journal article·2018-04

Studies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 °C

Min Cao, Li Liu, Zhongfen Yu, Lei Fan, Li Ying, Fuhui Wang

Corrosion Science· Volume 133
Publisher page

Abstract

Abstract The corrosion behavior of Fe-20Cr in NaCl solution spray at 600 °C, compared with that under solid NaCl deposit in water vapor, has been studied by mass-gain measurements, scanning electron microscopy, X-ray diffraction, X-ray photoelectron spectroscopy, secondary ion mass spectrometry and transmission electron microscopy methods The results demonstrated that Fe-20Cr undergoes serious corrosion in NaCl solution spray. Significantly different corrosion products with outer Fe2O3 and inner FeCr2O4 layers were formed. Meanwhile, a small amount of Cl was found in the corrosion scale, which was thought to have an important effect on corrosion. The corrosion behavior of Fe-20Cr in NaCl solution spray at 600 °C has been discussed in detail.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Synergestic effect of NaCl and water vapor on the corrosion of 1Cr11Ni2W2MoV steel at 500–700 °C10.1023/A:1018854202982 ↗
2. Synergestic effect of NaCl and water vapor on the corrosion of Ti60 alloy at 500–700 °C10.1023/A:1018864216554 ↗
3. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗
4. Corrosion behavior of a sputtered K38G nanocrystalline coating with a solid NaCl deposit in wet oxygen at 600–700 °C10.1023/A:1016072726338 ↗
5. Influence of Cr content on the corrosion of Fe-Cr alloys: the synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
6. Corrosion inhibition of 304 stainless steel by nano-sized Ti/silicone coatings in an environment containing NaCl and water vapor at 400–600 °C10.1023/B:OXID.0000038782.77162.5b ↗
7. Corrosion behavior of metals or alloys with a solid NaCl deposit in wet oxygen at medium temperature10.1007/s11431-011-4675-7 ↗
8. The high temperature oxidation behavior of MgGdYZr alloy10.1007/s11085-009-9145-2 ↗
9. KCl-induced corrosion of a 304-type austenitic stainless steel in O2 and in O2+ H2O environment: the influence of temperature10.1007/s11085-009-9153-2 ↗
10. The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 and 500 °C10.1002/maco.201005942 ↗
11. KCl-induced corrosion of the FeCrAl alloy Kanthal® AF at 600C and the effect of H2O10.1007/s11085-014-9506-3 ↗
12. KCl-Induced corrosion of an FeCrAl alloy at 600 °C in O2+ H2O environment: the effect of pre-oxidation10.1007/s11085-014-9507-2 ↗
13. An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe–2.25Cr–1Mo steel at 400 °C10.1016/j.corsci.2011.03.007 ↗
14. The effects of KCl, K2SO4 and K2CO3 on the high temperature corrosion of a 304-type austenitic stainless steel10.1007/s11085-011-9240-z ↗
15. The influence of small amounts of KCl(s) on the initial stages of the corrosion of alloy Sanicro 28 at 600 °C10.1007/s11085-008-9118-x ↗
16. KCl-induced high temperature corrosion of the austenitic Fe-Cr-Ni alloys 304L and Sanicro 28 at 600 °C10.1016/j.corsci.2005.05.018 ↗
17. KCl induced corrosion of a 304-type austenitic stainless steel at 600 °C: the role of potassium10.1007/s11085-005-5704-3 ↗
18. Internal oxidation of Fe-Al alloys in a KCl-air atmosphere at 650 °C10.1023/B:OXID.0000025337.64394.bf ↗
19. The influence of KCl on the corrosion of an austenitic stainless steel (304L) in oxidizing humid conditions at 600 °C: a microstructural study10.1007/s11085-009-9156-z ↗
20. Alkali induced high temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
21. A pilot plant study of the effect of alkali salts on initial stages of the high temperature corrosion of alloy 304L
22. The influence of sulphur additions on the corrosive environment in a waste-fired CFB boiler
23. Deposition and high temperature corrosion in a 10 MW straw fired boiler10.1016/S0378-3820(97)00062-3 ↗
24. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
25. Accelerated oxidation rate of chromium induced by sodium chloride10.1007/BF00659274 ↗
26. The effects of chlorides hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
27. Lab-scale investigations of high-temperature corrosion phenomena in straw-fired boilers10.1021/ef990001g ↗
28. Field test corrosion experiments in Denmark with biomass fuels part 1: straw-firing10.1002/1521-4176(200202)53:2<121::AID-MACO121>3.0.CO;2-R ↗
29. Corrosion behaviour of some Fe-base alloys in H(2)-H(2)O and H2-H2O-HCl gas mixtures at 973 K10.4028/www.scientific.net/MSF.251-254.591 ↗
30. The effect of chlorine on mixed oxidation/sulfidation of stainless steels below 600 °C10.4028/www.scientific.net/MSF.251-254.575 ↗
31. Behaviour of Fecralloy and iron aluminides alloys in coal gasification atmospheres containing HCl10.4028/www.scientific.net/MSF.251-254.583 ↗
32. Air conditioning design manual, China Architecture & Building Press, The Tenth Research Institute of the Ministry of electronics industry, (2005) ISBN:711202626.
33. Effects of water-vapor on oxide-growth on 304 stainless-steel at 900 °C, international conference on the microscopy and oxidation
34. Quantification of aluminum outward diffusion during oxidation of FeCrAl alloys10.1007/s11085-005-4391-4 ↗
35. A critique of internal oxidation in alloys during the post-wagner era10.1007/BF01046724 ↗
36. Grain boundary ridge formation during initial high temperature oxidation of Mn/Al TRIP steel10.1080/14786430701324139 ↗
37. The relationship between grain boundary character and the intergranular oxide distribution in IN718 superalloy10.1002/adem.200500036 ↗
38. Liang · 1993 · vol. 8
39. Barin · 1996