journal article·2021-12

CMAS corrosion behavior of Sc doped Gd2Zr2O7 /YSZ thermal barrier coatings and their corrosion resistance mechanisms

Bowen Li, Jingyong Sun, Lei Guo

Corrosion Science· Volume 193
Publisher page

Abstract

Abstract YSZ thermal barrier coatings (TBCs) are vulnerable to calcium-magnesium-alumina-silicate (CMAS) attack, and a CMAS resistant TBC of Sc doped Gd2Zr2O7/YSZ are developed in this study. At 1250 ℃, corrosion products form a reaction layer at the CMAS/coating interface, which largely suppresses CMAS further infiltration. Compared with Gd2Zr2O7, Sc doped Gd2Zr2O7 has a higher ability to keep its lattice structure in the presence of CMAS, which is beneficial to maintain the coating microstructure under CMAS conditions, alleviating the coating degradation. First-principles calculation was conducted to investigate the corrosion products formation mechanisms, and the characteristics of CMAS/reaction layer and reaction layer/coating interfaces.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Overview on advanced thermal barrier coatings10.1016/j.surfcoat.2010.08.151 ↗
2. Problems of aircraft engine thermal barrier coating and its developing direction
3. Progress in research on high temperature protective coatings for aero-engines
4. Progress update on failure mechanisms of advanced thermal barrier coatings: a review10.1016/j.porgcoat.2015.09.019 ↗
5. Plasma sprayed thermal barrier coatings: new materials, processing issues and solutions10.1007/s11666-013-9889-8 ↗
6. Phase stability of t′-zirconia-based thermal barrier coatings: mechanistic insights
7. Process maps for plasma spraying of yttria-stabilized zirconia: an integrated approach to design, optimization and reliability10.1016/j.msea.2008.07.058 ↗
8. Effect of thermal treatment on the grain growth of nanostructured YSZ thermal barrier coating prepared by air plasma spraying10.1016/S1000-9361(11)60224-0 ↗
9. Experimental and numerical investigation on the thermal and mechanical behaviors of thermal barrier coatings exposed to CMAS corrosion10.1007/s40145-021-0457-2 ↗
10. CMAS corrosion behavior and protection method of thermal barrier coatings for aeroengine
11. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
12. Zirconia and pyrochlore oxides for thermal barrier coatings in gas turbine engines
13. Thermal shock resistance and failure mechanism of CMAS deposited PS-PVD 7YSZ coating
14. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
15. Jet engine coatings for resisting volcanic ash damage10.1002/adma.201004783 ↗
16. Microstructures and mechanical properties of Gd2Zr2O7/ZrO2(3Y) ceramics10.1016/j.jallcom.2015.05.054 ↗
17. Toughening effect of Yb2O3 stabilized ZrO2 doped in Gd2Zr2O7 ceramic for thermal barrier coatings10.1016/j.msea.2015.09.081 ↗
18. Mechanical properties of zirconia composite ceramics10.1016/j.ceramint.2013.03.014 ↗
19. Strong and tough metal/ceramic micro-laminates10.1016/j.actamat.2017.10.059 ↗
20. Enhanced thermal expansion and fracture toughness of Sc2O3-doped Gd2Zr2O7 ceramics10.1016/j.ceramint.2015.05.008 ↗
21. Mechanism of crack nucleation and growth in YSZ thermal barrier coatings corroded by CMAS at high temperatures: first-principles calculation10.1016/j.corsci.2018.07.033 ↗
22. High-temperature corrosion mechanism of YSZ coatings subject to calcium-magnesium-aluminosilicate (CMAS) deposits: first-principles calculations10.1016/j.corsci.2017.07.010 ↗
23. Corrosion behavior and thermos-physical properties of a promising Yb2O3 and Y2O3 co-stabilized ZrO2 ceramic for thermal barrier coatings subject to calcium-magnesium-aluminum-silicate (CMAS) deposition: experiments and first-principles calculation10.1016/j.corsci.2020.109230 ↗
24. Hot corrosion behavior of (Gd0.9Sc0.1)2Zr2O7 in V2O5 molten salt at 700-1000 ℃10.1016/j.ceramint.2017.04.048 ↗
25. Preparation of (Gd0.9Sc0.1)2Zr2O7/YSZ thermal barrier coatings and their corrosion resistance to V2O5 molten salt10.1016/j.surfcoat.2020.125677 ↗
26. Thermal spray coatings engineered from nanostructured ceramic agglomerated powders for structural, thermal barrier and biomedical applications: a review10.1007/s11666-006-9010-7 ↗
27. Corrosion resistance of non-stoichiometric gadolinium zirconate fabricated by laser-enhanced chemical vapor deposition10.1007/s40145-020-0454-x ↗
28. Effects of laser glazing on CMAS corrosion behavior of Y2O3 stabilized ZrO2 thermal barrier coatings10.1016/j.corsci.2019.06.025 ↗
29. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
30. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set10.1016/0927-0256(96)00008-0 ↗
31. Generalized gradient approximation for the exchange-correlation hole of a many-electron system10.1103/PhysRevB.54.16533 ↗
32. Infiltration mechanism of Ca-Mg-Al-silicate (CMAS) melt on Yttria stabilized zirconia (YSZ) columnar crystal at high temperature: first-principles research10.1016/j.apsusc.2020.145712 ↗
33. Influence of Yb:Hf ratio on ytterbium hafnate/molten silicate (CMAS) reactivity10.1111/jace.13964 ↗
34. EB-PVD alumina (Al2O3) as a top coat on 7YSZ TBCs against CMAS/VA infiltration: Deposition and reaction mechanisms10.1016/j.jeurceramsoc.2018.03.027 ↗
35. Erosion performance of atmospheric plasma sprayed thermal barrier coatings with diverse porosity levels10.3390/coatings11010086 ↗
36. Thermal shock resistances of nanostructured and conventional zirconia coatings deposited by atmospheric plasma spraying10.1016/j.surfcoat.2004.08.225 ↗
37. An investigation on erosion behavior of nanostructured 7YSZ coatings at elevated temperature10.1016/j.surfcoat.2016.05.003 ↗
38. Self-crystallization characteristics of calcium-magnesium-alumina-silicate (CMAS) glass under simulated conditions for thermal barrier coating applications10.1016/j.jeurceramsoc.2020.07.025 ↗
39. Plasma sprayed gadolinium zirconate thermal barrier coatings that are resistant to damage by molten Ca-Mg-Al-silicate glass10.1016/j.surfcoat.2012.03.051 ↗
40. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca-Mg-Al-silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
41. Raman spectra of oxides with the fluorite structure10.1063/1.1680227 ↗
42. The structural transformation from the pyrochlore structure, A2B2O7, to the fluorite structure, AO2, studied by Raman spectroscopy and defect chemistry modeling10.1006/jssc.2000.9142 ↗
43. Determination of cubic-tetragonal phase boundary in Zr1−xYxO2−x/2 solid solutions by Raman spectroscopy10.1063/1.354989 ↗
44. Thermochemistry of calcium rare-earth silicate oxyapatites
45. Corrosion behavior of Sc2O3-Y2O3 co-stabilized ZrO2 thermal barrier coatings with CMAS attack10.1016/j.ceramint.2019.05.063 ↗
46. Environmental-barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part II, β-Yb2Si2O7 and β-Sc2Si2O710.1016/j.jeurceramsoc.2018.03.010 ↗
47. Corrosion products evolution and hot corrosion mechanisms of REPO4 (RE=Gd, Nd, La) in the presence of V2O5+ Na2SO4 molten salt10.1016/j.jeurceramsoc.2018.10.031 ↗
48. CaO-MgO-Al2O3-SiO2(CMAS) Corrosion of Gd2Zr2O7 and Sm2Zr2O710.1149/2.0301610jes ↗
49. Transient and steady states of Gd2Zr2O7 and 2ZrO2∙Y2O3 (ss) interactions with calcium magnesium aluminum silicates10.1016/j.jeurceramsoc.2018.12.016 ↗
50. CMAS resistance characteristics of LaPO4/YSZ thermal barrier coatings at 1250 ℃-1350 ℃10.1016/j.corsci.2019.04.014 ↗
51. Comparative study of EB-PVD gadolinium-zirconate and yttria-rich zirconia coatings performance against Fe-containing calcium-magnesium-aluminosilicate (CMAS) infiltration10.1016/j.corsci.2021.109660 ↗
52. Volcanic ash-induced decomposition of EB-PVD Gd2Zr2O7 thermal barrier coatings to Gd-oxyapatite, zircon, and Gd, Fe-zirconolite10.1111/jace.12251 ↗
53. Optical temperature sensing using upconversion luminescence in rare-earth ions doped Ca2Gd8(SiO4)6O2 phosphors10.1016/j.jallcom.2018.09.022 ↗
54. Mechanochemical synthesis of ultrafine ZrO2 powder10.1016/S0965-9773(97)00067-6 ↗
55. High temperature thermal expansion of BaAl2Si2O8, CaAl2Si2O8, and Ca2Al2SiO7 studied by high-temperature X-ray diffraction (HT-XRD)10.1016/j.solidstatesciences.2014.10.010 ↗
56. Enthalpy of formation of wollastonite (CaSiO3) and anorthite (CaAl2Si2O8) by experimental phase equilibrium measurements and high-temperature solution calorimetry
57. Influence of partial substitution of Sc2O3 with Gd2O3 on the phase stability and thermal conductivity of Sc2O3-doped ZrO210.1016/j.ceramint.2012.09.100 ↗
58. Thermophysical properties of rare earth-stabilized zirconia and zirconate pyrochlores as surrogates for actinide-doped zirconia10.1007/s10765-007-0232-9 ↗
59. The effect of heat treatment on the stiffness of zirconia top coats in plasma-sprayed TBCs10.1016/S1359-6454(01)00065-9 ↗
60. Lattice softening in nanometer-size iron particles10.1103/PhysRevB.44.11689 ↗