal spraying onto 304 stainless steels for protection against chlorine induced corrosion in a biomass-fired boiler. The corrosion test was conducted in a synthetic gas containing 500 ppm HCl with 10 wt% KCl ash deposit at 700 °C for 250 h. Severe corrosion was observed with the fast growing alumina at the coating/substrate interface initiating from sample edges. Possible corrosion mechanism was proposed: as supplied by HCl/KCl, the formation of volatile chlorine/chloride acted as a catalyst and promoted the growth of alumina at relatively lower application temperatures (<900 °C).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Thermal and Kinetic Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Biomass combustion in fluidized bed boilers: potential problems and remedies10.1016/j.fuproc.2008.07.012 ↗
2. Potential applications of renewable energy sources, biomass combustion problems in boiler power systems and combustion related environmental issues10.1016/j.pecs.2005.02.002 ↗
3. Performance testing of iron based thermally sprayed HVOF coatings in a biomass-fired fluidised bed boiler10.1016/j.surfcoat.2014.04.025 ↗
4. Oxide scale growth and presumed exfoliation in a 700°C or higher steam condition: a simulation study for future operations of ultra-supercritical power plants10.1016/j.supflu.2014.06.002 ↗
5. Development of advanced ultra supercritical fossil power plants in Japan: materials and high temperature corrosion properties10.4028/www.scientific.net/MSF.696.236 ↗
6. Investigations on the behavior of HVOF and cold sprayed Ni-20Cr coating on T22 boiler steel in actual boiler environment10.1007/s11666-011-9698-x ↗
7. Corrosion testing of Ni alloy HVOF coatings in high temperature environments for biomass applications10.1007/s11666-012-9820-8 ↗
8. Microstructural characteristics of high-velocity oxygen-fuel (HVOF) sprayed nickel-based alloy coating10.1016/j.jallcom.2013.07.109 ↗
9. The erosion–corrosion behaviour of high velocity oxy-fuel (HVOF) thermally sprayed inconel-625 coatings on different metallic surfaces10.1016/j.surfcoat.2005.08.143 ↗
10. Effects of thermal spray coating composition and microstructure on coating response and substrate protection at high temperatures10.5006/1.3292116 ↗
11. Microstructural characterization of high velocity oxy-fuel sprayed coatings of Inconel 62510.1023/A:1018589230250 ↗
12. Fireside corrosion behavior of HVOF and plasma-sprayed coatings in advanced coal/biomass co-fired power plants10.1007/s11666-013-9887-x ↗
13. Nickel-based HVOF coatings promoting high temperature corrosion resistance of biomass-fired power plant boilers10.1016/j.fuproc.2014.04.006 ↗
14. High temperature corrosion of coatings and boiler steels in reducing chlorine-containing atmosphere10.1016/S0257-8972(02)00472-3 ↗
15. Deposition and high temperature corrosion in a 10 MW straw fired boiler10.1016/S0378-3820(97)00062-3 ↗
16. In‐situ corrosion investigation at Masnedø CHP plant?a straw‐fired power plant10.1002/(SICI)1521-4176(199910)50:10<579::AID-MACO579>3.0.CO;2-M ↗
17. Lab-scale investigations of high-temperature corrosion phenomena in straw-fired boilers10.1021/ef990001g ↗
18. Synergistic effect of NaCl and water vapor on the corrosion of 1Cr-11Ni-2W-2Mo-V steel at 500–700C10.1023/A:1018854202982 ↗
19. KCl-induced high temperature corrosion of the austenitic Fe–Cr–Ni alloys 304L and Sanicro 28 at 600°C10.1016/j.corsci.2005.05.018 ↗
20. The effects of KCl, K2SO4 and K2CO3 on the high temperature corrosion of a 304-type austenitic stainless steel10.1007/s11085-011-9240-z ↗
21. A comparison of the oxidation behaviours of Al 2 O 3 formers and Cr 2 O 3 formers at 700 C–oxide solid solutions acting as a template for nucleation10.1016/j.corsci.2007.12.012 ↗
22. Oxidation of FeCrAl alloys at 500–900C in dry O210.1002/maco.200503882 ↗
23. High temperature interaction of Al/Si-modified Fe-Cr alloys with KCl10.1016/j.corsci.2006.10.019 ↗
24. KCl-induced corrosion of an FeCrAl alloy at 600C in O2+ H2O environment: the effect of pre-oxidation10.1007/s11085-014-9507-2 ↗
25. A microstructural and kinetic investigation of the KCl-induced corrosion of an FeCrAl alloy at 600°C10.1007/s11085-015-9546-3 ↗
26. Corrosion behaviour of various model alloys with NaCl?KCl coating10.1016/j.matchemphys.2005.03.015 ↗
27. Advances in coating design for high-performance gas turbines10.1557/mrs2003.194 ↗
28. Laser clad and HVOF-sprayed stellite 6 coating in chlorine-rich environment with KCl at 700°C10.1007/s11085-017-9776-7 ↗
29. HVOF and laser-cladded Fe–Cr–B coating in simulated biomass combustion: microstructure and fireside corrosion10.1007/s11085-017-9774-9 ↗
30. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700C10.1016/S0010-938X(99)00142-0 ↗
31. Modelling of phase diagrams and thermodynamic properties using Calphad method −development of thermodynamic databases10.1016/j.commatsci.2012.02.003 ↗
32. Saunders · 1998
33. Lukas · 2007
34. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
35. The development and validation of a new thermodynamic database for Ni-based alloys10.7449/2012/Superalloys_2012_803_812 ↗
36. Thermodynamic calculations in the development of high-temperature Co–Re-based alloys10.1016/j.jallcom.2013.07.055 ↗
37. Influence of oxygen partial pressure in sintering atmosphere on properties of Cr–Mo prealloyed powder metallurgy steel10.1179/174329007X205073 ↗
38. Microstructural evolution of a MCrAlY coating upon isothermal annealing10.1016/j.matchar.2008.03.011 ↗
39. Thermodynamic investigation into the equilibrium phases in the NiCoCrAl system at elevated temperatures10.1016/j.surfcoat.2010.09.009 ↗
40. Investigation into the effects of Fe additions on the equilibrium phase compositions, phase fractions and phase stabilities in the Ni–Cr–Al system10.1016/j.actamat.2009.10.059 ↗
41. Phase stabilities in a NiCrAlYRe coating alloy10.1016/j.surfcoat.2011.11.021 ↗
42. Phase constituents and thermal expansion behavior of a NiCrAlYRe coating alloy10.1007/s10853-010-4953-y ↗
43. Microstructural evolution of a NiCoCrAlY coating on an IN100 substrate10.1016/j.surfcoat.2004.06.014 ↗
44. Modelling of phase equilibria in MCrAlY coating systems10.1016/j.surfcoat.2004.02.018 ↗
45. A prominent driving force for the spallation of thermal barrier coatings: chemistry dependent phase transformation of the bond coat10.1016/j.actamat.2017.06.037 ↗
46. Roine · 2002
47. High-temperature oxidation of FeCr (Ni) alloys: the behaviour after Breakaway10.1007/s11085-017-9731-7 ↗
48. Capability of thermodynamic calculation in the development of alloys for deposition of corrosion-protection coatings via thermal spraying10.1002/maco.200704056 ↗
49. Chloridation-oxidation of nine commercial high-temperature alloys at 800°C10.1007/BF02153465 ↗
50. Mixed Oxidation of Iron–Chromium Alloys in Gases Containing Oxygen and Chlorine at 900–1200°K10.5006/1.3585177 ↗
51. The effects of chlorides, hydrogen-chloride, and sulfur-dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
52. Corrosion of high alloy steels and Fe-Cr-alloys beneath deposits from waste incinerator plants10.4028/www.scientific.net/MSF.251-254.527 ↗
53. A surface analytical approach to the high temperature chlorination behaviour of inconel 600 at 700C10.1016/S0010-938X(96)00112-6 ↗
54. Corrosion behavior of Fe (Ni) CrAIX alloys in an HCl- h 2 O- H 2 gas mixture at 800°C10.1007/BF01046895 ↗
55. Investigations of the degradation of high-temperature alloys in a potentially oxidizing-chloridizing gas mixture10.1007/BF00665491 ↗
56. High-temperature chloridation of binary Fe Cr alloys at 1000°C10.1016/0921-5093(89)90719-3 ↗
57. Accelerated oxidation of chromium by trace of sodium chloride vapor10.2320/matertrans1989.32.969 ↗
58. Ignition of nickel in environments containing oxygen and chlorine10.1007/BF02668559 ↗
59. Influence of H2O (g) on the oxide microstructure of the stainless steel 353MA at 900°C in oxygen10.1149/1.2768909 ↗
60. The influence of KCl on the corrosion of an austenitic stainless steel (304L) in oxidizing humid conditions at 600C: a microstructural study10.1007/s11085-009-9156-z ↗
61. An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe–2. 25 Cr–1Mo steel at 400C10.1016/j.corsci.2011.03.007 ↗
62. Oxidation of binary FeCr alloys (Fe–2. 25 Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2+ H2O environment at 600C10.1007/s11085-010-9229-z ↗
63. Oxidation of Fe–10Cr in o 2 and in o 2+ H 2 O environment at 600C: a microstructural investigation10.1016/j.corsci.2013.06.016 ↗
64. Microstructural investigation of the HCl-induced corrosion of the austenitic alloy 310S (52Fe26Cr19Ni) at 500C10.1007/s11085-013-9468-x ↗
65. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
66. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600C10.1016/j.corsci.2005.08.012 ↗
67. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe–Cr and Fe–Cr–X alloys10.1007/s11085-010-9215-5 ↗
68. The effect of H2 and H2O on the oxidation of 304L-stainless steel at 600°C: general behaviour (part I)10.1007/s11085-015-9597-5 ↗
69. Diffusion in oxides10.2138/rmg.2010.72.17 ↗
70. Point defects and cation tracer diffusion in (CrxFe1- x) 3- δO4 spinels10.1016/0167-2738(95)00190-H ↗
71. Spallation and transient oxide growth on PWA 1484 superalloy10.1016/j.msea.2008.01.043 ↗
72. Compositional factors affecting the establishment and maintenance of Al2O3 scales on Ni–Al–Pt systems10.1007/s10853-009-3251-z ↗
73. Oxidation of NiAl and FeAl10.1016/S0966-9795(99)00037-0 ↗