Corrosion mechanism of Ti2AlC MAX phase coatings under the synergistic effects of water vapor and solid NaCl at 600 °C
Source abstract
Abstract
Abstract The corrosion behavior of Ti2AlC MAX phase coatings coated on 1Cr11Ni2W2MoV substrates in NaCl deposit in water vapor at 600 °C has been fully investigated. The results demonstrated that the substrates underwent serious corrosion, but the coatings performed better. The mass gain per unit area of coatings was less than 1/6 of substrates, because of the formed compact and uniform corrosion scale. Such dense corrosion scale was composed of NaxTiyOz fine grains with the size of 11 ± 0.4 nm and amorphous Al2O3 phases which self-healed the generated defects during corrosion, benefiting from the novel layered structure of MAX phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Common failures in gas turbine blades10.1016/j.engfailanal.2004.07.004 ↗
2. Corrosion behavior of Ti60 alloy under a solid NaCl deposit in wet oxygen flow at 600 °C10.1038/srep29019 ↗
3. Effects of the different solid deposits on the corrosion behavior of pure Fe in water vapor at 500 °C10.1155/2020/6280725 ↗
4. Corrosion behavior of Ti60 alloy under a solid NaCl deposit in wet oxygen flow at 600 °C10.1038/srep29019 ↗
5. Effect of streaming water vapor on the corrosion behavior of Ti60 alloy under a solid NaCl deposit in water vapor at 600 °C10.1016/j.corsci.2019.108177 ↗
6. Studies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 °C10.1016/j.corsci.2018.01.033 ↗
7. Effects of pre-oxidation on the corrosion behavior of pure Ti under coexistence of solid NaCl deposit and humid oxygen at 600 °C: the diffusion of chlorine10.1038/s41598-020-73034-y ↗
8. The influence of TiAlN and enamel coatings on the corrosion behavior of Ti6Al4V alloy in the presence of solid NaCl deposit and water vapor at 450 °C10.1016/j.surfcoat.2006.10.038 ↗
9. A new insight into the NaCl-induced hot corrosion mechanism of TiN coatings at 500 °C10.1016/j.corsci.2020.108794 ↗
10. Mechanical properties and oxidation behavior of a graded (Ti,Al)N coating deposited by arc-ion plating10.1007/s11085-006-9015-0 ↗
11. The electrochemical corrosion behavior of TiN and (Ti,Al)N coatings in acid and salt solution10.1016/S0010-938X(02)00223-8 ↗
12. Effects Ti/TiAlN composite multilayer coatings on corrosion resistance of titanium alloy in solid NaCl-H2O-O2 at 600 °C10.1016/j.jallcom.2017.11.035 ↗
13. Studies on corrosion resistance of thick Ti/TiN multilayer coatings under solid NaCl–H2O–O2 at 450 °C10.1016/j.ceramint.2020.04.267 ↗
14. Dense and high-stability Ti2AlN MAX phase coatings prepared by the combined cathodic arc/sputter technique10.1016/j.apsusc.2016.11.183 ↗
15. Studying the oxidation of Ti2AlC MAX phase in atmosphere: a review10.1016/j.ijrmhm.2016.07.006 ↗
16. Deformation of polycrystalline Ti2AlC under compression10.1007/s100190100132 ↗
17. Corrosion behavior of select MAX phases in NaOH, HCl and H2SO410.1016/j.corsci.2006.04.005 ↗
18. Self-healing performance of Ti2AlC ceramic10.1039/c2jm16123k ↗
19. Reducing the self-healing temperature of Ti2AlC MAX phase coating by substituting Al with Sn10.1016/j.jeurceramsoc.2019.09.009 ↗
20. Diffusion-controlled intercalation approach to synthesize the Ti2AlC MAX phase coatings at low temperature of 550 °C10.1016/j.apsusc.2019.144130 ↗
21. Effect of homogenization-pressure-assisted enzymatic hydrolysis on the structural and physicochemical properties of lotus-seed starch nanoparticles10.1016/j.ijbiomac.2020.11.113 ↗
22. Comparative study on oxidation behavior of Ti2AlN coatings in air and pure steam10.1016/j.ceramint.2019.02.004 ↗
23. Synthesis of Ti2AlC & Ti3AlC2 MAX phases by Arc-PVD using Ti–Al target in C2H2/Ar gas mixture and subsequent annealing10.1016/j.ceramint.2019.10.235 ↗
24. Deposition and characterization of phase-pure Ti2AlC and Ti 3AlC2 coatings by DC magnetron sputtering with cost-effective targets10.1016/j.vacuum.2018.04.001 ↗
25. The scaling behavior andmechanismof Ti2AlCMAX phase coatings in air and pure water vapor10.1016/j.surfcoat.2015.03.037 ↗
26. Oxidation behaviour of Ti–Al–C films composed mainly of a Ti2AlC phase10.1016/j.corsci.2011.05.033 ↗
27. A high oxidation resistance Ti2AlC coating on Zirlo substrates for loss-of-coolant accident conditions10.1016/j.ceramint.2019.04.089 ↗
28. Influence of water vapour on the oxidation behaviour of titanium aluminides10.1016/S0966-9795(01)00104-2 ↗
29. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
30. Effect of annealing on microstructure evolution and corrosion resistance of an amorphous Cr-Al-C coating10.1016/j.corsci.2020.109062 ↗
31. Oxidation mechanism of Fe–16Cr alloy as SOFC interconnect in dry/wet air10.1016/j.jallcom.2013.05.072 ↗
32. Corrosion behavior of Ti60 alloy coated with a solid NaCl deposit in O2 plus water vapor at 500–700 °C10.1023/A:1018864216554 ↗
33. Self-healing metal-enamel composite coating and its protection for TiAl alloy against oxidation under thermal shock in NaCl solution10.1016/j.corsci.2020.108526 ↗
34. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature10.1016/j.corsci.2007.06.007 ↗
35. Degradation mechanism of Ti-6Al-2Sn-4Zr-2Mo-Si alloy exposed to solid NaCl deposit at high temperature10.1016/j.corsci.2020.108611 ↗
36. Microstructural characterization of layered ternary Ti2AlC10.1016/j.actamat.2005.10.028 ↗
37. Deposition of aluminium on magnesium by a CVD process10.1016/j.surfcoat.2003.10.065 ↗
38. Corrosion behaviour of electrodeposited Ni/Al2O3 composite coating covered with a NaCl salt film at 800 °C10.1002/maco.200905617 ↗
39. Influence of Al2O3 overlay on corrosion resistance of plasma sprayed yttria-stabilized zirconia coating in NaCl-KCl molten salt10.1016/j.surfcoat.2019.01.054 ↗