journal article·2017-03

Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys

J.X. Chang, D. Wang, G. Zhang, L.H. Lou, J. Zhang

Corrosion Science· Volume 117
Publisher page

Abstract

Abstract Type-I hot corrosion behaviour of single crystal Ni-base superalloys with different Cr and Ta contents in sodium sulphate (Na 2 SO 4 ) at 900 °C and 950 °C in static air were investigated using the “deposit recoat” method. It was shown that, increasing corrosion temperature shortened the incubation period. Loss of hot corrosion resistance causing by Cr reduction cannot be compensated by increasing Ta content. The effect of Ta addition on hot corrosion resistance can be described by introducing the quantitative parameter Ta/Cr (wt.%) ratio. Interaction of Cr, Ta and temperature on hot corrosion behaviour was discussed in detail in the present paper.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Chapter 8. Corrosion by sulfur
2. Oxidation of Ni-Cr-Al alloys between 1000° and 1200°C10.1149/1.2407837 ↗
3. Role of sodium in accelerated oxidation phenomenon termed sulfidation10.1007/BF02813266 ↗
4. Relationship between relative oxide ion content of Na2SO4, presence of liquid-metal oxides and sulfidation attack10.1007/BF02665406 ↗
5. Mechanisms for the hot corrosion of nickel-base alloys10.1007/BF02649626 ↗
6. Effects of chromate and vanadate anions on the hot corrosion of preoxidized Ni by a thin fused Na2SO4 film at 900-degrees-C10.1149/1.2086437 ↗
7. Alloying effects on surface stability and creep strength of nickel based single crystal superalloys containing 12mass%Cr
8. Na2SO4-induced accelerated oxidation (hot corrosion) of nickel10.1007/BF02642794 ↗
9. Development of a new alloy for directional solidification of large industrial gas turbine blades
10. Design and development of hot corrosion-resistant nickel-base single-crystal superalloys by the d-electrons alloy design theory. 1. Characterization of the phase-stability10.1007/BF02646523 ↗
11. The development of the CMSX-11B and CMSX-11C alloys for industrial gas turbine application
12. Development of Ni base superalloy for industrial gas turbine10.7449/2004/Superalloys_2004_707_712 ↗
13. Evaluation of PWA1483 for large single crystal IGT blade applications
14. Reed · 2006
15. Mechanism of beneficial effect of tantalum in hot corrosion of nickel-base superalloys10.1149/1.2133502 ↗
16. Chemical-reactions involved in the initiation of hot corrosion of B-1900 and NASA-TRW VIA10.1149/1.2123928 ↗
17. Chemical-reactions involved in the initiation of hot corrosion of IN-73810.1149/1.2115455 ↗
18. Alloy design of Ni-based single crystal superalloys for the combination of strength and surface stability at elevated temperatures10.2355/isijinternational.43.1244 ↗
19. Influence of Ta content on hot corrosion behaviour of a directionally solidified nickel base superalloy10.1016/j.jallcom.2014.08.259 ↗
20. Role of tantalum in the hot corrosion of a Ni-base single crystal superalloy10.1016/j.corsci.2015.05.066 ↗
21. Oxidative vaporization kinetics of Cr2O3 in oxygen from 1000° to 1300°C10.1149/1.2401958 ↗
22. Effect of oxide volatilization on oxidation kinetics of Cr and Fe-Cr alloys10.1149/1.2424115 ↗
23. Chromium vaporization from high-temperature alloys I. Chromia-forming steels and the influence of outer oxide layers10.1149/1.2434690 ↗
24. Birks · 2006
25. Hot corrosion of coated and uncoated single crystal gas turbine materials10.1002/maco.200804130 ↗
26. Hot corrosion behaviour of Co modified NiAl coating on nickel base superalloys10.1016/j.corsci.2012.06.027 ↗
27. Hot corrosion behaviour and its mechanism of a new alumina-forming austenitic stainless steel in molten sodium sulphate10.1016/j.corsci.2013.08.003 ↗
28. Investigation of the mechanisms of Type-II hot corrosion of superalloy CMSX-410.1016/j.corsci.2013.11.048 ↗
29. Oxidation and hot corrosion behaviour of Al2O3/YSZ coatings prepared by cathode plasma electrolytic deposition10.1016/j.corsci.2016.03.017 ↗
30. Improved hot corrosion resistance of Dy-Co-modified aluminide coating by pack cementation process on nickel base superalloys10.1016/j.corsci.2016.09.011 ↗
31. Preparation and hot corrosion behaviour of Pt modified AlSiY coating on a Ni-based superalloy10.1016/j.corsci.2015.12.007 ↗
32. Nonstoichiometry and thermodynamics of chromium sulfides10.1149/1.2403666 ↗
33. Solubilities of Cr2O3 in fused Na2SO4 at 1200-K10.1149/1.2108648 ↗
34. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
35. Molten Salts 1
36. Oxidation of single crystal PWA 1483 at 950°C in flowing air10.1016/j.corsci.2008.06.033 ↗
37. Development of a diffusion mobility database for Ni-base superalloys10.1016/S1359-6454(01)00383-4 ↗
38. Die oxydationsgeschwindigkeit von nickel bei kleinen zusatzen von chrom und mangan – beitrag zur theorie des anlaufvorganges10.3891/acta.chem.scand.01-0547 ↗