Abstract
Abstract The oxidation behavior of a Fe-20Cr-25Ni-Nb austenitic stainless steel was investigated in an oxidizing environment at 1000 °C. Results show that an accelerated oxidation occurs after a transition point and some oxide nodules with two layers are formed on the steel surface. The oxidation of intergranular Fe2Nb phases can induce micro-cracks and promotes the formation of re-generated Cr2O3 phases. The formation and growth of the re-generated Cr2O3 phases are related to the cracking and spallation of the oxide scale, which result in the formation of these oxide nodules and the associative accelerated oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Nuclear applications of oxide dispersion strengthened and nano-featured alloys: an introduction10.1007/s11837-014-1211-9 ↗
2. Selection of fuel cladding material for nuclear fission reactors10.1016/j.engfailanal.2011.06.010 ↗
3. Managing nuclear power plant safety with FeCrAl alloy fuel cladding
4. Performance degradation of candidate accident-tolerant cladding under corrosive environment10.1515/corrrev-2017-0014 ↗
5. Characterization of the initial oxide formed on annealed and unannealed 20Cr-25Ni-Nb-stabilized steel in 50 torr CO2 at 973 K10.1007/BF00664230 ↗
6. A study of the high temperature oxidation behaviour of stainless steel using time lapse photomicrography10.1016/S0010-938X(70)80061-0 ↗
7. Intergranular corrosion of austenitic stainless steel10.1149/1.2407966 ↗
8. Intergranular corrosion of iron-nickel-chromium alloys
9. Oxidation behavior of 20% Cr/25% Ni/Nb stabilized stainless steel in CO2 environments10.1007/BF00741470 ↗
10. The influence of a titanium nitride dispersion on the oxidation behavior of 20% Cr-25% Ni stainless steel10.1007/BF00603805 ↗
11. Chromium depletion at 2-dimensional features during the selective oxidation of a 20Cr–25Ni austenitic steel10.1007/s11085-006-9039-5 ↗
12. Oxidation behavior of Fe–25Cr–20Ni–2.8Si during isothermal oxidation at 1286 K: life-time prediction10.1007/s11085-008-9097-y ↗
13. A determination of the chromium concentration for ‘healing’ layer formation during the oxidation of chromium-depleted 20Cr–25Ni–Nb stainless steel10.1016/0010-938X(84)90065-9 ↗
14. Spallation of oxide from stainless steel AGR nuclear fuel cladding: mechanisms and consequences10.1179/mst.1988.4.5.414 ↗
15. The development of localized pits during stainless steel oxidation10.1007/BF00604566 ↗
16. Formation of protective oxide film on chromium-depleted stainless steel10.1179/msc.1981.15.6.267 ↗
17. On the computation of saturation vapor pressure10.1175/1520-0450(1967)006<0203:OTCOSV>2.0.CO;2 ↗
18. Young · 2008
19. Li · 2003
20. The oxidation of metals10.1088/0034-4885/37/2/002 ↗
21. Formation and growth of spinel and Cr2O3 oxides on 20%Cr–25%Ni–Nb stainless steel in CO2 environments10.1007/BF00659904 ↗
22. COSP for Windows–Strategies for rapid analyses of cyclic-oxidation behavior10.1023/A:1015308606869 ↗
23. Oxidation characteristics of the electron beam surface-treated Alloy 617 in high temperature helium environments10.1016/j.jnucmat.2014.09.043 ↗
24. Oxidation behaviour of an Alloy 617 in very high-temperature air and helium environments10.1016/j.ijpvp.2007.11.010 ↗
25. Oxidation/vaporization kinetics of Cr2O310.1111/j.1151-2916.1971.tb12225.x ↗
26. Oxidation characteristics and oxide layer evolution of Alloy 617 and Haynes 230 at 900 °C and 1100 °C10.1007/s11085-009-9142-5 ↗
27. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe–Cr alloys10.1149/1.2424115 ↗
28. Hydrogen effects on oxidation behaviors of Haynes 230 in high temperature steam environments10.1016/j.ssi.2013.04.010 ↗
29. Investigation into the failure mechanism of chromia scale thermally grown on an austenitic stainless steel in pure steam10.1016/j.corsci.2016.03.021 ↗
30. Stress effects in high temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
31. Heterogeneous creep deformations and correlation to microstructures in Fe–30Cr–3Al alloys strengthened by an Fe2Nb laves phase10.1007/s11661-017-4274-8 ↗
32. Formation and stability of oxide layer in FeCrAl fuel cladding material under high-temperature steam10.1016/j.jallcom.2016.05.145 ↗
33. Nanoindentation study on solid solution softening of Fe-rich Fe2Nb laves phase by Ni in Fe–Nb–Ni ternary alloys10.1016/j.intermet.2015.11.003 ↗
34. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
35. Kendall · 2015
36. Niobium oxides and niobates physical properties: review and prospects10.1016/j.pmatsci.2016.02.001 ↗
37. Effect of dissolved oxygen in steam on the corrosion behaviors of zirconium alloys
38. The role of oxide grain boundaries in the development of growth stresses during oxidation10.1016/0010-938X(83)90099-9 ↗
39. Oxidation and mechanical behavior of intermetallic alloys in the Ti–Nb–Al ternary system10.1016/0921-5093(92)90257-2 ↗
40. Oxidation of intermetallic alloys in Ti–Al–Nb ternary system10.5006/1.3315897 ↗
41. Development of high strength ferritic steel for interconnect application in SOFCs10.1016/j.jpowsour.2007.12.028 ↗
42. Effect and role of alloyed Nb on the air oxidation behaviour of Ni–Cr–Fe alloys at 1000 °C10.1016/j.corsci.2017.08.003 ↗