journal article·2020-03

Anodisation of aluminium alloy AA7075 – Influence of intermetallic particles on anodic oxide growth

Fan Zhang, Cem Örnek, Jan-Olov Nilsson, Jinshan Pan

Corrosion Science· Volume 164
Publisher page

Abstract

Abstract Microstructure and Volta-potential analyses were conducted to characterise intermetallic-particles (IMPs) in AA7075-T5. EIS and AFM were applied under operando-conditions to investigate anodisation processes. IMPs have pronounced influence on the growth of anodic aluminium oxide (AAO) films resulting in low charge-transfer resistance. Cu-bearing constituents show cathodic-character, whereas Mg2Si and MgZn2 particles show anodic-character. During anodisation, Al7Cu2Fe remain stable with peripheral-dissolution around boundary. De-alloying of S-phase particles leads to the detachment. Mg2Si undergoes de-alloying at low potential, and re-passivation at high potential. MgZn2 dissolves entirely upon anodization. Localised-dissolution in large-IMPs boundaries or nanometre-sized IMPs facilitates bubble evolution, confirming local breakdown of barrier-layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. High strength Al-alloys: microstructure, corrosion and principles of protection
2. Analysis of precipitate density of an aluminium alloy by TEM and AFM10.1590/0370-44672016690019 ↗
3. Characterisation of structural similarities of precipitates in Mg–Zn and Al–Zn–Mg alloys systems
4. Corrosion behaviour of different tempers of AA7075 aluminium alloy10.1016/j.electacta.2004.01.046 ↗
5. Effect of solution heat treatment on galvanic coupling between intermetallics and matrix in AA7075-T610.1016/S0010-938X(03)00004-0 ↗
6. Electrochemical behavior and localized corrosion associated with Al7Cu2Fe particles in aluminum alloy 7075-T65110.1016/j.corsci.2006.02.007 ↗
7. Effect of Cu content on corrosion behavior of 7xxx series aluminum alloys10.1149/1.1695385 ↗
8. Dissolution behavior of Al2CuMg (S phase) in chloride and chromate conversion coating solutions10.1149/1.2177005 ↗
9. Schütze · 2010
10. Dealloying of Al2Cu, Al7Cu2Fe, and Al2CuMg intermetallic phases to form nanoparticulate copper films10.1002/maco.201307550 ↗
11. Integration of electrochemical and synchrotron-based x-ray techniques for in-situ investigation of aluminum anodization10.1016/j.electacta.2017.04.154 ↗
12. Anodization of Al (100), Al (111) and Al Alloy 6063 studied in situ with x-ray reflectivity and electrochemical impedance spectroscopy10.1016/j.jelechem.2017.07.010 ↗
13. In situ anodization of aluminum surfaces studied by x-ray reflectivity and electrochemical impedance spectroscopy10.1063/1.4890318 ↗
14. Electrochemical characteristics of intermetallic phases in aluminum alloys an experimental survey and discussion10.1149/1.1869984 ↗
15. Volta potential evolution of intermetallics in aluminum alloy microstructure under thin aqueous adlayers: a combined DFT and experimental study10.1007/s11244-018-0939-9 ↗
16. Preferential anodic oxidation of second‐phase constituents during anodising of AA2024‐T3 and AA7075‐T6 alloys10.1002/sia.3191 ↗
17. Characterization of AA2024‐T3 by scanning kelvin probe force microscopy10.1149/1.1838633 ↗
18. In-situ monitoring of alloy dissolution and residual film formation during the pretreatment of Al-alloy AA2024-T310.1149/2.1121605jes ↗
19. Nano-scale dissolution phenomena in Al–Cu–Mg alloys10.1016/j.elecom.2007.10.032 ↗
20. Atomic emission spectroelectrochemical investigation of the anodization of AA7050T74 aluminum alloy10.1016/j.elecom.2010.11.008 ↗
21. Anodisation of aluminium alloys by micro-capillary technique as a tool for reliable, cost-efficient, and quick process parameter determination10.1155/2016/1374897 ↗
22. Detection of nanoscale η‐MgZn2 phase dissolution from an Al‐Zn‐Mg‐Cu alloy by electrochemical microtransients10.1002/sia.2868 ↗
23. In situ and operando AFM and EIS studies of anodization of Al 6060: influence of intermetallic particles10.1149/2.0061610jes ↗
24. Evaluation of a simple microstructural-electrochemical model for corrosion damage accumulation in microstructurally complex aluminum alloys10.1016/j.engfracmech.2008.11.003 ↗
25. Modelling the anodizing behaviour of aluminium alloys in sulphuric acid through alloy analogues10.1016/j.corsci.2008.09.019 ↗
26. On the nature of the Fe-bearing particles influencing hard anodizing behavior of AA 7075 extrusion products10.1007/s11661-998-1007-z ↗
27. Pulsed current effect on hard anodizing process of 7075-T6 aluminium alloy10.1016/j.surfcoat.2015.03.010 ↗
28. Study of the electrochemical behaviour of the 7075 aluminum alloy in the presence of sodium oxalate10.1016/S0010-938X(98)00164-4 ↗
29. Orazem · 2011
30. Electrochemical impedance spectroscopy analysis on the electrochemical dissolution of aluminum in an alkaline solution10.1016/S0022-0728(03)00266-3 ↗
31. Technical note: concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
32. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
33. Stability, reactivity and breakdown of passive films. Problems of recent and future research10.1016/S0013-4686(00)00347-9 ↗
34. On the Volta potential measured by SKPFM–fundamental and practical aspects with relevance to corrosion science
35. Passive film characterisation of duplex stainless steel using scanning Kelvin prove force microscopy in combination with electrochemical measurements
36. Unusual correlation between SKPFM and corrosion of nickel aluminum bronzes10.1149/2.0391709jes ↗
37. Characterization of 475 C embrittlement of duplex stainless steel microstructure via scanning kelvin probe force microscopy and magnetic force microscopy10.1149/2.0311706jes ↗
38. Corrosion inhibition of aluminum alloy AA6063-T5 by vanadates: microstructure characterization and corrosion analysis10.1149/2.0341803jes ↗
39. Challenges in modeling electrochemical reaction energetics with polarizable continuum models10.1021/acscatal.8b02793 ↗
40. G. Bengough, J. Stuart, The anodic oxidation of aluminium and its alloys as a protection against corrosion, British Patent, 223994 (1923).
41. Effects of hydroxide ion addition on anodic dissolution of pure aluminium in chloride ion-containing solution10.1016/S0013-4686(99)00164-4 ↗
42. A method developed for getting kinetic information from electrochemical impedance spectroscopy measured for anodized Ti in fluoride10.1149/2.016310jes ↗
43. Characterization of surface films formed on aluminum during mass-transfer limited anodic dissolution in phosphoric acid10.1149/2.0731702jes ↗
44. The behavior of aluminum in alkaline media10.1016/S0010-938X(00)00055-X ↗
45. Electrochemical impedance spectroscopy as a tool to obtain mechanistic information on the passive behaviour of aluminium10.1016/0013-4686(95)00462-9 ↗
46. An EIS study of aluminium barrier-type oxide films formed in different media10.1016/0013-4686(92)85124-4 ↗
47. A FEM model for investigation of micro-galvanic corrosion of Al alloys and effects of deposition of corrosion products10.1016/j.electacta.2016.01.179 ↗
48. Investigation and discussion of characteristics for intermetallic phases common to aluminum alloys as a function of solution pH10.1149/1.2829897 ↗
49. Investigation of intrinsic mechanisms of aluminium anodization processes by analyzing the current density10.1039/c2ra01050j ↗
50. Corrosion of aluminium in acidic and neutral solutions10.1016/0013-4686(93)80329-X ↗
51. On the intrinsic electrochemical nature of the inductance in EIS: a Monte Carlo simulation of the two-consecutive-step mechanism: The flat surface 2 D case10.1016/j.electacta.2008.07.023 ↗
52. Three-dimensional impedance spectroscopy diagrams for processes involving electrosorbed intermediates, introducing the third electrode-potential variable—examination of conditions leading to pseudo-inductive behavior10.1016/0013-4686(93)80302-G ↗
53. Thin anodic oxide layers on aluminium and other valve metals: high field regime10.1016/0927-796X(93)90005-N ↗
54. Localized corrosion of 2024 T351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
55. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024‐T310.1149/1.1837874 ↗
56. Electronic currents and the formation of nanopores in porous anodic alumina10.1088/0957-4484/20/47/475303 ↗
57. Self-assembly of periodic serrated nanostructures10.1021/cm8022242 ↗
58. Studies of oxide growth location on anodization of Al and Ti provide evidence against the field-assisted dissolution and field-assisted ejection theories10.1016/j.elecom.2018.01.003 ↗
59. Cavities between the double walls of nanotubes: evidence of oxygen evolution beneath an anion-contaminated layer10.1016/j.elecom.2018.03.009 ↗
60. The mechanism of hydrogen evolution during anodic polarization of aluminium10.1016/j.electacta.2015.08.076 ↗