Oxidation resistance of SiCf/SiC composites with a PyC/SiC multilayer interface at 500 °C to 1100°C
Source abstract
Abstract
Abstract SiC fiber-reinforced SiC ceramic matrix composites with a novel PyC/SiC multilayer interface were oxidized at 500 °C–1100 °C for more than 400 h. The oxidation resistance of the composites was evaluated by microstructural and mechanical evolution. Results showed that the PyC layer of composites was completely consumed after oxidation at 500 °C and 700 °C, thereby resulting in significant mechanical-property degradation. By contrast, 97 % and 101 % strength remained after oxidation at 900 °C and 1100 °C, respectively. The transformation was associated with the self-healing characteristics of the composites beyond 900 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Potential application of ceramic matrix composites to aero-engine components10.1016/S1359-835X(98)00139-0 ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. Ceramic matrix composite turbing vanes for gas turbing engines
4. Single‐ and Multilayered Interphases in SiC/SiC Composites Exposed to Severe Environmental Conditions: An Overview10.1111/j.1744-7402.2009.02424.x ↗
5. Enhanced oxidation resistance of SiC/SiC minicomposites via slurry infiltration of oxide layers10.1016/j.jeurceramsoc.2017.03.065 ↗
6. Current status and prospects of SiCf/SiC for fusion structural applications10.1016/j.jeurceramsoc.2013.02.013 ↗
7. Stability of SiC and its composites at high neutron fluence10.1016/j.jnucmat.2010.12.088 ↗
8. Effect of SiC nanowires on the high-temperature microwave absorption properties of SiCf/SiC composites10.1016/j.jeurceramsoc.2019.01.018 ↗
9. Quantification of crack area in ceramic matrix composites at single-fiber push-out testing and influence of pyrocarbon fiber coating thickness on interfacial fracture toughness10.1016/j.jeurceramsoc.2015.04.033 ↗
10. Appropriate thickness of pyrolytic carbon coating on SiC fiber reinforcement to secure reasonable quasi-ductility on NITE SiC/SiC composites10.1016/j.ceramint.2018.07.158 ↗
11. Effect of interface type on the static and dynamic mechanical properties of 3D braided SiCf/SiC composites10.1016/j.msea.2016.05.080 ↗
12. Oxidation resistance of NITE-SiC/SiC composites with/without CVD-SiC environmental barrier coating10.1016/j.ceramint.2018.06.194 ↗
13. Influence of surface fibre properties and textural organization of a pyrocarbon interphase on the interfacial shear stress of SiC/SiC minicomposites reinforced with Hi-Nicalon S and Tyranno SA3 fibres10.1016/j.jeurceramsoc.2013.08.027 ↗
14. Enchanced high-temperature performances of SiC/SiC composites by high densification and crystalline structure10.1016/j.compscitech.2010.11.026 ↗
15. Single-crystal SiC nanowires with a thin carbon coating for stronger and tougher ceramic composites10.1002/adma.200500104 ↗
16. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
17. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
18. Intermediate temperature strength degradationin SiC/SiC composites10.1016/S0955-2219(02)00144-9 ↗
19. Influence of SiC coating thickness on mechanical properties of SiCf/SiC composite10.1016/j.jnucmat.2013.08.038 ↗
20. Fabrication of advanced SiC fiber/F-CVI SiC matrix composites with SiC/C multi-layer interphase10.1016/j.jnucmat.2004.04.120 ↗
21. SiC/SiC minicomposites with nanoscale multilayered fibre coatings10.1016/S0266-3538(00)00131-7 ↗
22. Mechanical properties of several advanced Tyranno-SA fiber-reinforced CVI-SiC matrix composites10.1016/S0921-5093(02)00468-9 ↗
23. The effect on the tensile properties of PIP-processed SiC/SiC composite of a chemical vapor-infiltrated SiC layer overlaid on the pyrocarbon interface layer10.1016/j.compositesa.2016.04.021 ↗
24. Fiber coatings for SiC-Fiber-Reinforced BMAS glass-ceramic composites10.1111/j.1151-2916.1997.tb02823.x ↗
25. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
26. Thermophysical and mechanical properties of near-stoichiometric fiber CVI SiC/SiC composites after neutron irradiation at elevated temperatures10.1016/j.jnucmat.2010.06.002 ↗
27. Tensile static fatigue of 2D SiC/SiC composites with multilayered (PyC–SiC)n interphases at high temperatures in oxidizing atmosphere10.1016/S1359-835X(98)00093-1 ↗
28. Mechanical properties of advanced SiC fiber composites irradiated at very high temperatures10.1016/j.jnucmat.2011.02.006 ↗
29. The effect of neutron irradiation on the fiber/matrix interphase of silicon carbide composites10.1016/j.jnucmat.2008.11.015 ↗
30. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗
31. Oxidation of carbon fibers and films in ceramic matrix composites: a weak link process10.1016/0008-6223(95)00034-B ↗
32. Oxidation behaviour of SiC fibre reinforced SiC10.1016/0022-3115(95)00133-6 ↗
33. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: I, an experimental approach10.1111/j.1151-2916.1994.tb07015.x ↗
34. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: II, modeling10.1111/j.1151-2916.1994.tb07016.x ↗
35. Ceramic composites with multilayer interface coatings10.1111/j.1151-2916.2000.tb01676.x ↗
36. Micro-mechanical evaluation of SiC-SiC composite interphase properties and debond mechanisms10.1016/j.compositesb.2017.07.035 ↗
37. The effect of the PyC interphase coating on the microwave heating sintered SiC/SiC composites10.1016/j.jallcom.2016.07.288 ↗
38. Influence of pyrolytic carbon interface thickness on microstructure and mechanical properties of SiC/SiC composites by NITE process10.1016/j.compscitech.2007.05.037 ↗
39. Oxidation of the carbon interface in nicalon-fiber-Reinforced silicon carbide composite10.1111/j.1151-2916.1997.tb02868.x ↗