journal article·2022-11Open access

Hydrogen effects on passivation and SCC of 2205 DSS in acidified simulated seawater

Yue Pan, Baozhuang Sun, Zhiyong Liu, Wei Wu, Xiaogang Li

Corrosion Science· Volume 208

Abstract

In this work, hydrogen effects on passivation and stress corrosion cracking (SCC) of 2205 duplex stainless steel (DSS) in acidified seawater were investigated. Results show hydrogen deteriorates passive film, accelerates localized anodic dissolution (AD) and causes hydrogen damage, leading to high SCC susceptibility by hydrogen embrittlement (HE) and hydrogen facilitated anodic dissolution (HFAD). SCC initiates in ferrite, and propagates as transgranular-SCC (TGSCC) and intergranular-SCC (IGSCC). When loaded along rolling direction (RD), hydrogen segregating in austenite hardens austenite during SCC propagation; while hydrogen enriching in ferrite causes hydrogen enhanced localized plasticity (HELP) effect for transverse direction (TD) load.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Laboratory investigation of microbiologically influenced corrosion of 2205 duplex stainless steel by marine Pseudomonas aeruginosa biofilm using electrochemical noise10.1016/j.corsci.2018.08.018 ↗
2. Stress-assisted microbiologically influenced corrosion mechanism of 2205 duplex stainless steel caused by sulfate-reducing bacteria10.1016/j.corsci.2020.108746 ↗
3. A new study for healing pitting defects of 316L stainless steel based on microarc technology10.1016/j.corsci.2021.109505 ↗
4. The effect of ɳ-Ni3Ti precipitates and reversed austenite on the passive film stability of nickel-rich Custom 465 steel10.1016/j.corsci.2019.04.016 ↗
5. Effect of hydrogen charging on the stress corrosion behavior of 2205 duplex stainless steel under 3.5 wt% NaCl thin electrolyte layer10.1007/s11665-017-2713-8 ↗
6. Effect of hydrogen charging on SCC of 2205 duplex stainless steel with varying microstructures in simulated deep-sea environment10.1016/j.corsci.2021.110026 ↗
7. Effects of microstructural characteristics on the hydrogen embrittlement characteristics of austenitic, ferritic, and γ–α duplex stainless steels10.1016/j.msea.2021.140851 ↗
8. Stress corrosion cracking behavior and mechanism of Fe-Mn-Al-C-Ni high specific strength steel in the marine atmospheric environment10.1016/j.corsci.2021.109760 ↗
9. Comparative study of the stress corrosion behavior of a multiuse bainite steel in the simulated tropical marine atmosphere and seawater environments10.1016/j.conbuildmat.2019.117903 ↗
10. Fundamental investigation of stress corrosion cracking of E690 steel in simulated marine thin electrolyte layer10.1016/j.corsci.2018.12.029 ↗
11. Investigation on hydrogen embrittlement susceptibility in martensitic steels with 1000 MPa yield strength10.1016/j.jmrt.2021.11.130 ↗
12. Effect of vanadium and rare earth microalloying on the hydrogen embrittlement susceptibility of a Fe-18Mn-0.6C TWIP steel studied using the linearly increasing stress test10.1016/j.corsci.2021.109440 ↗
13. On the suitability of slow strain rate tensile testing for assessing hydrogen embrittlement susceptibility10.1016/j.corsci.2019.108291 ↗
14. Effect of cathodic potential on stress corrosion cracking behavior of different heat-affected zone microstructures of E690 steel in artificial seawater10.1016/j.jmst.2019.08.029 ↗
15. Corrosion evolution and stress corrosion cracking of E690 steel for marine construction in artificial seawater under potentiostatic anodic polarization10.1016/j.conbuildmat.2019.117763 ↗
16. Effect of cathodic polarisation on stress corrosion cracking behaviour of a Ni(Fe, Al)-maraging steel in artificial seawater10.1016/j.corsci.2020.109176 ↗
17. Hydrogen permeation and stress corrosion cracking of heat-affected zone of E690 steel under the combined effect of sulfur species and cathodic protection in artificial seawater10.1016/j.conbuildmat.2021.123721 ↗
18. The effect of crack tip environment on crack growth behaviour of a low alloy steel at cathodic potentials in artificial seawater10.1016/j.jmst.2020.04.034 ↗
19. Effect of radial hydride on delayed hydride cracking behaviour of Zr-2.5Nb pressure tube material10.1016/j.jnucmat.2020.152457 ↗
20. A decohesion pathway for hydrogen embrittlement in nickel: mechanism and quantitative prediction10.1016/j.actamat.2019.11.062 ↗
21. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
22. Temperature change induce crack mode transition of 316L stainless steel in H2S environment revealed by dislocation configurations10.1016/j.corsci.2021.109896 ↗
23. The effects of interstitial hydrogen and carbon atoms and aging temperature on annihilation behavior of hydrogen-enhanced strain-induced vacancies in iron10.1016/j.scriptamat.2021.114031 ↗
24. Determination of the hydrogen effects on the passive film and the micro-structure at the surface of 2205 duplex stainless steel10.1016/j.apsusc.2021.149597 ↗
25. Duplex stainless steel passive film electrical properties studied by in situ current sensing atomic force microscopy10.1016/j.corsci.2013.08.031 ↗
26. Hydrogen effects on microstructural evolution and passive film characteristics of a duplex stainless steel10.1016/j.elecom.2017.04.013 ↗
27. Synergistic effect of cold work and hydrogen charging on the pitting susceptibility of 2205 duplex stainless steel10.1016/j.electacta.2019.135081 ↗
28. Load partitioning between single bulk grains in a two-phase duplex stainless steel during tensile loading10.1016/j.actamat.2009.09.053 ↗
29. Hydrogen embrittlement of super duplex stainless steel – Towards understanding the effects of microstructure and strain10.1016/j.ijhydene.2018.05.028 ↗
30. Electrochemical characteristic and stress corrosion behavior of API X70 high-strength pipeline steel under a simulated disbonded coating in an artificial seawater environment10.1016/j.jelechem.2019.05.044 ↗
31. Constant-phase-element behavior caused by resistivity distributions in films10.1149/1.3499565 ↗
32. Effect of annealing time on the microstructure and SCC behavior of an austenite-based low-density steel in a marine atmosphere10.1016/j.corsci.2022.110466 ↗
33. Insight into electrochemical passivation behavior and surface chemistry of 2205 duplex stainless steel: effect of tensile elastic stress10.1016/j.corsci.2021.109903 ↗
34. On the implication of mobile hydrogen content on the surface reactivity of an austenitic stainless steel10.1016/j.electacta.2021.139684 ↗
35. The electrochemical behavior and characteristic of passive film on 2205 duplex stainless steel under various hydrogen charging conditions
36. Effect of secondary passivation on corrosion behavior and semiconducting properties of passive film of 2205 duplex stainless steel10.1016/j.jmrt.2021.11.118 ↗
37. Point defect model for passivity breakdown on hyper-duplex stainless steel 2707 in solutions containing bromide at different temperatures10.1016/j.corsci.2021.109959 ↗
38. Passive film on 2205 duplex stainless steel studied by photo-electrochemistry and ARXPS methods10.1016/j.corsci.2018.10.020 ↗
39. Semiconductivities of passive films formed on stainless steel bend under erosion-corrosion conditions10.1016/j.corsci.2018.08.045 ↗
40. Passivity of Sanicro28 (UNS N-08028) stainless steel in polluted phosphoric acid at different temperatures studied by electrochemical impedance spectroscopy and Mott–Schottky analysis10.1016/j.corsci.2014.04.056 ↗
41. Characterization of passive film on 2205 duplex stainless steel in sodium thiosulphate solution10.1016/j.apsusc.2011.06.077 ↗
42. A comparative study of primary and secondary passive films formed on AM355 stainless steel in 0.1 M NaOH10.1016/j.apsusc.2017.08.151 ↗
43. Adaptation of the point defect model to simulate oxidation kinetics of 316L stainless steel in the pressurised water reactor environment10.1016/j.corsci.2021.109454 ↗
44. Hydrogen detection in high strength dual phase steel using scanning Kelvin probe technique and XPS analyses10.1016/j.corsci.2021.110072 ↗
45. Investigation of multiplet splitting of Fe 2p XPS spectra and bonding in iron compounds10.1002/sia.1984 ↗
46. Synergistic effect of erosion and hydrogen on properties of passive film on 2205 duplex stainless steel10.1016/j.jmst.2020.08.004 ↗
47. Hydrogen segregation near a crack tip in nickel10.1016/j.scriptamat.2020.113697 ↗
48. Analyses of hydrogen distribution around fatigue crack on type 304 stainless steel using secondary ion mass spectrometry10.1016/j.ijhydene.2011.03.111 ↗
49. Topography and field effects in secondary ion mass spectrometry – part i: conducting samples10.1007/s13361-011-0201-1 ↗
50. Effects of hydrogen and stress on the electrochemical and passivation behaviour of 304 stainless steel in simulated PEMFC environment10.1016/j.electacta.2018.10.028 ↗
51. Hydrogen effect on the passivation and crevice corrosion initiation of AISI 304L using Scanning Kelvin Probe10.1016/j.corsci.2020.109225 ↗
52. Effect of negative half-wave alternating current on stress corrosion cracking behavior and mechanism of X80 pipeline steel in near-neutral solution10.1016/j.conbuildmat.2017.07.076 ↗
53. The mechanism of hydrogen-facilitated anodic-dissolution-type stress corrosion cracking: theories and experiments10.1080/01418610108216638 ↗
54. Role of hydrogen in stress corrosion cracking of austenitic stainless steels10.1080/14786435.2010.515262 ↗
55. Local additional potential model for effect of strain rate on SCC of pipeline steel in an acidic soil solution10.1016/j.corsci.2009.08.019 ↗
56. Fundamentally understanding the effect of Non-stable cathodic potential on stress corrosion cracking of pipeline steel in Near-neutral pH solution10.1016/j.conbuildmat.2021.123117 ↗
57. Effect of hydrogen charging on the microstructure evolution of duplex stainless steel10.1016/S0254-0584(03)00054-3 ↗
58. Edge dislocations emitted along multiple inclined slip planes from a Mode I crack. I. Sequential emission10.1016/0167-6636(96)00024-5 ↗
59. In situ TEM study of stress corrosion cracking of austenitic stainless steel10.1016/S0010-938X(02)00225-1 ↗
60. Effect of hydrogen trapping on hydrogen permeation in a 2205 duplex stainless steel: role of austenite–ferrite interface10.1016/j.corsci.2022.110332 ↗
61. Effect of plastic deformation at room temperature on hydrogen diffusion of S3040810.1016/j.ijhydene.2018.07.156 ↗
62. Modeling of hydrogen diffusion in duplex stainless steel based on microstructure using finite element method10.1016/j.ijpvp.2019.104031 ↗