Formation of an incombustible oxide film on a molten Mg-Al-Ca alloy
Source abstract
Abstract
A nonflammable Mg-10Al-5Ca (at.%) alloy that can be melted in air without a cover gas or flux is developed. The alloy immediately forms a protective oxide film consisting of three layers, a fine CaO outer layer, a fine MgO intermediate layer, and a coarse MgO innermost layer. The anionic volume ratio of the CaO/MgO interface is 1.48. This interface ratio is sufficiently large to suggest the generation of a strong compressive force in the CaO layer. The dense, uniform fine CaO layer may act as a protective layer preventing the diffusion of oxygen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Weight Loss with Magnesium Alloys10.1126/science.1182848 ↗
2. Marker · 2013
3. Overcoming barriers of magnesium ignition and flammability
4. Controlling the ignition and flammability of magnesium for aerospace applications10.1016/j.corsci.2014.04.047 ↗
5. The ignition temperature of Mg alloys WE43, AZ31 and AZ9110.1016/j.corsci.2011.09.004 ↗
6. Influence of Al and Y on the ignition and flammability of Mg alloys10.1016/j.corsci.2011.10.014 ↗
7. Oxidation characteristics of magnesium alloys10.1007/s11837-012-0477-z ↗
8. Improving aluminum castings with beryllium
9. Beryllium in aluminum and magnesium alloys
10. A new approach to magnesium die casting
11. Behavior of surface oxidation on molten Mg–9Al–0.5Zn–0.3Be alloy10.1016/S0921-5093(00)01798-6 ↗
12. Oxidation resistance of Mg–9Al–1Zn alloys micro-alloyed with Be10.1016/j.scriptamat.2015.12.022 ↗
13. Effects of Ca and Be addition on high temperature oxidation behavior of AZ91 alloys10.4028/www.scientific.net/MSF.419-422.639 ↗
14. Flame-resistant magnesium alloys by calcium
15. Suppression of ignition and burning of molten Mg alloys by Ca bearing stable oxide film10.1023/A:1018526708423 ↗
16. The effect of calusium additions on the oxidation behavior in magnesium alloys10.1016/S1359-6462(00)00344-4 ↗
17. Effect of Ca addition on the oxidation resistance of AZ91 magnesium alloys at elevated temperatures10.1007/BF03027194 ↗
18. Effect of Ca and Y additions on oxidation behavior of AZ91 alloy at elevated temperatures10.1016/S1003-6326(08)60268-X ↗
19. Effect of CaO and hot extrusion on the oxidation of AZ61 magnesium alloys10.1007/s11085-015-9579-7 ↗
20. Effects of Al and Y additions on the oxidation behavior of Mg-Ca base molten alloys10.4028/www.scientific.net/MSF.419-422.581 ↗
21. Effect of yttrium, calcium and zirconium on ignition-proof principle and mechanical properties of magnesium alloys10.1016/S1002-0721(10)60642-4 ↗
22. Surface oxidation behavior of Mg-Y-Ce alloys at high temperature10.1007/s11661-005-0155-7 ↗
23. Early oxidation behaviors of Mg–Y alloys at high temperatures10.1016/j.jallcom.2007.06.065 ↗
24. Oxidation behavior of ignition-proof magnesium alloys with rare earth addition10.1016/j.jallcom.2010.10.168 ↗
25. Effects of Ca addition on the microstructure and mechanical properties of AZ91magnesium alloy10.1023/A:1017927109291 ↗
26. Effect of substituting cerium-rich mischmetal with lanthanum on high temperature properties of die-cast Mg-Zn-Al-Ca-RE alloys10.1016/j.msea.2004.03.039 ↗
27. Effects of Ca and Sr addition on mechanical properties of a cast AZ91 magnesium alloy at room and elevated temperature10.1016/j.msea.2005.05.028 ↗
28. Precipitation strengthening of a Mg-Al-Ca–Based AXJ530 die-cast alloy10.1007/s11661-007-9455-4 ↗
29. Effect of Zr addition on the mechanical properties of as-extruded Mg-Zn-Ca-Zr alloys10.1016/j.msea.2009.12.024 ↗
30. Extruded Mg–Zn–Ca–Mn alloys with low yield anisotropy10.1016/j.msea.2012.08.012 ↗
31. High strength nanocrystalline Mg-Al-Ca alloys produced by rapidly solidified powder metallurgy processing10.4028/www.scientific.net/MSF.350-351.111 ↗
32. Flame-resistant magnesium alloys with high strength
33. Solidification paths and eutectic intermetallic phases in Mg-Al-Ca ternary alloys10.1016/j.actamat.2005.03.001 ↗
34. Characterization of Mg-rich clusters in the C36 phase of the Mg-5Al-3Ca-0.7Sr-0.2Mn alloy10.1016/j.jallcom.2014.02.029 ↗
35. Thermodynamic property of CaO-MgO-Al2O3 melts10.2205/2011NZ000230 ↗
36. The oxidation behavior of an AZ91D magnesium alloy at high temperatures10.1016/S1359-6454(02)00094-0 ↗
37. effect of Ca and Y additions on oxidation behavior of AZ91D alloy at elevated temperatures10.1016/S1003-6326(08)60268-X ↗
38. Phase equilibria in the system CaO-MgO10.1111/j.1151-2916.1963.tb11737.x ↗
39. Reducibility of oxides and sulphides in metallurgical processes
40. Knacke · 1991
41. Model for nonprotective oxidation of AI-Mg alloys10.1007/BF00664426 ↗
42. Nucleation and growth of Al2O3/metal composites by oxidation of aluminum alloys10.1557/JMR.1991.1964 ↗
43. The oxidation of metals at high temperatures
44. High-temperature oxidation
45. The observation of stress effects during the high temperature oxidation of iron10.1007/BF00540812 ↗