Oxidation behavior and incombustibility of molten Mg-Zn-Y alloys with Ca and Be addition
Source abstract
Abstract
Abstract By addition of Ca or Be, non-flammable high strength Mg97Zn1Y2 (at%) alloys are developed. The addition of Ca results in the formation of a thin and continuous CaO and MgO outermost layer above Y2O3 inner layer, what helps to prevent the internal oxidation of Y and an increased ignition temperature can be achieved. The addition of a small amount of Be also helps to suppress the internal oxidation of Y. The most likely explanation for the enhancement of incombustibility is that the segregation of Be along the grain boundaries in the Y2O3 layer impedes the grain boundary diffusion of oxygen and cations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Weight loss with magnesium alloys10.1126/science.1182848 ↗
2. Rapidly solidified power metallurgy Mg97Zn1Y2 alloys with excellent tensile strength above 600 MPa10.2320/matertrans.42.1172 ↗
3. Relation between corrosion behavior and microstructure of Mg-Zn-Y alloys prepared by rapid solidification at various cooling rates10.1016/j.corsci.2008.11.003 ↗
4. Influence of cooling rate on corrosion resistance of rapidly solidified Mg-Zn-Y alloys with a long period stacking ordered phase, ECS transactions, vol. 16
5. Development of high-strength and highly corrosion-resistant bulk nanocrystalline Mg-Zn-Y alloys with long period stacking ordered phase10.1149/1.3091907 ↗
6. Nanocrystalline LPSO Mg-Zn-Y-Al alloys with high mechanical strength and corrosion resistance10.4028/www.scientific.net/MSF.638-642.1476 ↗
7. Corrosion and passivation behavior of Mg-Zn-Y-Al alloys prepared by cooling rate-controlled solidification10.1016/j.apsusc.2011.01.046 ↗
8. Microstructure and mechanical properties of extruded Mg-Zn-Y alloys with 14H long period ordered structure10.2320/matertrans.47.959 ↗
9. Formation and mechanical properties of Mg97Zn1RE2 alloys with long-period stacking ordered structure10.2320/matertrans.MER2007142 ↗
10. Effect of long-period stacking ordered phase on mechanical properties of Mg97Zn1Y2 extruded alloy10.1016/j.actamat.2010.07.050 ↗
11. Effect of multimodal microstructure evolution on mechanical properties of Mg-Zn-Y extruded alloy10.1016/j.actamat.2011.02.038 ↗
12. Marker · 2013
13. The ignition temperature of Mg alloys WE43, AZ31 and AZ9110.1016/j.corsci.2011.09.004 ↗
14. Influence of Al and Y on the ignition and flammability of Mg alloys10.1016/j.corsci.2011.10.014 ↗
15. Oxidation characteristics of magnesium alloys10.1007/s11837-012-0477-z ↗
16. Overcoming barriers of magnesium ignition and flammability
17. Controlling the ignition and flammability of magnesium for aerospace applications10.1016/j.corsci.2014.04.047 ↗
18. Oxidation resistance of Mg–9Al–1Zn alloys micro-alloyed with Be10.1016/j.scriptamat.2015.12.022 ↗
19. Effect of CaO and hot extrusion on the oxidation of AZ61 magnesium alloys10.1007/s11085-015-9579-7 ↗
20. Formation of an incombustible oxide film on a molten Mg-Al-Ca alloy10.1016/j.corsci.2017.01.026 ↗
21. Improving aluminum castings with beryllium
22. Beryllium in aluminum and magnesium alloys
23. Flame-resistant magnesium alloys by calcium
24. Suppression of ignition and burning of molten Mg alloys by Ca bearing stable oxide film10.1023/A:1018526708423 ↗
25. A new approach to magnesium die casting
26. The effect of calcium additions on the oxidation behavior in magnesium alloys10.1016/S1359-6462(00)00344-4 ↗
27. Behavior of surface oxidation on molten Mg-9Al-0.5Zn-0.3Be alloy10.1016/S0921-5093(00)01798-6 ↗
28. Effects of Ca addition on the microstructure and mechanical properties of AZ91magnesium alloy10.1023/A:1017927109291 ↗
29. Effects of Ca and Be addition on high temperature oxidation behavior of AZ91 alloys10.4028/www.scientific.net/MSF.419-422.639 ↗
30. Effect of Ca addition on the oxidation resistance of AZ91 magnesium alloys at elevated temperatures10.1007/BF03027194 ↗
31. Effects of Al and Y additions on the oxidation behavior of Mg-Ca base molten alloys10.4028/www.scientific.net/MSF.419-422.581 ↗
32. Surface oxidation behavior of Mg-Y-Ce alloys at high temperature10.1007/s11661-005-0155-7 ↗
33. Early oxidation behaviors of Mg–Y alloys at high temperatures10.1016/j.jallcom.2007.06.065 ↗
34. Effect of Ca and Y additions on oxidation behavior of AZ91 alloy at elevated temperatures10.1016/S1003-6326(08)60268-X ↗
35. Oxidation behavior of ignition-proof magnesium alloys with rare earth addition10.1016/j.jallcom.2010.10.168 ↗
36. Effect of yttrium, calcium and zirconium on ignition-proof principle and mechanical properties of magnesium alloys10.1016/S1002-0721(10)60642-4 ↗
37. Phase equilibria in the systems Dy2O3-CaO, Y2O3-CaO, Yb2O3-CaO
38. The oxidation of metals at high temperatures
39. Lopato · 1963 · 2 · 454
40. Knacke · 1991
41. Phase equilibria in the system CaO-MgO10.1111/j.1151-2916.1963.tb11737.x ↗
42. Tilley · 2004
43. The reactive element effect on high-temperature oxidation of magnesium10.1179/1743280415Y.0000000001 ↗
44. The early stage oxidation and evaporation of Mg-9%Al-1%Zn alloy10.1016/S0010-938X(03)00151-3 ↗
45. Kinetics, Microstructures and Mechanism of Internal Oxidation - Its Effect and Prevention in High Temperature Alloy Oxidation10.5006/0010-9312-21.12.382 ↗
46. In-situ determination of growth and thermal stresses in chromia scales formed on a ferritic stainless steel10.1002/1521-4176(200207)53:7<486::AID-MACO486>3.0.CO;2-P ↗
47. Cullity · 2001 · 431
48. Determination of residual stresses by X-ray diffraction - issue 2, DTI
49. Elastic properties of polycrystalline yttrium oxide, dysprosium oxide, holmium oxide, and erbium oxide: room temperature measurements10.1111/j.1151-2916.1969.tb11974.x ↗
50. On the mechanism of microcrack formation in nanocrystalline Fe-Ni electrodeposits10.1023/A:1018693005002 ↗