Hot corrosion behaviour of single-phase platinum-modified aluminide coatings: Effect of Pt content and pre-oxidation
Source abstract
Abstract
Abstract Hot corrosion behaviour of nickel-based aluminide coatings with different thicknesses of initial Pt plating was evaluated in the Na 2 SO 4 /NaCl (75:25, wt./wt.) salt mixture at 900 °C. Compared to plain aluminide, the Pt-modified coatings showed better hot corrosion resistance by hindering the outward diffusion of undesirable elements from the substrate alloy. Pre-oxidation was confirmed to be capable of preventing molten salt from accessing the alloy surface and reversibly dissolving the oxide scale. Oxide growth and dissolution, acting as two competitive processes, occurred simultaneously and had an important impact on the entire performance of the Pt-modified aluminide coatings in hot corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Semiconductor materials and devices · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Materials design for the next generation thermal barrier coatings10.1146/annurev.matsci.33.011403.113718 ↗
2. Progress in coatings for gas turbine airfoils10.1016/S0257-8972(98)00667-7 ↗
3. NiAl bond coats made by a directed vapor deposition approach10.1016/j.msea.2004.11.017 ↗
4. Hot corrosion behavior of Co modified NiAl coating on nickel base superalloys10.1016/j.corsci.2012.06.027 ↗
5. Effects of platinum on the hot corrosion behavior of Hf-modified (γ′-Ni3Al+γ-Ni-based alloys10.1007/s11085-011-9251-9 ↗
6. Influence of sulfur platinum, and hafnium on the oxidation behavior of CVD NiAl bond coatings10.1023/A:1020525123056 ↗
7. Hot corrosion and oxidation behavior of a novel Pt+Hf-modified (γ′-Ni3Al+γ-Ni-based coating10.1016/j.surfcoat.2006.07.250 ↗
8. The influence of platinum on the oxidation and sodium sulfate induced hot corrosion of NiAl diffusion coatings10.3184/096034011X13188762374132 ↗
9. Preparation and hot corrosion behaviour of two Co modified NiAl coatings on a Ni-based superalloy10.1016/j.corsci.2013.07.008 ↗
10. Effect of Y2O3 content in the pack on microstructure and hot corrosion resistance of Y-Co-modified aluminide coating10.1016/j.corsci.2014.05.018 ↗
11. Hot corrosion behavior of Ni-Co-Cr-Al-Y-Si-B coating deposited by AIP
12. Sulfur segregation at Al2O3/γ-Νi+γ′-Ni3Al: effects of Pt, Cr and Hf additions10.1007/s11085-009-9149-y ↗
13. Oxidation behavior of NiAl—II. Cavity formation beneath the oxide scale on NiAl of different stoichiometries10.1016/0010-938X(93)90271-H ↗
14. Influence of Pt on the metal-oxide interface during high temperature oxidation of NiAl bulk materials10.1016/j.corsci.2008.12.016 ↗
15. Examination of the platinum effect on the oxidation behavior of nickel-aluminide coatings10.1016/j.surfcoat.2007.06.013 ↗
16. The hot-corrosion behavior of novel Co-deposited chromium-modified aluminide coatings10.1007/BF00665662 ↗
17. The effect of Pt content on the scale development on β-NiAl at very early oxidation stages10.1007/s11085-017-9714-8 ↗
18. Effect of aluminisation characteristics on the microstructure of single phase β-(Ni, Pt)Al coating and the isothermal oxidation behaviour10.1016/j.corsci.2016.01.024 ↗
19. Cyclic oxidation and rumpling behaviour of single phase β-(Ni, Pt)Al coatings with different thickness of initial Pt plating10.1016/j.corsci.2016.05.011 ↗
20. Some practical aspects of corrosion and coatings in utility gas turbines10.4028/www.scientific.net/MSF.251-254.483 ↗
21. Hot corrosion behaviour of NiAl in sulphate-chloride mixtures in the atmosphere10.1016/j.corsci.2006.10.010 ↗
22. Evolution of oxide scale on aluminide and Pt-aluminide coatings exposed to Type I (870°C) hot corrosion10.1007/s11085-015-9580-1 ↗
23. Compositional effects on the Type I hot corrosion of β-NiAl alloys10.1016/j.surfcoat.2011.06.025 ↗
24. Effect of composition on the oxidation and hot corrosion resistance of NiAl doped with precious metals10.1016/S0257-8972(00)00878-1 ↗
25. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
26. Hot corrosion properties of composite coatings in the presence of NaCl at 700 and 900°C10.1016/j.corsci.2013.01.004 ↗
27. A study of hot corrosion behaviour of NiAl coatings in an aggressive environment10.4028/www.scientific.net/SSP.226.177 ↗
28. Hot corrosion of arc ion plating NiCrAlY and sputtered nanocrystalline coatings on a nickel-based single-crystal superalloy10.1016/j.corsci.2017.04.004 ↗
29. Formation and healing of voids at the metal-oxide interface in NiAl Alloys10.1007/s11085-008-9132-z ↗
30. Synthesis and cyclic oxidation behavior of a (Ni, Pt) Al coating on a desulfurized Ni-base superalloy10.1007/s11661-999-0308-1 ↗
31. Surface and interface segregation in β-NiAl with and without Pt addition10.1016/j.scriptamat.2005.10.065 ↗
32. Substrate effect on the high-temperature oxidation behavior of a Pt-modified aluminide coating. Part I: influence of the initial chemical composition of the coating surface10.1007/s11085-006-9024-z ↗
33. Effect of platinum on the oxide-to-metal adhesion in thermal barrier coating systems10.1007/s10853-007-2130-8 ↗
34. Microstructures and cyclic oxidation behaviour of Pt-free and low-Pt NiAl coatings on the Ni-base superalloy Rene-8010.1016/j.corsci.2011.10.037 ↗
35. Partial thermodynamic properties of γ′-(Ni, Pt)3Al in the Ni-Al-Pt system10.1007/s11669-006-9004-7 ↗
36. Preparation and hot corrosion behaviour of an Al-gradient NiCoCrAlYSiB coating on a Ni-base superalloy10.1016/j.corsci.2009.01.003 ↗
37. Corrosion failures in gas turbine hot components10.1007/s11668-012-9571-3 ↗
38. Preparation and hot corrosion behaviour of Pt modified AlSiY coating on a Ni-based superalloy10.1016/j.corsci.2015.12.007 ↗