Accelerated test for evaluation of intergranular stress corrosion cracking initiation characteristics of non-sensitized 316 austenitic stainless steel in simulated pressure water reactor environment
Source abstract
Abstract
Abstract Accelerated technique has been developed for evaluation of intergranular stress corrosion cracking (IGSCC) initiation behavior of non-sensitized materials in pressure water reactor environment by means of the implementation of hollowed cylindrical specimens under slow strain rate tensile. Typical IGSCC feature was observed on the fracture surface. The crack depth distribution showed two peaks feature which relates to the worked hardened layer on the inner surface. The specimens tested at lower strain rate showed higher fraction of IGSCC, larger number of cracks initiation, shorter elongation and smaller crack opening displacement, suggesting the transition behavior of IGSCC initiation and short crack growth.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
2. Dependence of stress corrosion cracking for cold-worked stainless steel on temperature and potential, and role of diffusion of vacancies at crack tips10.5006/1.3278507 ↗
3. Cold work and temperature dependence of stress corrosion crack growth of austenitic stainless steels in hydrogenated and oxygenated high-temperature water10.5006/1.3278329 ↗
4. Intergranular stress corrosion cracking behavior of austenitic stainless steels in hydrogenated high-temperature water10.5006/1.3278254 ↗
5. Effects of water chemistry and loading conditions on stress corrosion cracking of cold-rolled 316NG stainless steel in high temperature water10.1016/j.corsci.2010.09.018 ↗
6. IGSCC of non-sensitized stainless steels in high temperature water10.1016/j.jnucmat.2008.08.005 ↗
7. Stress corrosion cracking behavior of alloys in aggressive nuclear reactor core environments10.5006/1.3278331 ↗
8. Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water10.1016/j.corsci.2016.02.030 ↗
9. Modelling of environment assisted cracking10.1016/0010-938X(93)90072-O ↗
10. The effect of dissolved oxygen on fatigue behavior of Alloy 690 steam generator tubes in borated and lithiated high temperature water10.1016/j.corsci.2015.10.032 ↗
11. Role of TiN inclusion on corrosion fatigue behavior of Alloy 690 steam generator tubes in borated and lithiated high temperature water10.1016/j.corsci.2014.07.059 ↗
12. Corrosion fatigue behavior of Alloy 690 steam generator tube in borated and lithiated high temperature water10.1016/j.corsci.2014.08.027 ↗
13. Effect of chemical composition on grain boundary microchemistry and stress corrosion cracking in Alloy 18210.1016/j.corsci.2012.10.012 ↗
14. Characterization of microstructure, local deformation and microchemistry in Alloy 600 heat-affected zone and stress corrosion cracking in high temperature water10.1016/j.corsci.2012.01.029 ↗
15. Stress corrosion cracking of uni-directionally cold worked 316NG stainless steel in simulated PWR primary water with various dissolved hydrogen concentrations10.1016/j.corsci.2011.04.013 ↗
16. Characterization of microstructure and local deformation in 316NG weld heat-affected zone and stress corrosion cracking in high temperature water10.1016/j.corsci.2011.02.009 ↗
17. Formulating stress corrosion cracking growth rates by combination of crack tip mechanics and crack tip oxidation kinetics10.1016/j.corsci.2009.10.041 ↗
18. Mechanistic aspects of intergranular stress corrosion cracking of ferritic steels10.5006/1.3292124 ↗
19. The stress corrosion cracking of reactor pressure vessel steel in high temperature water10.1016/0010-938X(85)90003-4 ↗
20. The stress corrosion cracking of type 316 stainless steel in oxygenated and chlorinated high temperature water10.1016/0010-938X(85)90010-1 ↗
21. Effect of machining-induced surface residual stress on initiation of stress corrosion cracking in 316 austenitic stainless steel10.1016/j.corsci.2016.03.008 ↗
22. Effects of scratching on corrosion and stress corrosion cracking of Alloy 690TT at 58°C and 330°C10.1016/j.corsci.2009.07.015 ↗
23. A sensitive technique for evaluating susceptibility to IGSCC of alloy 600 in high temperature water10.1016/0036-9748(86)90431-X ↗
24. Activation energy for IGSCC of alloy 600 in an aqueous solution containing dissolved H2 at 300–350°C10.1016/0036-9748(87)90404-2 ↗
25. Effect of strain rate on primary water stress corrosion cracking fracture mode and crack growth rate of nickel alloy and austenitic stainless steel10.5006/1.3280631 ↗
26. Technical note: hydrogen induced IGSCC of two unsensitized austenitic stainless steels in high-temperature water10.5006/1.3583908 ↗
27. Effect of hydrogen on the intergranular stress corrosion cracking of Alloy 600 in high temperature aqueous environments10.5006/1.3583894 ↗
28. Mechanical behaviour of SSRT specimens optimized for IGSCC concerns10.1016/j.corsci.2007.10.007 ↗
29. Serrated plastic flow10.1007/BF02743993 ↗
30. Activation energy for serrated flow in a 15Cr–15Ni Ti-modified austenitic stainless steel10.1016/0956-7151(92)90406-5 ↗
31. Microstructural manifestation of dynamic strain aging in AISI 316 stainless steel10.1016/j.jnucmat.2009.10.047 ↗
32. Dynamic strain aging of nickel-base Alloys 800H and 69010.1007/s11661-012-1335-x ↗
33. The effects of strain rate and carbon concentration on the dynamic strain aging of cold rolled Ni-based alloy in high temperature water10.1016/j.scriptamat.2015.05.033 ↗
34. New observations on the mechanisms of dynamic strain aging and of jerky flow10.1016/0001-6160(79)90130-5 ↗
35. Strain aging and strain hardening in Ni–C alloys10.1016/0001-6160(85)90026-4 ↗
36. The problem of the negative strain-rate sensitivity of metals under the portevin-lechatelier deformation conditions10.1016/0001-6160(81)90089-4 ↗
37. Microstructural and mechanical influences on dynamic strain aging phenomena10.1179/imr.1994.39.3.113 ↗
38. Dynamic strain aging effect on the fatigue resistance of type 316L stainless steel10.1016/j.ijfatigue.2005.06.037 ↗
39. Mechanism of dynamic strain aging and characterization of its effect on the low-cycle fatigue behavior in type 316L stainless steel10.1016/j.jnucmat.2004.12.012 ↗
40. The role of dynamic strain-ageing in the environment assisted cracking observed in pressure vessel steels10.1111/j.1460-2695.1997.tb00396.x ↗
41. Interaction between blue brittleness and stress corrosion cracking10.1016/S0022-3115(00)00065-9 ↗
42. Dynamic strain aging and hydrogen-induced softening in alpha titanium10.1007/BF02651937 ↗
43. Hydrogen-enhanced localized plasticity-a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
44. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
45. Hydrogen-involved tensile and cyclic deformation behavior of low-alloy pressure vessel steel10.1007/s11661-004-0256-8 ↗
46. Stress corrosion cracking susceptibility of nickel-molybdenum alloys by slow strain rate and immersion testing10.5006/1.3292154 ↗
47. Progression markings, striations, and crack-arrest markings on fracture surfaces10.1016/j.msea.2006.09.083 ↗
48. Mechanistic and fractographic aspects of stress corrosion cracking10.1515/corrrev-2012-0501 ↗
49. Metallographic contributions to understanding mechanisms of environmentally assisted cracking10.1016/0026-0800(89)90016-5 ↗
50. Testing the film-induced cleavage model of stress-corrosion cracking10.1016/0010-938X(93)90174-F ↗
51. Role of slip step emergence in the early stages of stress corrosion cracking in face centered iron–nickel–chromium alloys10.5006/0010-9312-23.5.117 ↗
52. The kinetics and micromechanics of hydrogen assisted cracking in Fe-3 pct Si single crystals10.1007/BF03350949 ↗
53. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
54. The interaction of strain-rate and repassivation rate in stress corrosion crack propagation10.1016/0010-938X(80)90080-3 ↗
55. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process10.1016/0001-6160(88)90113-7 ↗
56. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
57. Stress corrosion crack coalescence10.5006/1.3585136 ↗
58. In situ Raman spectroscopic investigation of aqueous iron corrosion at elevated temperatures and pressures10.1149/1.1393565 ↗
59. Effects of hydrogen peroxide on corrosion of stainless steel, (V) characterization of oxide film with multilateral surface analyses10.1080/18811248.2006.9711173 ↗
60. Alloy 600 aqueous corrosion at elevated temperatures and pressures: an in situ Raman spectroscopic investigation10.1149/1.3056038 ↗
61. Role of work-hardened surface layer in initiation of environmentally assisted cracking in high-temperature water10.5006/1.3278292 ↗
62. Initiation of environmentally assisted cracking in high-temperature water10.5006/1.3278168 ↗
63. The characterization of damage in SCC by an electrochemical impedance and statistical study of multiple cracking10.1016/0010-938X(94)90172-4 ↗
64. Comprehensive interpretation of CERTs: a method for the characterization and the prediction of IGSCC10.5006/1.3582031 ↗
65. Initiation and propagation of stress corrosion cracking of type 304L austenitic stainless steel in hot aqueous chloride solution10.5006/1.3292160 ↗
66. Lifetime estimation and accelerated stress corrosion cracking test of stainless steel in a neutral chloride environment10.5006/1.3580860 ↗
67. Measurement of small crack lengths under creep-fatigue condition by means of image processing
68. Surface small crack growth behavior in low-cycle fatigue at elevated temperature and application limit of macroscopic crack growth law10.1016/0029-5493(89)90284-7 ↗