Corrosion behaviour and hardness of in situ consolidated nanostructured Al and Al–Cr alloys produced via high-energy ball milling
Source abstract
Abstract
Abstract This paper presents a hypothesis and its experimental validation that simultaneous improvement in the hardness and corrosion resistance of aluminium can be achieved by the combination of suitable processing route and alloying additions. More specifically, the corrosion resistance and hardness of Al– x Cr ( x = 0–10 wt.%) alloys as produced via high-energy ball milling were significantly higher than pure Al and AA7075-T651. The improved properties of the Al– x Cr alloys were attributed to the Cr addition and high-energy ball milling, which caused nanocrystalline structure, extended solubility of Cr in Al, and uniformly distributed fine intermetallic phases in the Al–Cr matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Aluminium in innovative light-weight car design10.2320/matertrans.L-MZ201132 ↗
2. Review of warm forming of aluminum–magnesium alloys10.1016/j.jmatprotec.2008.03.057 ↗
3. Electrochemical characteristics of intermetallic phases in aluminum alloys: an experimental survey and discussion10.1149/1.1869984 ↗
4. Metastable pitting characteristics of aluminium alloys measured using current transients during potentiostatic polarisation10.1016/j.electacta.2012.01.090 ↗
5. Davis · 1999
6. Electrochemical behaviour of the β-phase intermetallic (Mg2Al3) as a function of pH as relevant to corrosion of aluminium–magnesium alloys10.1016/j.corsci.2012.12.022 ↗
7. Electrochemical behavior and localized corrosion associated with Mg2Si particles in Al and Mg alloys10.1149/2.002201eel ↗
8. Davis · 1996
9. Polmear · 2006
10. Pitting of sputtered aluminum alloy thin films10.1149/1.2096864 ↗
11. Mechanisms of passivity of nonequilibrium Al–W alloys10.1149/1.2056234 ↗
12. Corrosion behaviour of amorphous Al–Cr and Al–Cr–(N) coatings deposited by dc magnetron sputtering on mild steel substrate10.1016/j.tsf.2003.11.315 ↗
13. On the pitting resistance of sputter-deposited aluminum alloys10.1149/1.2220794 ↗
14. The effect of heat treatment on the corrosion behavior of sputter-deposited aluminum-chromium alloys10.1016/S0010-938X(98)00130-9 ↗
15. Microstructure dependence of nanometre corrosion in Al–Ni–Y glassy alloys10.1080/095008300176344 ↗
16. Relating the early evolution of microstructure with the electrochemical response and mechanical performance of a Cu-rich and Cu-lean 7xxx aluminum alloy10.1149/2.062211jes ↗
17. Nano-scale dissolution phenomena in Al–Cu–Mg alloys10.1016/j.elecom.2007.10.032 ↗
18. Quantification of sensitization in AA5083-H131 via imaging ga-embrittled fracture surfaces10.5006/0804 ↗
19. Investigating localized corrosion susceptibility arising from Sc containing intermetallic Al3Sc in high strength Al-alloys10.1016/j.scriptamat.2007.01.036 ↗
20. A theoretical study of the influence of microalloying on of AA5083 and moderation of sensitisation of a model Al–Mg–Mn alloy via Sr additions10.5006/1117 ↗
21. Electrochemical and corrosion response of commercially pure aluminum alloyed with binary additions of strontium10.1149/2.001308jes ↗
22. Imparting sensitization resistance to an Al–5Mg alloy via neodymium additions10.5006/0833 ↗
23. Influence of alloyed Nd content on the corrosion of an Al–5Mg alloy10.1016/j.corsci.2013.03.034 ↗
24. Role of nanostructure in pitting of Al–Cu–Mg alloys10.1016/j.electacta.2010.02.001 ↗
25. Nanostructural hierarchy increases the strength of aluminium alloys10.1038/ncomms1062 ↗
26. Fabrications and mechanical properties of bulk amorphous, nanocrystalline, nanoquasicrystalline alloys in aluminum-based system10.1016/S1471-5317(00)00004-3 ↗
27. A high-strength bulk nanocrystalline Al–Fe alloy processed by mechanical alloying and spark plasma sintering10.1016/j.scriptamat.2007.04.010 ↗
28. Structure and properties of attrition-milled aluminium powder10.1023/A:1018653607670 ↗
29. Effect of heat treatment on tensile properties of the cold-compacted nanocrystalline Al10.1016/S0965-9773(99)00391-8 ↗
30. Microstructure and mechanical properties of bulk nanocrystalline Al–Fe alloy processed by mechanical alloying and spark plasma sintering10.1016/j.actamat.2009.04.012 ↗
31. Microstructure and microhardness of an Al–Fe alloy subjected to severe plastic deformation and aging10.1016/S0965-9773(98)00107-X ↗
32. Microstructure and mechanical properties of nanocrystalline Al–Ti alloys consolidated by plasma activated sintering10.1016/S0925-8388(99)00518-6 ↗
33. Consolidation behavior of nanocrystalline Al–5at.%Ti alloys synthesized by cryogenic milling10.1016/S0925-8388(00)01213-5 ↗
34. Mechanical behavior of nanocrystalline aluminum-zirconium10.1016/S0921-5093(97)00129-9 ↗
35. Hardness of high strength nanocomposite Al–X–Zr (X=Si,Cu,Ni) alloys10.1016/j.msea.2003.10.189 ↗
36. Microstructure and mechanical properties of Al–Zr nanocomposite materials10.1016/j.msea.2009.04.032 ↗
37. Processing and mechanical properties of nanocrystalline 5083 Al alloy10.1016/S0965-9773(99)00110-5 ↗
38. Mechanical behavior and microstructure of a thermally stable bulk nanostructured Al alloy10.1007/s11661-001-0207-6 ↗
39. Al–Mg alloy engineered with bimodal grain size for high strength and increased ductility10.1016/S1359-6462(03)00283-5 ↗
40. Al–Mg alloy with ultrahigh strength and good ductility10.1016/j.scriptamat.2005.09.028 ↗
41. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
42. Nanostructured materials by mechanical alloying: New results on property enhancement10.1007/s10853-010-4252-7 ↗
43. Synthesis and mechanical behavior of nanostructured materials via cryomilling10.1016/j.pmatsci.2005.04.004 ↗
44. Structural evolution in mechanically alloyed Al–Fe powders10.1007/BF02670665 ↗
45. Extended solid solubility in ball-milled Al–Mg alloys10.1007/BF00349027 ↗
46. Microstructural evolution during recovery and recrystallization of a nanocrystalline Al–Mg alloy prepared by cryogenic ball milling10.1016/S1359-6454(03)00083-1 ↗
47. Influence of Mn solute content on grain size reduction and improved strength in mechanically alloyed Al–Mn alloys10.1016/j.msea.2013.09.047 ↗
48. Alloying of immiscible Ge with Al by ball milling10.1016/S0167-577X(03)00149-6 ↗
49. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
50. The influence of nanocrystalline structure and processing route on corrosion of stainless steel: a review10.1016/j.corsci.2014.11.041 ↗
51. Synthesis of bulk nanostructured Zn by combinations of cryomilling and powder consolidation by room temperature milling: optimizing mechanical properties10.1016/S1359-6462(03)00297-5 ↗
52. Ultratough nanocrystalline copper with a narrow grain size distribution10.1063/1.1779342 ↗
53. Tensile properties of in situ consolidated nanocrystalline Cu10.1016/j.actamat.2004.12.005 ↗
54. Synthesis, characterization and mechanical behaviour of an in situ consolidated nanocrystalline FeCrNi alloy10.1007/s10853-011-5986-6 ↗
55. Cullity · 2001
56. Mondolfo · 1976
57. VanHorn · 1967 · vol. 1
58. Pandat® software. Pandat and PanAl databases, Computherm. LLC. Available from: http://www.computherm.com/, December 2014.
59. Nanocrystalline materials10.1016/0079-6425(89)90001-7 ↗
60. Gupta · 2012
61. Synthesis of nanostructured materials by mechanical milling: problems and opportunities10.1016/S0965-9773(97)00014-7 ↗
62. Novel materials synthesis by mechanical alloying/milling10.1179/imr.1998.43.3.101 ↗
63. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
64. The corrosion behaviour of nanocrystalline nickel10.1016/0956-716X(91)90171-V ↗
65. Electrochemical corrosion behavior of nanocrystalline materials – a review10.1016/S1005-0302(10)60001-1 ↗
66. Effect of nanocrystalline structure on the corrosion of a Fe20Cr alloy10.1016/S1452-3981(23)14806-1 ↗
67. Effect of vacuum system base pressure on corrosion resistance of sputtered Al thin films10.1149/2.056404jes ↗
68. The determination of yield strength from hardness measurements10.1007/BF02913433 ↗
69. Improvement of toughness and ductility of a cryomilled Al–Mg alloy via microstructural modification10.1007/s11661-005-0329-3 ↗
70. Mechanical behavior of a cryomilled nanostructured Al–7.5 pct Mg alloy10.1007/s11661-004-0019-6 ↗