journal article·2020-07

Investigation of microstructure and corrosion behavior of weathering steel in aqueous solution containing different anions for simulating service environments

Pan Liu, Lulu Hu, Xuyang Zhao, Qinhao Zhang, Zuosi Yu, Jiming Hu, Yiqing Chen, Fangfang Wu, Fahe Cao

Corrosion Science· Volume 170
Publisher page

Abstract

Abstract The microstructure and corrosion behavior of weathering steel in three solutions (S1: 3.5 wt.% NaCl, S2: 3.5 wt.% NaCl+0.052 wt.% NaHSO3, S3: 3.5 wt.% NaCl+0.907 wt.% NaHCO3) were investigated. A high proportion of random boundaries is responsible for strong corrosion sensitivity. The thickness of rust increases with immersion time and is in the order of S1>S3>S2. The rust formed in S1 and S2 solutions mainly consists of γ-FeOOH phase, but the latter is less protective. The rust formed in S1 solution is dense and thick resulting in its protection being similar to that in S3 solution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Corrosion and Durability · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Materials science: Share corrosion data10.1038/527441a ↗
2. The cost of corrosion in China10.1038/s41529-017-0005-2 ↗
3. Mechanism of MnS-mediated pit initiation and propagation in carbon steel in an anaerobic sulfidogenic media10.1016/j.corsci.2013.06.049 ↗
4. Multianalytical approach to study the dissolution process of weathering steel: The role of urban pollution10.1016/j.corsci.2013.06.038 ↗
5. Steels fit for the countryside
6. Influence of carbon content and microstructure on corrosion behaviour of low alloy steels in a Cl− containing environment10.1016/j.corsci.2008.10.025 ↗
7. Effect of tempering heat treatment on the CO2 corrosion resistance of quench-hardened Cr-Mo low-alloy steels for oil and gas applications10.1016/j.corsci.2019.03.036 ↗
8. Incipient corrosion behavior and mechanical properties of low-alloy steel in simulated industrial atmosphere10.1016/j.conbuildmat.2018.08.082 ↗
9. Microscale investigation of the correlation between microstructure and galvanic corrosion of low alloy steel A508 and its welded 309/308L stainless steel overlayer10.1016/j.corsci.2019.03.027 ↗
10. The mechanism of atmospherIic rusting and the protective amorphous rust on low alloy steel10.1016/S0010-938X(74)80037-5 ↗
11. Atmospheric corrosion of weathering steels. Overview for engineers. Part I: Basic concepts10.1016/j.conbuildmat.2019.03.334 ↗
12. Atmospheric corrosion data of weathering steels10.1016/j.corsci.2013.08.021 ↗
13. An study on accelerated corrosion testing of weathering steel10.1016/j.matchemphys.2013.07.009 ↗
14. Weathering steels: From empirical development to scientific design10.1016/j.corsci.2014.03.006 ↗
15. Atmospheric corrosion resistance of MnCuP weathering steel in simulated environments10.1016/j.corsci.2011.08.028 ↗
16. Revie · 2000 · 1227
17. Effects of alloying elements on the corrosion of steel in industrial atmospheres10.5006/1.3290374 ↗
18. Corrosion mechanisms for iron and low alloy steels exposed to the atmosphere10.1149/1.2086948 ↗
19. Microstructural characterisation and corrosion performance of old railway girder bridge steel and modern weathering structural steel10.1016/j.corsci.2016.10.004 ↗
20. On the corrosion behaviour of novel high carbon rail steels in simulated cyclic wet–dry salt fog conditions10.1016/j.corsci.2008.02.021 ↗
21. Corrosion behavior of weathering steel under thin electrolyte layer at different relative humidity10.1007/s11665-017-3101-0 ↗
22. Influence of alloyed chromium on the atmospheric corrosion resistance of weathering steels10.1016/j.corsci.2013.05.008 ↗
23. The influence of chromium content on the electrochemical behavior of weathering steels10.1016/j.corsci.2013.03.002 ↗
24. Atmospheric corrosion monitoring of a weathering steel under an electrolyte film in cyclic wet–dry condition10.1016/j.corsci.2013.09.008 ↗
25. Effect of tin addition on corrosion behavior of a low-alloy steel in simulated costal-industrial atmosphere10.1016/j.jmst.2019.01.008 ↗
26. The corrosion mechanisms of carbon steel and weathering steel in SO2 polluted atmospheres10.1016/S0254-0584(97)80019-3 ↗
27. Mössbauer studies on particle volume distribution of α-FeOOH in rust formed on weathering steel10.1143/JJAP.39.3382 ↗
28. Nature of atmospheric rust on iron10.1149/1.2129376 ↗
29. Mössbauer spectroscopic study of rust formed on a weathering steel and a mild steel exposed for a long term in an industrial environment10.2320/matertrans.43.694 ↗
30. Corrosion resistance and mechanical properties of low-alloy steels under atmospheric conditions10.1016/j.corsci.2004.04.009 ↗
31. Anomalous evolution of corrosion behaviour of warm-rolled type 304 austenitic stainless steel10.1016/j.corsci.2019.04.025 ↗
32. Effect of cold rolling on the corrosion properties of low-alloy steel in an acid-chloride solution10.1007/s12540-014-3009-2 ↗
33. Effect of cold rolling on the structure and mechanical properties of austenitic corrosion-resistant 10Kh18N8D3BR steel10.1134/S0036029512090133 ↗
34. Atmospheric corrosion of copper exposed in a simulated coastal-industrial atmosphere10.1016/j.jmst.2016.03.024 ↗
35. Evaluation of aluminum coatings in simulated marine environment10.1016/j.surfcoat.2012.12.011 ↗
36. Atmospheric corrosion of metals in industrial city environment10.1016/j.dib.2015.02.017 ↗
37. Atmospheric corrosion of carbon steel in Colombia10.1016/j.corsci.2009.09.006 ↗
38. Kelly · 2003
39. A fabrication of iridium oxide film pH micro-sensor on Pt ultramicroelectrode and its application on in-situ pH distribution of 316L stainless steel corrosion at open circuit potential10.1016/j.snb.2017.08.219 ↗
40. Mechanisms of corrosion and electrochemical significance of metallurgy and environment with corrosion of iron and steel in bicarbonate and carbonate solutions—a review10.5006/1213 ↗
41. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
42. Grain-boundaries: criteria of specialness and deviation from CSL misorientation10.1016/0001-6160(87)90217-3 ↗
43. The effect of grain size and grain boundary misorientation on the corrosion resistance of commercially pure aluminium10.1016/j.corsci.2018.11.035 ↗
44. Overview no. 127 the role of the grain boundary plane in cubic polycrystals10.1016/S1359-6454(97)00338-8 ↗
45. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
46. Effect of grain size on corrosion: A review10.5006/1.3462912 ↗
47. Influence of temperature on the corrosion behavior of API-X100 pipeline steel in 1-bar CO2-HCO3− solutions: An electrochemical study10.1016/j.matchemphys.2013.03.061 ↗
48. Optimizing the nickel content in weathering steels to enhance their corrosion resistance in acidic atmospheres10.1016/j.corsci.2016.11.016 ↗
49. Effect of tannic acid on corrosion behavior of carbon steel in NaCl solution10.1016/j.jmst.2018.09.001 ↗
50. The effects of anions on the behaviour of scratched iron electrodes in aqueous solutions10.1016/0010-938X(80)90145-6 ↗
51. Effects of a magnetic field on the anodic dissolution, passivation and transpassivation behaviour of iron in weakly alkaline solutions with or without halides10.1016/j.corsci.2005.11.014 ↗
52. Study of iron electrodissolution in carbonate/bicarbonate solutions by electrochemical impedance spectroscopy10.1016/0022-0728(92)80013-T ↗
53. The stress corrosion cracking of C-Mn steel in CO2-HCO3−-CO32− solutions. II: Electrochemical and other data10.1016/S0010-938X(97)89248-7 ↗
54. Corrosion of aluminium alloy AlSi7Mg0.3 in artificial sea water with added sodium sulphide10.1016/j.corsci.2018.08.038 ↗
55. An electrochemical impedance spectroscopy study of the corrosion behaviour of PVD coated steels in 0.5 N NaCl aqueous solution Part II. EIS interpretation of corrosion behaviour10.1016/S0010-938X(02)00214-7 ↗
56. The preparation and corrosion behaviors of MAO coating on AZ91D with rare earth conversion precursor film10.1016/j.apsusc.2010.11.153 ↗
57. Iron oxide/hydroxide (α,γ-FeOOH) nanoparticles as high potential adsorbents for lead removal from polluted aquatic media10.1016/j.jiec.2014.07.039 ↗
58. Synthesis of rod-like α-FeOOH nanoparticles and its photocatalytic activity in degradation of an azo dye: Empirical kinetic model development10.1016/j.molcata.2015.06.037 ↗
59. Influence of native oxide film age on the passivation of carbon steel in neutral aqueous solutions with a dicarboxylic acid10.1016/j.corsci.2019.03.033 ↗
60. XPS depth profiling of an ultrathin bioorganic film with an argon gas cluster ion beam10.1116/1.4948341 ↗
61. Native oxide layers formed on the surface of ultra high-purity iron and copper investigated by angle resolved XPS10.2320/matertrans1989.38.1004 ↗
62. XPS study of oxides formed on the surface of high‐purity iron exposed to air10.1002/1096-9918(200008)30:1<372::AID-SIA721>3.0.CO;2-R ↗
63. Nondestructive in-depth composition profile of oxy-hydroxide nanolayers on iron surfaces from ARXPS measurement10.1002/sia.2362 ↗
64. Chemical state quantification of iron and chromium oxides using XPS: the effect of the background subtraction method10.1016/j.susc.2005.01.019 ↗
65. Use of QUASES™/XPS measurements to determine the oxide composition and thickness on an iron substrate10.1002/sia.1842 ↗
66. Photoelectron spectroscopy study of the inhibition of mild steel corrosion by molybdate and nitrite anions10.1016/j.corsci.2009.09.030 ↗
67. Studies of the oxidation of iron by air after being exposed to water vapour using angle‐resolved x‐ray photoelectron spectroscopy and QUASES™10.1002/sia.1992 ↗
68. A study of the 42CrMo4 steel surface by quantitative XPS electron spectroscopy10.1016/j.apsusc.2008.01.090 ↗
69. Evolution of atmospheric corrosion of MnCuP weathering steel in a simulated coastal-industrial atmosphere10.1016/j.corsci.2012.03.010 ↗
70. Corrosion engineering: principles and solved problems
71. Environmental conditions for akaganeite formation in marine atmosphere mild steel corrosion products and its characterization10.5006/1672 ↗
72. Synergisitic effect of chloride and sulphur-bearing pollutant in atmospheric corrosion of mild steel
73. The effects of bicarbonate on the corrosion and passivation of iron10.5006/0010-9312-36.8.416 ↗
74. The influence of ionic composition on the electrodissolution and passivation of iron electrodes in potassium carbonate-bicarbonate solutions in the 8.4–10.5 pH range at 25 oC10.1016/0010-938X(86)90063-6 ↗