Environmentally assisted cracking of forged 316LN stainless steel and its weld in high temperature water
Source abstract
Abstract
Abstract The corrosion fatigue (CF) and stress corrosion cracking (SCC) crack growth rates (CGRs) of type 316LN SS and its welds that are used for pressurized water reactor primary water components were evaluated. Effects on CGRs of loading condition, water chemistry and metallurgical microstructure were studied. Experimental results indicated that stress intensity factor K, loading ratio, and frequency control the CGRs of materials along with corrosion potential, chloride, and pH also significantly influencing the cracking behavior. Similar CGRs under various conditions were observed in the base metal and its weld, with low SCC susceptibility in hydrogenated water, but high SCC susceptibility in oxygenated water. The weld metal showed lower SCC CGRs than base metal in oxygenated high purity water but shifted to higher values after adding ppb levels of chloride because of the presence of δ-ferrite in the weld.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Overview: high-nitrogen alloying of stainless steels10.1016/0921-5093(95)09991-3 ↗
2. Effect of metallurgical variables on the stress corrosion crack growth behaviour of AISI type 316LN stainless steel10.1016/j.corsci.2009.12.031 ↗
3. Stress corrosion cracking of nitrogen-containing stainless steel 316LN in high temperature water environments
4. Evaluation of stress corrosion cracking phenomenon in an AISI type 316LN stainless steel using acoustic emission technique10.1016/j.corsci.2006.06.007 ↗
5. Strain-rate dependent fatigue behavior of 316LN stainless steel in high-temperature water10.1016/j.jnucmat.2017.03.040 ↗
6. Effect of temperature and loading mode on environmentally assisted crack growth of a forged 316L SS in oxygenated high-temperature water10.1016/j.corsci.2014.06.035 ↗
7. Experience and assessment of stress corrosion cracking in L-grade stainless steel BWR internals10.1016/S0029-5493(97)00131-3 ↗
8. IGSCC of non-sensitized stainless steels in high temperature water10.1016/j.jnucmat.2008.08.005 ↗
9. Environmentally assisted cracking of types 304L/316L/316NG stainless steel in 288 C water10.5006/1.3582044 ↗
10. Corrosion fatigue crack growth behaviour of austenitic stainless steels under light water reactor conditions10.1016/j.corsci.2011.10.005 ↗
11. A review of the effects of coolant environments on the fatigue life of LWR structural materials10.1115/1.3027496 ↗
12. Structural evaluation of thermal stratification for PWR surge line10.1016/S0029-5493(97)00224-0 ↗
13. Stress corrosion cracking in low carbon stainless steel components in BWRs
14. Stress corrosion cracking crack growth behavior of type 316L stainless steel weld metals in boiling water reactor environments10.5006/1.3279925 ↗
15. Intergranular cracking of AISI 316NG stainless steel in BWR environment
16. Synergistic effects of local strain-hardening and dissolved oxygen on stress corrosion cracking of 316NG weld heat-affected zones in simulated BWR environments10.1016/j.jnucmat.2011.12.030 ↗
17. Characterization of microstructure and local deformation in 316NG weld heat-affected zone and stress corrosion cracking in high temperature water10.1016/j.corsci.2011.02.009 ↗
18. Effects of water chemistry on stress corrosion cracking of 316NG weld metals in high temperature water10.1179/1743278214Y.0000000186 ↗
19. Role of δ-ferrite in stress corrosion cracking retardation near fusion boundary of 316NG welds10.1016/j.jnucmat.2012.02.006 ↗
20. SCC growth and retardation behavior of low carbon stainless steel piping in the region near the weld fusion boundary
21. Proposed modification to schaeffler diagram for chrome equivalents and carbon for more accurate prediction of martensite content
22. Effects of chloride and oxygen on stress corrosion cracking of cold worked 316/316L austenitic stainless steel in high temperature water10.1016/j.corsci.2016.04.035 ↗
23. SCC crack growth rate of cold worked 316L stainless steel in PWR environment10.1016/j.jnucmat.2014.09.054 ↗
24. Stress corrosion cracking of stainless steels and nickel alloys in high-temperature water10.5006/1.3278457 ↗
25. Effects of water chemistry and loading conditions on stress corrosion cracking of cold-rolled 316NG stainless steel in high temperature water10.1016/j.corsci.2010.09.018 ↗
26. Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water10.1016/j.corsci.2016.02.030 ↗
27. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water10.1016/j.corsci.2016.12.011 ↗
28. Corrosion fatigue and microstructural characterisation of Type 316 austenitic stainless steels tested in PWR primary water10.1016/j.corsci.2017.10.022 ↗
29. Influence of hold times on fatigue crack growth of austenitic stainless steel in PWR environments and implications for mechanistic understanding
30. Effects of material composition on corrosion fatigue crack growth of austenitic stainless steels in high temperature water
31. ASME, Code Case N-809, Boston, Massachusetts, USATechnical Basis for Code Case N-809 on Reference Fatigue Crack Growth Curves for Austenitic Stainless Steels in Pressurized Water Reactor Environments2015
32. Effect of rising and falling K profiles on SCC growth rates in high-temperature water
33. Andresen · 2007
34. Characterization of the roles of electrochemistry, convection and crack chemistry in stress corrosion cracking
35. Effect of corrosion potential on the corrosion fatigue crack growth behaviour of low-alloy steels in high-temperature water10.1016/j.jnucmat.2007.10.010 ↗
36. Plastic strain and residual stress distributions in an AISI 304 stainless steel BWR pipe weld10.1002/9781118456835.ch244 ↗
37. Stress corrosion cracking of current structural materials in commercial nuclear power plants10.5006/0801 ↗
38. Deformation localisation and EAC in inhomogeneous microstructures of austenitic stainless steels
39. Effects of yield strength, corrosion potential, stress intensity factor, silicon and grain boundary character on the SCC of stainless steels
40. Quantification of yield strength effects on IGSCC of austenitic stainless steels in high temperature water
41. Characterizing environmental degradation in PWRs by 3D FIB sequential sectioning10.1007/978-3-319-48760-1_60 ↗
42. Development and use of a predictive model of crack propagation in 304/316L, A533B/A508 and Inconel 600/182 alloys in 288℃ water