Molten salt corrosion (FLiNaK) of a Ni–Mo–Cr alloy and its welds for application in energy-generation and energy-storage systems
Source abstract
Abstract
Abstract The molten salt corrosion performance of a Ni–Mo–Cr (GH3535) alloy weldment, produced using matching filler metal, was assessed. Corrosion testing was performed in FLiNaK molten salt at 750 °C for 500 h. Present results reveal that, despite a similar chemical composition, the weld metal has somewhat superior corrosion resistance to the parent metal. The difference is primarily attributed to the significantly lower density of high-angle grain boundaries (HAGBs) in the weld metal. Results further suggest that large M6C carbides present in the parent metal may contribute to corrosion attack of the alloy matrix via galvanic corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. UNFCCC · 2015
2. Williams · 2006
3. High-temperature liquid-fluoride-Salt closed-brayton-Cycle solar power towers10.1115/1.2710245 ↗
4. The molten salt reactor (MSR) in generation IV: overview and perspectives10.1016/j.pnucene.2014.02.014 ↗
5. Safety assessment of molten salt reactors in comparison with light water reactors
6. Molten salts and nuclear energy production10.1016/j.jnucmat.2006.08.017 ↗
7. Thermodynamic properties and phase diagrams of fluoride salts for nuclear applications10.1016/j.jfluchem.2008.07.014 ↗
8. GIF · 2002
9. Sohal · 2010
10. Electrochemical study of the corrosion of a Ni-based alloy GH3535 in molten (Li,Na,K)F at 700 °C10.1016/j.jfluchem.2015.06.014 ↗
11. Effects of SO42− ions on the corrosion of GH3535 weld joint in FLiNaK molten salt10.1016/j.jnucmat.2017.05.020 ↗
12. Review of commercial thermal energy storage in concentrated solar power plants: steam vs. Molten salts10.1016/j.rser.2017.05.084 ↗
13. Corrosion effects between molten salts and thermal storage material for concentrated solar power plants10.1016/j.apenergy.2011.12.057 ↗
14. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
15. Solar thermal energy with molten-salt storage for residential heating application10.1016/j.egypro.2017.03.134 ↗
16. Comptroller General of the United States · 1963
17. The aircraft reactor experiment - design and construction10.13182/NSE57-A35495 ↗
18. The molten salt reactor adventure10.13182/NSE90-374 ↗
19. Chemistry and technology of Molten Salt Reactors – history and perspectives10.1016/j.jnucmat.2006.08.008 ↗
20. Generation IV advanced nuclear energy systems
21. Canada’s generation IV national program
22. Holcomb · 2013
23. Considerations of alloy N code extension for commercial molten salt reactor development and deployment
24. Material performance in molten salts
25. Generation IV International Forum: A decade of progress through international cooperation10.1016/j.pnucene.2014.02.010 ↗
26. Materials challenges for generation IV nuclear energy systems10.13182/NT08-A3961 ↗
27. Structural materials for Gen-IV nuclear reactors: challenges and opportunities10.1016/j.jnucmat.2008.08.044 ↗
28. Structural materials challenges for advanced reactor systems10.1016/j.jnucmat.2008.11.026 ↗
29. Khanna · 2002
30. Corrosion in molten salts10.1016/B978-0-12-398538-5.00012-3 ↗
31. Corrosion of 316L stainless steel alloy and Hastelloy-N superalloy in molten eutectic LiF-NaF-KF salt and interaction with graphite10.13182/NT13-95 ↗
32. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
33. Corrosion of reduced activation ferritic martensitic steel JLF-1 in purified FLiNaK at static and flowing conditions10.1016/j.fusengdes.2010.03.064 ↗
34. Long-term corrosion behaviors of Hastelloy-N and Hastelloy-B3 in moisture-containing molten FLiNaK salt environments10.1016/j.jnucmat.2013.11.045 ↗
35. Effect of moisture on corrosion of Ni-based alloys in molten alkali fluoride FLiNaK salt environments10.1016/j.jnucmat.2013.02.021 ↗
36. High temperature corrosion studies in molten salt-FLiNaK, Corrosion Engineering
37. Preparation of high-purity molten FLiNaK salt by the hydrofluorination process10.1016/j.jfluchem.2017.03.006 ↗
38. Chapter 1: basic understanding of weld corrosion
39. Material corrosion in molten fluoride salts10.20964/2018.05.33 ↗
40. Impact of corrosion test container material in molten fluorides10.1115/1.4031682 ↗
41. Sabharwall · 2010
42. Effects of exposing temperature on corrosion performance of weld joint of a Ni–Mo–Cr alloy10.1016/j.jfluchem.2015.12.005 ↗
43. Effects of exposing duration on corrosion performance in weld joint of Ni-Mo-Cr alloy in FLiNaK molten salt10.1016/j.jfluchem.2016.07.007 ↗
44. Evolution of carbide precipitates in Hastelloy N joints during welding and post weld heat treatment10.1016/j.matchar.2017.11.045 ↗
45. MATLAB · 2018
46. Texture analysis with MTEX – free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
47. Fluoride salts and container materials for thermal energy storage applications in the temperature range 973 to 1400 K
48. Intergranular corrosion of high temperature alloys in molten fluoride salts10.3184/096034010X12743509428336 ↗
49. DeVan · 1969
50. Effect of SO42− on the corrosion of 316L stainless steel in molten FLiNaK salt10.1016/j.corsci.2018.08.057 ↗
51. Corrosion of Incoloy 800H alloys with nickel cladding in FLiNaK salts at 850 °C10.1016/j.corsci.2018.01.026 ↗
52. Corrosion performance of Ni-16%wt.Mo-X%wt.SiC alloys in FLiNaK molten salt10.1016/j.corsci.2018.08.036 ↗
53. Chase · 1998
54. The effect of cold-rolling on the microstructure and corrosion behaviour of 316L alloy in FLiNaK molten salt10.1016/j.corsci.2018.07.006 ↗
55. Microstructure and local strains in GH3535 alloy heat affected zone and their influence on the mechanical properties10.1016/j.msea.2017.05.072 ↗
56. Microstructure and mechanical properties of Fiber laser welded GH3535 superalloy10.1016/j.jmst.2016.11.026 ↗
57. Temperature dependence of nickel ion irradiation damage in GH3535 alloy weld metal10.1016/j.jnucmat.2017.06.005 ↗
58. Characterization of complex carbide–silicide precipitates in a Ni–Cr–Mo–Fe–Si alloy modified by welding10.1016/j.matchar.2015.05.001 ↗
59. Phase instability in Hastelloy N
60. Effect of long-term thermal exposure on microstructure and stress rupture properties of GH3535 superalloy10.1016/j.jmst.2014.07.021 ↗
61. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
62. Effect of composition and structure on crevice, intergranular, and stress corrosion of some wrought Ni-Cr-Mo alloys10.5006/0010-9312-32.3.79 ↗
63. Galvanic corrosion of Al alloys—III10.1016/S0010-938X(75)80019-9 ↗
64. Influence of cathode-to-anode area ratio and separation distance on galvanic corrosion currents of steel in concrete containing chlorides10.1016/0008-8846(95)00094-S ↗
65. Wire-feed additive manufacturing of metal components: technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
66. Measurement of Gibbs energies of formation of CoF2 and MnF2 using a new composite dispersed solid electrolyte10.1007/BF02744391 ↗
67. Schaefer · 1976
68. Standard free energies of formation of metal fluorides by solid electrolytic galvanic cell method I. Metal difluorides10.1149/1.2134208 ↗
69. Jehn · 1989 · Vol. B5