Stress corrosion cracking behavior and mechanism of 2205 duplex stainless steel under applied polarization potentials
Source abstract
Abstract
In this work, a non-steady electrochemical model for assessing stress corrosion cracking (SCC) of 2205 duplex stainless steel (DSS) under applied polarization potentials was proposed, and the SCC mechanism was revealed. With the negative shift of potentials, hydrogen enhances SCC susceptibility by deteriorating passive film, inhibiting repassivation and causing serious damage. In particular, at −850 mV (vs. SCE), the synergetic effect of anodic dissolution (AD) and hydrogen embrittlement (HE) causes severe pitting and SCC. The negative shift of applied potentials changes the preferential pit/SCC initiation site due to high hydrogen concentration in austenite.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Effect of cold deformation on the corrosion behaviour of UNS S31803 duplex stainless steel in simulated concrete pore solution10.1016/j.corsci.2017.05.021 ↗
2. Hydrogen effects on passivation and SCC of 2205 DSS in acidified simulated seawater10.1016/j.corsci.2022.110640 ↗
3. Determination of the hydrogen effects on the passive film and the micro-structure at the surface of 2205 duplex stainless steel10.1016/j.apsusc.2021.149597 ↗
4. Insight into electrochemical passivation behavior and surface chemistry of 2205 duplex stainless steel: effect of tensile elastic stress10.1016/j.corsci.2021.109903 ↗
5. Hydrogen embrittlement of duplex stainless steel under cathodic protection in acidic artificial sea water in the presence of sulphide ions10.1016/j.corsci.2005.01.004 ↗
6. Synergistic effect of cold work and hydrogen charging on the pitting susceptibility of 2205 duplex stainless steel10.1016/j.electacta.2019.135081 ↗
7. Effect of hydrogen on pitting susceptibility of 2507 duplex stainless steel10.1016/j.corsci.2013.01.022 ↗
8. Stress corrosion cracking and corrosion fatigue cracking of steels
9. Mechanistic aspect of non-steady electrochemical characteristic during stress corrosion cracking of an X70 pipeline steel in simulated underground water10.5006/1153 ↗
10. Fundamentally understanding the effect of Non-stable cathodic potential on stress corrosion cracking of pipeline steel in Near-neutral pH solution10.1016/j.conbuildmat.2021.123117 ↗
11. Understanding the non-steady electrochemical mechanism on SCC of 304 SS under applied polarization potentials10.1016/j.corsci.2023.111686 ↗
12. Effect of cathodic potentials on the SCC behavior of E690 steel in simulated seawater10.1016/j.msea.2015.05.109 ↗
13. Effect of cathodic polarisation on stress corrosion cracking behaviour of a Ni(Fe, Al)-maraging steel in artificial seawater10.1016/j.corsci.2020.109176 ↗
14. Effect of cathodic protection potential on stress corrosion susceptibility of X80 steel10.1016/j.corsci.2023.111184 ↗
15. Identification of microstructure factors affecting hydrogen embrittlement of a 2205 duplex stainless steel10.1016/j.corsci.2022.110643 ↗
16. Effect of hydrogen trapping on hydrogen permeation in a 2205 duplex stainless steel: role of austenite–ferrite interface10.1016/j.corsci.2022.110332 ↗
17. Stress-assisted microbiologically influenced corrosion mechanism of 2205 duplex stainless steel caused by sulfate-reducing bacteria10.1016/j.corsci.2020.108746 ↗
18. Insights from electrochemical crack tip modeling of atmospheric stress corrosion cracking10.1016/j.corsci.2022.110756 ↗
19. Predictive approaches to stress corrosion cracking failure10.1016/0010-938X(80)90128-6 ↗
20. Li · Constr. Build. Mater. · 2018 · 189 · 128610.1016/j.conbuildmat.2018.08.186 ↗
21. Effect of secondary passivation on corrosion behavior and semiconducting properties of passive film of 2205 duplex stainless steel10.1016/j.jmrt.2021.11.118 ↗
22. Hydrogen-facilitated anodic dissolution of austenitic stainless steels10.5006/1.3284854 ↗
23. Characteristics of hydrogen embrittlement in high-pH stress corrosion cracking of X100 pipeline steel in carbonate/ bicarbonate solution10.1016/j.conbuildmat.2020.120124 ↗
24. Corrosion studies using potentiodynamic and EIS electrochemical techniques of welded lean duplex stainless steel UNS S8244110.1016/j.apsusc.2016.01.260 ↗
25. A comparative study of critical pitting temperature (CPT) of stainless steels by electrochemical impedance spectroscopy (EIS), potentiodynamic and potentiostatic techniques10.1016/j.corsci.2012.02.026 ↗
26. Effects of testing parameters on the susceptibility to hydrogen embrittlement in precipitation-hardened nickel-based alloys: the role of continuous straining10.1016/j.corsci.2022.110171 ↗
27. Sensitivity to hydrogen induced cracking, and corrosion performance of an API X65 pipeline steel in H2S containing environment: influence of heat treatment and its subsequent microstructural changes10.1016/j.jmrt.2021.07.118 ↗
28. Promotion of pitting corrosion at hydrogen-enriched α/γ phase boundaries in austenitic stainless steel weld joints10.1016/j.actamat.2022.117728 ↗
29. Evolution of dissolution processes at the interface of carbon steel corroding in a CO2 environment studied by EIS10.1016/j.corsci.2009.10.007 ↗
30. Consequences of mobile and trapped hydrogen on the dissolution kinetics and pitting processes of an austenitic stainless steel10.1016/j.corsci.2022.110546 ↗
31. The influence of nitrogen and molybdenum on passive films formed on the austenoferritic stainless steel 2205 studied by AES and XPS10.1016/0010-938X(94)00148-Y ↗
32. Electrochemical investigations on formation and pitting susceptibility of passive films on iron and iron-based alloys10.1016/S1452-3981(23)17101-X ↗
33. Effect of plastic deformation on the electrochemical and stress corrosion cracking behavior of X70 steel in near-neutral pH environment10.1016/j.msea.2016.09.033 ↗
34. Effect of AC current density on the stress corrosion cracking behavior and mechanism of E690 high-strength steel in simulated seawater10.1007/s11665-019-04405-4 ↗
35. Microstructure evolution and SSCC behavior of strain-strengthened 304 SS pre-strained at room temperature and cryogenic temperature10.1016/j.corsci.2022.110855 ↗
36. Temperature change induce crack mode transition of 316L stainless steel in H2S environment revealed by dislocation configurations10.1016/j.corsci.2021.109896 ↗
37. The mechanism of hydrogen-induced pitting corrosion in duplex stainless steel studied by SKPFM10.1016/j.corsci.2012.04.010 ↗
38. The mechanism of hydrogen-facilitated anodic-dissolution-type stress corrosion cracking: theories and experiments10.1080/01418610108216638 ↗
39. The effects of hydrogen on anodic dissolution and passivation of iron in alkaline solutions10.1016/j.corsci.2015.09.013 ↗
40. Crack growth behaviour of E690 steel in artificial seawater with various pH values10.1016/j.corsci.2019.108336 ↗
41. Stress corrosion cracking of E690 steel as a welded joint in a simulated marine atmosphere containing sulphur dioxide10.1016/j.corsci.2015.08.039 ↗
42. Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking10.1016/j.msea.2011.03.036 ↗
43. Edge dislocations emitted along multiple inclined slip planes from a Mode I crack. I. Sequential emission10.1016/0167-6636(96)00024-5 ↗
44. The role of hydrogen in stress corrosion cracking of 310 austenitic stainless steel in a boiling MgCl2 solution10.1016/j.corsci.2012.03.026 ↗
45. The effect of crack tip environment on crack growth behaviour of a low alloy steel at cathodic potentials in artificial seawater10.1016/j.jmst.2020.04.034 ↗
46. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
47. A decohesion pathway for hydrogen embrittlement in nickel: mechanism and quantitative prediction10.1016/j.actamat.2019.11.062 ↗
48. Effects of hydrogen and stress on the electrochemical and passivation behaviour of 304 stainless steel in simulated PEMFC environment10.1016/j.electacta.2018.10.028 ↗
49. Local additional potential model for effect of strain rate on SCC of pipeline steel in an acidic soil solution10.1016/j.corsci.2009.08.019 ↗
50. Hydrogen embrittlement of super duplex stainless steel – Towards understanding the effects of microstructure and strain10.1016/j.ijhydene.2018.05.028 ↗
51. Compatible strain evolution in two phases due to epsilon martensite transformation in duplex TRIP-assisted stainless steels with high hydrogen embrittlement resistance10.1016/j.ijplas.2016.09.012 ↗
52. Hydrogen-assisted cracking in 2205 duplex stainless steel: initiation, propagation and interaction with deformation-induced martensite10.1016/j.msea.2020.140079 ↗
53. Slip transmission and voiding during slip band Intersections in Fe70Ni10Cr20 stainless steel10.1016/j.scriptamat.2022.114925 ↗
54. First observation by EBSD of martensitic transformations due to hydrogen presence during straining of duplex stainless steel10.1016/j.matchar.2019.109843 ↗
55. Hydrogen-induced strain localization and failure of austenitic stainless steels at high hydrogen concentrations10.1016/0956-7151(91)90211-I ↗