Abstract The corrosion behavior of alumina-forming austenitic (AFA) 316 stainless steel (SS) and oxide dispersion strengthened (ODS) 316 SS in aerated supercritical water (SCW) at 650 °C/25 MPa was investigated. The results show that the weight gain curves of AFA and ODS 316 SS follow near-parabolic law. Both AFA and ODS 316 SS show higher corrosion resistance in SCW than normal 316 SS, which is because that Al-Cr rich oxide and Cr-rich oxide layer are formed on AFA and ODS 316 SS, respectively. The corrosion process and mechanism of AFA and ODS 316 SS are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
2. Corrosion of ferritic–martensitic steel HT9 in supercritical water10.1016/j.jnucmat.2006.07.010 ↗
3. Influence of dissolved oxygen content on corrosion of the ferritic–martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
4. Effect of nitrogen addition and test temperatures on elastic-plastic fracture toughness of SS316LN10.1016/j.proeng.2014.11.042 ↗
5. Environmentally assisted cracking of types 304L/316L/316NG stainless steel in 288 C Water10.5006/1.3582044 ↗
6. Characterization of microstructure and local deformation in 316NG weld heat-affected zone and stress corrosion cracking in high temperature water10.1016/j.corsci.2011.02.009 ↗
7. Oxidation of stainless steel 316 and nitronic 50 in supercritical and ultrasupercritical water10.1016/j.apsusc.2015.03.127 ↗
8. Corrosion of engineering materials in a supercritical water cooled reactor: characterization of oxide scales on alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
9. Oxidation of 316 stainless steel in supercritical water10.1016/j.corsci.2009.03.008 ↗
10. SCC susceptibility of type 316Ti stainless steel in supercritical water10.1016/j.jnucmat.2014.12.014 ↗
11. Preparation and properties of some ODS Fe-Cr-Al alloys10.1007/BF02646711 ↗
12. Radiation resistance and thermal creep of ODS ferritic steels10.1016/S0022-3115(01)00511-6 ↗
13. Perspective of ODS alloys application in nuclear environments10.1016/S0022-3115(02)01043-7 ↗
14. In situ observation of damage structure in ODS austenitic steel during electron irradiation10.1016/j.jnucmat.2010.12.156 ↗
15. The development of alumina-forming austenitic stainless steels for high-temperature structural use10.1007/s11837-008-0083-2 ↗
16. Creep-resistant Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
17. Alumina-forming austenitic stainless steels strengthened by laves phase and MC carbide precipitates10.1007/s11661-007-9319-y ↗
18. Alloying effects on creep and oxidation resistance of austenitic stainless steel alloys employing intermetallic precipitates10.1016/j.intermet.2007.12.005 ↗
19. Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels10.1007/s11661-009-9886-1 ↗
20. Corrosion of alumina-forming austenitic steel Fe-20Ni-14Cr-3Al-0.6Nb-0.1Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
21. Tem characterization of dispersoids and microstructure of ODS-316 austenitic steel10.3724/SP.J.1037.2012.00466 ↗
22. Microstructural evolution and mechanical properties of an Fe–18Ni–16Cr–4Al base alloy during aging at 950 °C10.1007/s12613-016-1240-1 ↗
23. Effects of minor alloy additions and oxidation temperature on protective alumina scale formation in creep-resistant austenitic stainless steels10.1016/j.scriptamat.2007.08.032 ↗
24. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗
25. A research on the corrosion and stress corrosion cracking susceptibility of 316L stainless steel exposed to supercritical water10.1016/j.corsci.2017.08.027 ↗
26. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C10.1016/j.corsci.2005.08.012 ↗
27. Localized corrosion of magnetite on ferritic–martensitic steels exposed to supercritical water10.1016/j.corsci.2009.08.021 ↗
28. Oxidation behavior of iron-based alloy HCM12A exposed in supercritical water10.1016/j.corsci.2005.10.010 ↗
29. Effects of exposure temperature and time on corrosion behavior of a ferritic–martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
30. Analyses of oxide films grown on AISI 304L stainless steel and incoloy 800HT exposed to supercritical water environment10.1016/j.jnucmat.2011.05.007 ↗
31. Surface film electrochemistry of austenitic stainless steel and its main constituents in supercritical water10.1016/j.supflu.2007.06.005 ↗
32. The characteristic of oxide scales on T91 tubeafter long-term service in an ultra-supercritical coal power plant10.1016/j.supflu.2012.08.015 ↗
33. Failure analysis of a boiler tube in USC coal power plant10.1016/j.engfailanal.2008.12.006 ↗
34. Corrosion phenomena induced by supercritical water in generation IV nuclear reactors
35. The corrosion and stress corrosion cracking behavior of a novel alumina-forming austenitic stainless steel in supercritical water10.1016/j.jnucmat.2016.10.039 ↗
36. The use of model alloys to develop corrosion-resistant stainless steels10.4028/www.scientific.net/MSF.461-464.815 ↗
37. Oxidation behavior of ferritic-martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
38. Corrosion behavior of a 14Cr-ODS steel in supercritical water10.1016/j.jnucmat.2013.02.002 ↗
39. Internal oxidation and crack susceptibility of alloy 310S stainless steel after long term exposure to supercritical water at 500 °C10.1016/j.supflu.2016.09.007 ↗