Initial microzonal corrosion mechanism of inclusions associated with the precipitated (Ti, Nb)N phase of Sb-containing weathering steel
Source abstract
Abstract
Abstract In this work, the effects of combined inclusions and precipitates on the initiation and propagation of pits in weathering steel were studied. The SKPFM results showed that the precipitated (Ti, Nb)N phases had the highest Volta potential, followed by that of the matrix. The inclusions had the lowest potential. The corrosion initiation and propagation processes were observed, in situ, at the site of the combined inclusion and precipitate; the matrix around the precipitated phase dissolved slowly. When inclusions were in contact with the matrix, they rapidly dissolved, forming pits. Subsequently, the surrounding matrix dissolved rapidly, causing the pits to expand.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Five-year atmospheric corrosion of Cu, Cr and Ni weathering steels in a wide range of environments10.1016/j.corsci.2018.06.039 ↗
2. Development and prospect of weathering steels
3. Qi · 1989
4. Glad · 1997 · 47
5. Precipitation harding in metals10.1179/026708399773002782 ↗
6. Mocroalloyed strip steels for the 21st
7. Development and technological advancement of niobium containing steel
8. Application of vanadium-nitrogen microalloyed technology in HSLA steel
9. Development of low alloy steel and microalloyed steel
10. Computer model for prediction of carbonitride precipitation during hot working in Nb-Ti bearing HSLA steels10.2355/isijinternational.32.283 ↗
11. Effects of nanosized Nb carbide precipitates on the corrosion behavior of high-strength low-alloy steel in simulated seawater10.20964/2017.09.35 ↗
12. The effect of nanosized NbC precipitates on electrochemical corrosion behavior of high-strength low-alloy steel in 3.5%NaCl solution10.1016/j.ijhydene.2017.03.087 ↗
13. Effect of nanosized NbC precipitates on hydrogen diffusion in X80 pipeline steel10.3390/ma10070721 ↗
14. Effect of Nb element on corrosion behavior of welding heat affect zone of X80 steel in simulated seawater
15. A transmission electron microscopy study of microscopic causes for localized-corrosion morphology variations in the AA7055 Al alloy10.1016/j.jmst.2018.05.006 ↗
16. Investigating the effect of Cu-rich phase on the corrosion behavior of Super 304H austenitic stainless steel by TEM10.1016/j.corsci.2017.11.001 ↗
17. Influence of aging treatment on the pitting behavior associated with the dissolution of active nanoscale β-phase precipitates for an Al–Mg alloy10.1016/j.corsci.2015.11.026 ↗
18. Detection and analysis of anodic current transients associated with nanoscale β-phase precipitates on an Al–Mg microelectrode10.1016/j.corsci.2015.03.001 ↗
19. The use of local electrochemical probes and surface analysis methods to study the electrochemical behaviour and pitting corrosion of stainless steels10.1016/j.electacta.2007.01.079 ↗
20. Use of the electrochemical microcell technique and the SVET for monitoring pitting corrosion at MnS inclusions10.1016/j.elecom.2004.05.001 ↗
21. Eff ;ect of MnS inclusion dissolution on carbon steel stress corrosion cracking in fuel-grade ethanol10.1016/j.corsci.2015.03.002 ↗
22. The eff ;ect of microstructure and non-metallic inclusions on corrosion behavior of low carbon steel in chloride containing solutions10.1016/j.corsci.2013.11.038 ↗
23. Microstructural characterization and corrosion performance of old railway girder bridge steel and modern weathering structural steel10.1016/j.corsci.2016.10.004 ↗
24. The combined eff ;ect of chemical and structural factors on pitting corrosion induced by MnS-(Cr, Mn, Al) O duplex inclusions
25. Eff ;ect of inclusions modified by rare earth elements (Ce, La) on localized marine corrosion in Q460NH weathering steel10.1016/j.corsci.2017.10.001 ↗
26. Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment10.1016/j.corsci.2018.04.007 ↗
27. Eff ;ect of MnS inclusion dissolution on carbon steel stress corrosion cracking in fuel-grade ethanol10.1016/j.corsci.2015.03.002 ↗
28. The eff ;ect of microstructure and non-metallic inclusions on corrosion behavior of low carbon steel in chloride containing solutions10.1016/j.corsci.2013.11.038 ↗
29. Pitting and sulphide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
30. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in NaCl solution10.5006/1837 ↗
31. Mechanism of MnS-mediated pit initiation and propagation in carbon steel in an anaerobic sulfidogenic media10.1016/j.corsci.2013.06.049 ↗
32. Pitting corrosion behavior in ad-vanced high strength steels10.1016/j.jallcom.2014.08.243 ↗
33. Influence of oxygen content on the inclusion formation and pitting corrosion resistance of hyper duplex stainless steels10.2320/matertrans.M2014164 ↗
34. Mechanism of (Mg, Al, Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
35. Eff ;ects of heat-treatment on the extent of chromium depletion and caustic corrosion resistance of Alloy 69010.1016/j.corsci.2006.05.043 ↗
36. The role of TiN inclusions in stress corrosion crack initiation for Alloy 690TT in high-temperature and high-pressure water10.1016/j.corsci.2009.11.015 ↗
37. Role of TiN inclusion on corrosion fatigue behavior of Alloy 690 steam generator tubes in borated and lithiated high temperature water10.1016/j.corsci.2014.07.059 ↗
38. Microstructure and properties of low manganese and niobium containing HIC pipeline steel10.1016/j.msea.2008.04.038 ↗
39. Microchemistry of Ti-carbonitrides and their role in the early stage of pit initiation of Alloy 60010.5006/1.3280673 ↗
40. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in NaCl solution10.5006/1837 ↗