Corrosion behavior of Sn-3.0Ag-0.5Cu alloy under chlorine-containing thin electrolyte layers

Bokai Liao, Hongyu Cen, Zhenyu Chen, Xingpeng Guo

Corrosion Science· Volume 143
Publisher page

Abstract

Abstract Corrosion behavior of Sn-3.0Ag-0.5Cu lead-free solder alloy under chlorine-containing thin electrolyte layers is studied. The emphasis is laid on discussion about influences of addition of alloying elements, concentration of chloride ion and thickness of electrolyte layer on its corrosion behavior. Results indicate that: mainly local corrosion occurs to the alloy; Existence of intermetallic compounds and β-Sn crystal boundary facilitates the process of Cl− infiltration into the base and galvanic corrosion. Metal ions are accumulated in pitting corrosion region, and hydrolysis of metallic ions promotes the solution acidification and transverse development of pitting corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Investigations on microhardness of Sn–Zn based lead-free solder alloys as replacement of Sn–Pb solder10.1016/j.jallcom.2004.08.079 ↗
2. Mechanism of passivation of Pb(Ca)–Sn alloys in sulfuric acid: role of tin10.1016/S0013-4686(99)00186-3 ↗
3. Recent advances of conductive adhesives as a lead-free alternative in electronic packaging: materials, processing, reliability and applications10.1016/j.mser.2006.01.001 ↗
4. Investigations of interfacial reactions of Sn–Zn based and Sn–Ag–Cu lead-free solder alloys as replacement for Sn–Pb solder10.1016/j.jallcom.2005.03.053 ↗
5. Microstructural evolution of Sn–9Zn–3Bi solder/Cu joint during long-term aging at 170°C10.1016/j.jallcom.2004.03.124 ↗
6. Effects of composition and reflowing on the corrosion behavior of Sn–Zn deposits in brine media10.1016/j.electacta.2005.11.031 ↗
7. Electronics without lead10.1126/science.1110168 ↗
8. A reliability model for SAC solder covering isothermal mechanical cycling and thermal cycling conditions10.1016/j.microrel.2009.08.008 ↗
9. Effect of 9wt.% in addition to Sn3. 5Ag0. 5Cu solder on the interfacial reaction with the Au/NiP metallization on Cu pads10.1016/j.jallcom.2005.01.001 ↗
10. Electrochemical corrosion behaviour of Pb-free Sn–8.5Zn–0.05Al–XGa and Sn–3Ag–0.5Cu alloys in chloride containing aqueous solution10.1016/j.corsci.2008.06.042 ↗
11. Electrochemical corrosion study of Sn–3Ag–3Cu solder alloy in NaCl solution10.1016/j.electacta.2009.07.030 ↗
12. Microstructure, corrosion behaviour and microhardness of a directionally solidified Sn–Cu solder alloy10.1016/j.electacta.2011.07.114 ↗
13. Electrochemical mechanism of atmospheric rusting10.1038/206980a0 ↗
14. The role of Zn precipitates and Cl− anions in pitting corrosion of Sn–Zn solder alloys10.1016/j.corsci.2014.12.014 ↗
15. Electrochemical migration, whisker formation, and corrosion behavior of printed circuit board under wet H2S environment10.1016/j.electacta.2013.10.051 ↗
16. A study of the corrosion of aluminum alloy 2024-T3 under thin electrolyte layers10.1016/j.corsci.2003.10.005 ↗
17. Pitting corrosion mechanism of stainless steels under wet-dry exposure in chloride-containing environments10.1016/S0010-938X(97)00124-8 ↗
18. Corrosion behaviour of copper under chloride-containing thin electrolyte layer10.1016/j.corsci.2011.06.004 ↗
19. The corrosion of tin under thin electrolyte layers containing chloride10.1016/j.corsci.2012.08.040 ↗
20. Concerning trend removal in electrochemical noise measurements10.1016/S0010-938X(00)00064-0 ↗
21. Effects of intermetallic compounds on properties of Sn–Ag–Cu lead-free soldered joints10.1016/S0925-8388(02)01166-0 ↗
22. Design of lead-free candidate alloys for low-temperature soldering applications based on the hypoeutectic Sn–6.5Zn alloy10.1016/j.matdes.2013.11.064 ↗
23. Lasia · 2014
24. Characterization of pitting corrosion of 7A60 aluminum alloy by EN and EIS techniques10.1016/S1003-6326(14)63550-0 ↗
25. Corrosion characterization of new tin–silver binary alloys in nitric acid solutions10.1016/j.corsci.2008.02.003 ↗
26. Influence of electrolyte layer thickness and pH on the initial stage of the atmospheric corrosion of iron10.1149/1.1837578 ↗
27. Dependence of the corrosion behavior of aluminum alloy 7075 on the thin electrolyte layers10.1016/j.mseb.2009.01.003 ↗
28. Pitting corrosion of rheocast A356 aluminium alloy in 3.5 wt.% NaCl solution10.1016/j.corsci.2013.04.023 ↗
29. Potentiodynamic polarization behaviour of AISI type 316 stainless steel in NaCl solution10.1016/j.corsci.2013.04.028 ↗
30. The influence of the cathodic process on the interpretation of electrochemical noise signals arising from pitting corrosion of stainless steels10.1016/j.corsci.2009.12.021 ↗
31. Initiation and repassivation of pitting corrosion of carbon steel in carbonated concrete pore solution10.1016/j.corsci.2010.12.028 ↗
32. XPS study of the surface chemistry of L-CVD SnO2 thin films after oxidation10.1016/j.tsf.2005.04.014 ↗
33. Some X-ray photoelectron spectroscopic measurements on Passivated Tin in some neutral media10.1002/mawe.19880190904 ↗
34. Characterisation of anodic layers on Cu–10Sn bronze (RDE) in aerated NaCl solution10.1016/j.corsci.2008.06.003 ↗
35. Angular distribution of electrons in ESCA spectra from a single crystal10.1088/0031-8949/1/5-6/017 ↗
36. Impact of 5% NaCl Salt Spray Pretreatment on the Long-Term Reliability of Wafer-Level Packages with Sn-Pb and Sn-Ag-Cu Solder Interconnects10.1007/s11664-011-1705-y ↗
37. Corrosion behaviour assessment of lead-free Sn–Ag–M (M = In, Bi, Cu) solder alloys10.1016/j.matchemphys.2007.12.006 ↗
38. The Role of Intermetallics on the Corrosion Initiation of Twin Roll Cast AZ31 Mg Alloy10.1149/2.0291509jes ↗
39. Corrosion resistance of WE43 and AZ91D magnesium alloys with phosphate PEO coatings10.1016/j.corsci.2008.03.002 ↗
40. Electrochemical behavior and localized corrosion associated with Al7Cu2Fe particles in aluminum alloy 7075-T65110.1016/j.corsci.2006.02.007 ↗
41. Pitting corrosion of metals - A review of the critical factors10.1149/1.1838615 ↗
42. The nature of crevice corrosion of aluminum in chloride solutions10.1002/maco.19880390304 ↗
43. Stochastic modeling of pitting corrosion: a new model for initiation and growth of multiple corrosion pits10.1016/j.corsci.2006.05.049 ↗
44. Exploration of the effect of chloride ion concentration and temperature on pitting corrosion of carbon steel in saturated Ca(OH)2 solution10.1016/j.corsci.2015.06.010 ↗
45. Passivity breakdown, pit initiation and propagation of pits in metallic materials – review10.1016/j.corsci.2014.10.006 ↗
46. The comparative breakdown of passivity of tin by fluorides and chlorides interpreted through the’ law of matching affinities’ concept10.1016/j.corsci.2015.02.012 ↗
47. The role of Cu-based intermetallics on the pitting corrosion behavior of Sn-Cu, Ti-Cu and Al-Cu alloys10.1016/j.electacta.2012.05.106 ↗
48. Initial stage of pitting corrosion of type 304 stainless steel under thin electrolyte layers containing chloride ions10.1149/1.1992470 ↗
49. Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions10.1016/j.corsci.2006.08.016 ↗
50. The corrosion of tin in nearly neutral solutions10.1039/tf9373301152 ↗
51. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
52. Pitting corrosion of metals10.1149/2.F03101if ↗
53. Corrosion characterization of tin–lead and lead free solders in 3.5 wt.% NaCl solution10.1016/j.corsci.2007.11.025 ↗
54. Corrosion and leaching behaviors of Sn-based alloy in simulated soil solutions10.1016/S1003-6326(16)64146-8 ↗
55. The effect of alloying element gallium on the polarization characteristics of Pb-free Sn–Zn–Ag–Al–XGa solders in NaCl solution10.1016/j.corsci.2005.02.003 ↗