journal article·2024-04

In-situ rolling friction stir welding of aluminum alloys towards corrosion resistance

Wei Wang, Xiangchen Meng, Wenjiang Dong, Yuming Xie, Xiaotian Ma, Dongxin Mao, Zeyu Zhang, Yongxian Huang

Corrosion Science· Volume 230
Publisher page

Abstract

In-situ rolling friction stir welding (IRFSW) was proposed to improve corrosion resistance of 7075-T6 aluminum alloy joint via microstructural design and residual stress regulation. The residual stress at the weld edge was changed from +58.3 MPa to –25.7 MPa. The dissolution of precipitates and narrowing of precipitate-free zones reduced corrosion potential difference between the precipitates and the matrices. The active corrosion path was cut off by discontinuous distribution of fine precipitates in grain boundary. The ultimate tensile strength and elongation of IRFSW joints were increased by 24.1 % and 100.0 % compared to conventional FSW joints after constant load stress corrosion.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Nanoparticle-enabled phase control for arc welding of unweldable aluminum alloy 707510.1038/s41467-018-07989-y ↗
2. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
3. Recent progress on control strategies for inherent issues in friction stir welding10.1016/j.pmatsci.2020.100706 ↗
4. Improved resistance to stress-corrosion-cracking failures via optimized retrogression and reaging of 7075-T6 aluminum sheets10.1007/s11661-008-9595-1 ↗
5. The effects of aging treatments on mechanical property and corrosion behavior of spray formed 7055 aluminium alloy10.1016/j.jallcom.2017.11.070 ↗
6. Stress corrosion cracking behaviour of 7xxx aluminum alloys: a literature review10.1016/S1003-6326(16)64220-6 ↗
7. Stress corrosion cracking and hydrogen embrittlement of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2004.06.023 ↗
8. Stress corrosion behavior and microstructure analysis of Al-Zn-Mg-Cu alloys friction stir welded joints under different aging conditions
9. Response of mechanical properties and corrosion behavior of Al–Zn–Mg alloy treated by aging and annealing: A comparative study10.1016/j.jallcom.2020.156561 ↗
10. Effect of recrystallization and heat treatment on strength and SCC of an Al–Zn–Mg–Cu alloy10.1016/j.jallcom.2013.07.177 ↗
11. Effects of pre-strain on the surface residual stress and corrosion behavior of an Al-Zn-Mg-Cu alloy plate10.1016/j.matchar.2020.110129 ↗
12. A facile method to modify the characteristics and corrosion behavior of 304 stainless steel by surface nanostructuring toward biomedical applications10.1021/acsami.5b03877 ↗
13. Fatigue behaviors of AISI 316L stainless steel with a gradient nanostructured surface layer10.1016/j.actamat.2014.12.057 ↗
14. Making strong nanomaterials ductile with gradients10.1126/science.1255940 ↗
15. Enhanced mechanical properties and corrosion resistance of 316L stainless steel by pre-forming a gradient nanostructured surface layer and annealing10.1016/j.actamat.2021.116773 ↗
16. Corrosion susceptibility of peened friction stir welded 7075 aluminum alloy joints10.1016/j.corsci.2008.09.031 ↗
17. Effect of laser shock peening on the microstructure and corrosion resistance in the surface of weld nugget zone and heat-affected zone of FSW joints of 7050 Al alloy10.1016/j.optlastec.2018.10.054 ↗
18. Insight on corrosion behavior of friction stir welded AA2219/AA2195 joints in astronautical engineering
19. Ameliorating strength-ductility efficiency of graphene nanoplatelet-reinforced aluminum composites via deformation-driven metallurgy10.1016/j.compscitech.2021.109225 ↗
20. Evolution of microstructure and mechanical properties in naturally aged 7050 and 7075 Al friction stir welds10.1016/j.msea.2009.11.057 ↗
21. Effect of rotational speeds on microstructure and mechanical properties of friction stir-welded 7075-T6 aluminium alloy10.1177/0954406211404633 ↗
22. Effectiveness of cold metal transfer process for welding 7075 aluminium alloys10.1179/1362171815Y.0000000017 ↗
23. Investigations on temperature distribution, microstructure evolution, and property variations along thickness in friction stir welded joints for thick AA7075-T6 plates10.1007/s00170-015-8182-z ↗
24. Role of tool design on thermal cycling and mechanical properties of a high-speed micro friction stir welded 7075-T6 aluminum alloy10.1016/j.jmapro.2019.10.025 ↗
25. The Effects of rotational speed on microstructure and mechanical properties of friction stir-welded 7075-T6 thin sheet10.1007/s11665-020-04733-w ↗
26. Improving mechanical properties of quasi-continuous-wave laser beam welded 7075 aluminum alloy through microstructural refinement and homogenization of the fusion zone
27. Thermal cycles, microstructures and mechanical properties of AA7075-T6 ultrathin sheet joints produced by high speed friction stir welding
28. Effect of partial rolling on the microstructure and mechanical properties of laser-TIG hybrid welded joints of 7075-T6 aluminum alloy10.1007/s00170-022-09287-w ↗
29. The effects of friction stir welding on microstructure and formability of 7075-T6 sheet
30. Microstructure evolution and deformation behavior of TIG welded 7075-T6 aluminum alloy followed by partial hot rolling10.1016/j.jmapro.2023.04.006 ↗
31. Enhancing corrosion resistance of Al 5050 alloy based on surface roughness and its fabrication methods; an experimental investigation10.1016/j.jmrt.2021.01.096 ↗
32. Effect of surface abrasion on pitting corrosion of Al-Li alloy10.1016/j.corsci.2018.04.010 ↗
33. Effects of elastic and plastic deformations on the electron work function of metals during bending tests10.1080/14786430412331305294 ↗
34. Effect of surface nanocrystallization induced by fast multiple rotation rolling on hardness and corrosion behavior of 316L stainless steel10.1016/j.apsusc.2011.02.127 ↗
35. Efficacy of external stationary shoulder for controlling residual stress and distortion in friction stir welding10.1007/s12666-019-01630-2 ↗
36. Corrosion and biological behavior of nanostructured 316L stainless steel processed by severe plastic deformation10.1002/sia.5806 ↗
37. Towards friction stir remanufacturing of high-strength aluminum components10.1007/s40195-022-01444-0 ↗
38. Lightweight design: friction-based welding between metal and polymer10.1007/s40195-023-01552-5 ↗
39. Properties of friction-stir-welded 7075 T651 aluminum10.1007/s11661-998-0021-5 ↗
40. Dislocation-aided electrochemical behavior of precipitates in stress corrosion cracking of Al–Zn–Mg–Cu alloys
41. Stress corrosion behavior of friction stir welding joint of 7N01 aluminum alloy10.1016/j.jmrt.2021.08.112 ↗
42. Effects of Sc and Zr microalloying additions and aging time at 120 °C on the corrosion behaviour of an Al–Zn–Mg alloy10.1016/j.corsci.2012.08.024 ↗
43. Mechanical properties, corrosion behavior and microstructures of a non-isothermal ageing treated Al-Zn-Mg-Cu alloy10.1016/j.msea.2017.01.086 ↗
44. Simultaneously enhanced mechanical strength and inter-granular corrosion resistance in high strength 7075 Al alloy10.1016/j.jallcom.2018.12.024 ↗