Long-term ablation behavior and mechanisms of 2D-Cf/ZrB2-SiC composites at temperatures up to 2400 °C

Bo-Wen Chen, De-Wei Ni, Chun-Jing Liao, You-Lin Jiang, Jun Lu, Shao-Ming Dong

Corrosion Science· Volume 177
Publisher page

Abstract

Abstract Long-term ablation behavior and mechanisms of 2D-Cf/ZrB2-SiC composites are studied by air plasma test at temperatures up to 2400 °C. After ablation at temperatures lower than 1800 °C for 60 s, a porous SiO2 layer forms on the sample surface, which turns to a continuous ZrO2-SiO2 glassy layer at higher temperatures (2000−2400 °C). As ablation temperature increases and ablation time extends, ZrO2 grains are precipitated from the ZrO2-SiO2 glass, further coarsening and sintered via a quasi-liquid phase assisted route, finally form a dense ceramic layer. Consequently, the 2D-Cf/ZrB2-SiC composites show a superior anti-ablation property even at 2400 °C for 300 s.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Ablation behavior of C/C-ZrC and C/SiC-ZrC composites fabricated by a joint process of slurry impregnation and chemical vapor infiltration10.1016/j.ceramint.2017.12.062 ↗
2. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs – a review
3. Carbon fiber reinforced ultra-high temperature ceramic matrix composites: a review10.1016/j.ceramint.2019.05.065 ↗
4. Effect of ZrC amount and distribution on the thermomechanical properties of Cf/SiC-ZrC composites10.1111/ijac.13217 ↗
5. Ablation behavior of Cf/ZrC-SiC-based composites fabricated by an improved reactive melt infiltration10.1016/j.jeurceramsoc.2019.07.007 ↗
6. Fabrication and properties of Cf/ZrC-SiC-based composites by an improved reactive melt infiltration10.1111/jace.15534 ↗
7. Effects of surface structure unit of 2D needled carbon fiber preform on the microstructure and ablation properties of C/C-ZrC-SiC composites10.1016/j.ceramint.2019.03.078 ↗
8. Characterization and mechanical properties of Cf/ZrB2-SiC composites fabricated by a hybrid technique based on slurry impregnation, polymer infiltration and pyrolysis and low-temperature hot pressing10.1016/j.ceramint.2018.12.001 ↗
9. Oxidation behavior and ablation mechanism of Cf/ZrB2-SiC composite fabricated by vibration-assisted slurry impregnation combined with low-temperature hot pressing10.1016/j.corsci.2019.108181 ↗
10. Microstructures and mechanical properties of Cf/ZrB2-SiC composite fabricated by nano slurry brushing combined with low-temperature hot pressing10.1016/j.jallcom.2019.03.147 ↗
11. A novel vibration-assisted slurry impregnation to fabricate Cf/ZrB2-SiC composite with enhanced mechanical properties10.1016/j.jeurceramsoc.2018.10.029 ↗
12. Effects of preform pore structure on infiltration kinetics and microstructure evolution of RMI-derived Cf/ZrC-ZrB2-SiC composite10.1016/j.jeurceramsoc.2019.11.020 ↗
13. Ablation behavior of three-dimensional Cf/SiC-ZrC-ZrB2 composites prepared by a joint process of sol-gel and reactive melt infiltration10.1016/j.corsci.2018.02.011 ↗
14. Interphase degradation of three-dimensional Cf/SiC-ZrC-ZrB2 composites fabricated via reactive melt infiltration10.1111/jace.14983 ↗
15. Influence of fibre content on the strength of carbon fibre reinforced HfC-SiC composites up to 2100 °C
16. Thermal properties of Cf/HfC and Cf/HfC-SiC composites prepared by precursor infiltration and pyrolysis10.1016/j.jeurceramsoc.2017.12.051 ↗
17. Ablation mechanism of Carbon/Carbon composites modified by HfC–SiC in two conditions under oxyacetylene torch10.1016/j.jmst.2016.01.013 ↗
18. Comparative ablation behaviors of C/SiC-HfC composites prepared by reactive melt infiltration and precursor infiltration and pyrolysis routes10.1016/j.ceramint.2017.08.175 ↗
19. Mechanical behaviour of carbon fibre reinforced TaC/SiC and ZrC/SiC composites up to 2100°C10.1016/j.jeurceramsoc.2018.11.017 ↗
20. Ablation behaviour of ultra-high temperature ceramic matrix composites: role of MeSi2 addition10.1016/j.jeurceramsoc.2019.03.031 ↗
21. Influence of SiC content on the oxidation of carbon fibre reinforced ZrB2/SiC composites at 1500 and 1650 °C in air10.1016/j.jeurceramsoc.2018.04.064 ↗
22. The corrosion behavior of CVI SiC matrix in SiCf/SiC composites under molten fluoride salt environment10.1016/j.jnucmat.2017.02.007 ↗
23. Effect of heat treatment on the mechanical properties of SiCf/BN/SiC fabricated by CVI10.1016/j.ceramint.2015.11.030 ↗
24. Thermal and mechanical properties of SiC/SiC-CNTs composites fabricated by CVI combined with electrophoretic deposition10.1016/j.msea.2014.12.105 ↗
25. Properties of Cf/SiC-ZrB2-TaxCy composite produced by reactive hot pressing and polymer impregnation pyrolysis (RHP/PIP)10.1016/j.jeurceramsoc.2019.02.025 ↗
26. Properties and microstructure evolution of Cf/SiC composites fabricated by polymer impregnation and pyrolysis (PIP) with liquid polycarbosilane10.1016/j.ceramint.2017.02.100 ↗
27. Ablation behavior and mechanism of SiC/Zr-Si-C multilayer coating for PIP-C/SiC composites under oxyacetylene torch flame10.1016/j.compositesb.2013.10.033 ↗
28. Improved ablation resistance of C/SiC-ZrB2 composites via polymer precursor impregnation and pyrolysis10.1016/j.ceramint.2017.06.118 ↗
29. Materials characterisation and mechanical properties of Cf-UHTC powder composites10.1016/j.jeurceramsoc.2018.12.043 ↗
30. Reactive melt infiltrated Cf/SiC composites with robust matrix derived from novel engineered pyrolytic carbon structure10.1016/j.ceramint.2017.01.089 ↗
31. 3D Cf/SiC-ZrC-ZrB2 composites fabricated via sol-gel process combined with reactive melt infiltration10.1016/j.jeurceramsoc.2016.04.011 ↗
32. Microstructure and mechanical properties of three dimensional Cf/SiC-ZrC-ZrB2 composites prepared by reactive melt infiltration method10.1016/j.jeurceramsoc.2016.07.002 ↗
33. Ablation behavior of C/C-SiC-ZrB2 composites in simulated solid rocket motor plumes10.1016/j.jallcom.2017.08.114 ↗
34. Oxidation-resistant ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
35. Preparation of SiC layer with sub-micro grain structure in TRISO particles by spouted bed CVD10.1016/j.jeurceramsoc.2019.02.005 ↗