journal article·2011-06

An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe–2.25Cr–1Mo steel at 400 °C

T. Jonsson, N. Folkeson, J.-E. Svensson, L.-G. Johansson, M. Halvarsson

Corrosion Science· Volume 53· Issue 6
Publisher page

Abstract

The initial oxidation of a low-alloyed steel (Fe-2.25Cr-1Mo) in the presence of small amounts of KCl(s) have been investigated through ESEM in situ exposure and analysis at 400 degrees C. The samples were also characterized by XRD, SEM/EDX and FIB. The present study shows the corrosive nature of KCl towards the low alloyed steel. It is concluded that the initial KCl distribution is important and that a KCl/FeCl2 liquid phase film forms on large parts of the oxide surface in the presence of KCl. It is proposed that Cl increases the oxidation rate (by decorating oxide grain boundaries) and decreases the oxide scale adhesion. (C) 2011 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Kofstad · 1988
2. N. Birks, H. Meier, Introduction to the High Temperature Oxidation of Metals, second ed., Cambridge University Press, London, 2006.10.1017/CBO9781139163903 ↗
3. Critical corrosion phenomena on superheaters in biomass and waste-fired boilers10.1016/S1006-706X(08)60048-5 ↗
4. T. Jonsson, J. Pettersson, K. Davidsson, L.-G. Johansson, J.-E. Svensson, Sewage sludge as additive to reduce the initial fireside corrosion caused by combustion of shredder residues in a waste-fired BFB boiler, in: Ninth Liège Conference on Materials for Advanced Power Engineering, Liege, 2010.
5. The Implications of Chlorine-associated Corrosion on the Operation of Biomass-fired Boilers10.1016/S0360-1285(00)00003-4 ↗
6. A surface analytical approach to the high temperature chlorination behaviour of inconel 600 at 700°C10.1016/S0010-938X(96)00112-6 ↗
7. Local reactions of KCl particles with iron, nickel and chromium surfaces10.1002/maco.200503903 ↗
8. The effects of chlorides, hydrogen-chloride, and sulfur-dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
9. Acceleration of the high temperature oxidation of metals by chlorine, high temperature corrosion
10. The influence of alloying elements on the chlorine-induced high temperature corrosion of Fe–Cr alloys in oxidizing atmospheres10.1002/(SICI)1521-4176(199910)50:10<561::AID-MACO561>3.0.CO;2-L ↗
11. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700°C10.1016/S0010-938X(99)00142-0 ↗
12. Accelerated corrosion of pure Fe, Ni, Cr and several Fe-based alloys induced by ZnCl2–KCl at 450°C in oxidizing environment10.1016/S0921-5093(02)00386-6 ↗
13. KCl-induced high temperature corrosion of the austenitic Fe–Cr–Ni alloys 304L and Sanicro 28 at 600°C10.1016/j.corsci.2005.05.018 ↗
14. The influence of small amounts of KCl(s) on initial stages of the corrosion of alloy Sanicro 28 at 600°C10.1007/s11085-008-9118-x ↗
15. J. Pettersson, J.E. Svensson, L.G. Johansson, Alkali induced corrosion of 304-type austenitic stainless steel at 600°C; comparison between KCl, K2CO3 and K2SO4, in: P. Steinmetz, I.G. Wright, A. Galerie, D. Monceau, S. Mathieu (Eds.), Seventh International Symposium on High Temperature Corrosion and Protection of Materials, Les Embiez, France, 2008, pp. 367–375.
16. The influence of KCl on the corrosion of an austenitic stainless steel (304L) in oxidizing humid conditions at 600°C: a microstructural study10.1007/s11085-009-9156-z ↗
17. T. Jonsson, J. Froitzheim, J. Pettersson, J.-E. Svensson, L.-G. Johansson, M. Halvarsson, Microstructural investigation of the influence of KCl on the corrosion of 304L exposed to 5% O2+N2, in: 16th International Corrosion Congress, Beijing, China, 2005.
18. Microstructural investigation of the KCl-induced corrosion of the austenitic alloy Sanicro 28 (35Fe27Cr31Ni) at 600°C10.3184/096034009X464339 ↗
19. N. Folkeson, T. Jonsson, M. Halvarsson, L.-G. Johansson, J.-E. Svensson, The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe–2.25Cr–1Mo steel at 400 and 500°C, Materials and Corrosion, n/a, doi:10.1002/maco.201005942.10.1002/maco.201005942 ↗
20. In situ scanning electron microscopy and electron backscatter diffraction investigation on the oxidation of pure iron10.3184/096034005782744092 ↗
21. High-temperature oxidation of iron and the decay of Wüstite studied with in situ ESEM10.1023/A:1013346813454 ↗
22. In situ ESEM investigations of the oxide growth on hot work tools: effect of the water vapour10.3184/096034003782750105 ↗
23. An ESEM in situ investigation of the influence of H2O on iron oxidation at 500°C10.1016/j.corsci.2009.05.016 ↗
24. Evidence for the suppression of the oxidation of a Fe 2.25Cr 1 Mo steel by traces of SO210.4028/www.scientific.net/MSF.369-372.173 ↗
25. A quantitative demonstration of the grain-boundary diffusion mechanism for the oxidation of metals10.1080/01418618208239905 ↗
26. Review of the high-temperature oxidation of iron and carbon steels in air or oxygen10.1023/A:1023685905159 ↗
27. C. Gleave, J.M. Calvert, D.G. Lees, P.C. Rowlands, A study of the mechanism of corrosion of some ferritic steels in high-pressure carbon dioxide with the aid of oxygen-18 as a tracer. II. High-silicon mild steel, in: R. Soc. Mathematical, Physical and Engineering Sciences, London, 1982, pp. 429–438.10.1098/rspa.1982.0024 ↗
28. The effect of traces of SO2 on iron oxidation: a microstructural study10.1007/s11085-007-9051-4 ↗
29. Void formation in magnetite scale formed on iron at 823K – elucidation by chemical potential distribution
30. N. Bertrand, C. Desgranges, D. Gauvain, D. Monceau, D. Poquillon, p. trans tech, Low temperature oxidation of pure iron: growth kinetics and scale morphologies, in: P. Steinmetz, I.G. Wright, G. Meier, A. Galerie, B. Pieraggi, R. Podor (Eds.), High Temperature Corrosion and Protection of Materials 6, Prt 1 and 2, Proceedings, Trans Tech Publications Ltd., Zurich-Uetikon, 2004, pp. 591–598.10.4028/www.scientific.net/MSF.461-464.591 ↗
31. Oxidation of iron at 400–600°C in dry and wet O210.1016/j.corsci.2010.01.002 ↗
32. Oxidation of binary FeCr alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2+H2O environment at 600°C10.1007/s11085-010-9229-z ↗
33. Point-defects and cation tracer diffusion in (CRXFE1-X)(3-DELTA)O-4 spinels10.1016/0167-2738(95)00190-H ↗
34. Levin · 1964
35. The vapor-pressures of hydroxides. 1. The alkali hydroxides KOH and CSOH10.1016/0021-9614(88)90214-5 ↗
36. Initial stages of the HCl-induced high-temperature corrosion of alloy 31010.1149/1.2754174 ↗