Abstract
Abstract The hot corrosion behavior of a Ni-based single-crystal (SC) superalloy treated by laser shock peening (LSP) against 75 wt.% Na2SO4+25 wt.% NaCl molten salts at 750 °C was studied. The results showed that LSP improved the hot corrosion resistance of the SC superalloy. This was attributed to significantly different LSP-induced dislocation structures in γ/γ′ phases, which promoted the formation of protective layered oxide films that inhibited the inward diffusion of corrosive media. In addition, the hot corrosion mechanism of LSP-treated SC superalloy was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Residual Stress · High-Temperature Coating Behaviors · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. A review of composition evolution in Ni-based single crystal superalloys10.1016/j.jmst.2020.01.026 ↗
2. Influence of the alloying element Re on the ideal tensile and shear strength of γ′-Ni3Al10.1016/j.scriptamat.2009.03.042 ↗
3. The iron effect on hot corrosion behaviour of MCrAlX coating in the presence of NaCl at 900 ℃10.1016/j.jallcom.2019.152381 ↗
4. Influences of solution cooling on microstructures, mechanical properties and hot corrosion resistance of a Ni-based superalloy10.1016/j.msea.2019.01.015 ↗
5. Microstructure and hot corrosion behavior of Co–Si modified aluminide coating on nickel based superalloys10.1016/j.corsci.2015.08.011 ↗
6. Improved hot corrosion resistance of plasma sprayed YSZ/Gd2Zr2O7 thermal barrier coating over single layer YSZ10.1016/j.matchar.2018.11.007 ↗
7. A review on failure mechanism of thermal barrier coatings and strategies to extend their life time10.1016/j.ceramint.2019.12.200 ↗
8. Severe hot corrosion of the superalloy IN718 in mixed salts of Na2SO4 and V2O5 at 700 ℃10.1007/s11665-018-3501-9 ↗
9. Effect of surface modification on the hot corrosion resistance of Inconel 718 at 700 °C
10. The effect of near-surface plastic deformation on the hot corrosion and high temperature corrosion-fatigue response of a Ni-based superalloy10.1016/j.jallcom.2020.154889 ↗
11. Microstructure and hot corrosion behavior of the Ni-based superalloy GH202 treated by laser shock processing10.1016/j.matchar.2017.01.021 ↗
12. Microstructure and hot corrosion of GH2036 alloy treated by laser shock peening10.1007/s11837-019-03857-2 ↗
13. Laser shock peening enhanced corrosion properties in a nickel based Inconel 600 superalloy10.1016/j.jallcom.2016.10.093 ↗
14. High temperature erosion behaviour of Type AISI 446 stainless steel under the combined effect of surface modification and pre hot-corrosion10.1016/j.engfailanal.2020.104873 ↗
15. Effect of laser shock peening on microstructure and hot corrosion of TC11 alloy10.1016/j.surfcoat.2017.12.003 ↗
16. Surface nano-hardness and microstructure of a single crystal nickel base superalloy after laser shock peening10.1016/j.optlastec.2016.12.032 ↗
17. Surface topography evolution of Ni-based single crystal superalloy under laser shock: formation of the nano-scale surface reliefs
18. Effect of laser shock on tensile deformation behavior of a single crystal nickel-base superalloy10.1016/j.msea.2017.01.039 ↗
19. Nonuniformity of morphology and mechanical properties on the surface of single crystal superalloy subjected to laser shock peening10.1016/j.jallcom.2015.10.238 ↗
20. Physical study of laser-produced plasma in confined geometry10.1063/1.346783 ↗
21. Comparison of mechanisms of advanced mechanical surface treatments in nickel-based superalloy10.1016/j.msea.2013.04.021 ↗
22. Effect of microstructure evolution and phase precipitations on hot corrosion behavior of IN718 alloy subjected to multiple laser shock peening10.1016/j.surfcoat.2019.04.060 ↗
23. Prediction modeling of Type-I hot corrosion performance of Ti-Al-Mo-X (X=Cr, Mn) alloys in (Na, K)2SO4 molten salt mixture environment at 900 °C10.1016/j.jallcom.2020.156010 ↗
24. Evolutions of microstructure, phase, microhardness, and residual stress of multiple laser shock peened Ni-based single crystal superalloy after short-term thermal exposure
25. Formation of omega phase induced by laser shock peening in Ti-17 alloy10.1016/j.matchar.2019.110017 ↗
26. Microstructure characteristics and formation mechanism of TC17titanium alloy induced by laser shock processing10.1016/j.jallcom.2017.06.127 ↗
27. Engineering Materials handbook Council · 1989
28. Experimental investigation on recrystallization mechanism of a Ni-base single crystal superalloy10.1016/j.jallcom.2016.02.149 ↗
29. Effects of long-term aging on the microstructures and tensile properties of Ni-Based single crystal superalloy10.1016/S1875-5372(15)30116-8 ↗
30. Structural evolution of topologically closed packed phase in a Ni-based single crystal superalloy10.1016/j.actamat.2019.12.014 ↗
31. Effects of Ta on microstructural stability and mechanical properties of hot corrosion resistant Ni-based single crystal superalloys during long-term thermal exposure10.1016/j.msea.2021.140829 ↗
32. Effect of ruthenium on the precipitation of topologically close packed phases in Ni-based superalloys of 3rd and 4th generation10.1016/j.actamat.2015.05.033 ↗
33. Effect of Hf on stress rupture properties of DD6 single crystal superalloy after long term aging10.1016/S1006-706X(12)60115-0 ↗
34. Oxidation behavior of a single-crystal Ni-base superalloy between 900 and 1000°C in air10.1016/j.jallcom.2009.10.261 ↗
35. Oxidation behavior of a single-crystal Ni-based superalloy over the temperature range of 850 °C–950 °C in air10.1016/j.apsusc.2019.04.089 ↗
36. Salt induced corrosion behaviour of superalloy IN718
37. Microstructural and compositional design of Ni-based single crystalline superalloys-A review10.1016/j.jallcom.2018.01.224 ↗
38. High cycle fatigue behavior of a single crystal superalloy at elevated temperatures10.1016/j.msea.2006.11.045 ↗
39. Influence of alloying elements on hot corrosion resistance of nickel-based single crystal superalloys coated with Na2SO4 salt at 900 °C10.1016/j.matdes.2020.109197 ↗
40. Hot corrosion behavior of super alloys
41. Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys10.1016/j.corsci.2017.01.011 ↗
42. Hot corrosion behavior of silicide coating on an Nb-Ti-Si based ultrahigh temperature alloy10.1016/j.corsci.2014.10.053 ↗
43. Evaluation of the hot corrosion behavior of Inconel 625 coatings on the Inconel 738 substrate by laser and TIG cladding techniques10.1016/j.optlastec.2018.09.011 ↗