Abstract The effects of pre-strain on hydrogen embrittlement of 304L K-TIG welded joint were investigated. As pre-strain of joint increased, fracture location of hydrogen-charged joint changed from weld metal to base metal. In low prestrained joints, fracture may be initiated at the sites of clustered dislocations due to hydrogen in weld metal with a high density of pre-existing dislocations. In high prestrained joints, some regions in base metal suffered severe strain-induced α′ martensitic transformation due to Ni depletion bands and cracking occurred at phase boundaries where may provide more sites for the accumulation of hydrogen atoms and dislocations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Peckner · 1977
2. Caskey · 1983
3. A new aspect on intergranular hydrogen embrittlement mechanism of solution annealed types 304, 316 and 310 austenitic stainless steels10.1016/j.corsci.2009.01.031 ↗
4. Effect of austenite instability on the hydrogen-enhanced crack growth of austenitic stainless steels10.1016/j.corsci.2007.01.008 ↗
5. Effect of hydrogen on tensile behaviour of micrometre-sized specimen fabricated from a metastable austenitic stainless steel10.1016/j.corsci.2010.10.019 ↗
6. Hydrogen uptake in 316L stainless steel: consequenceson the tensile propertis10.1016/j.corsci.2005.11.004 ↗
7. Hydrogen-assisted fatigue crack growth of AISI 316L stainless steel weld10.1016/j.corsci.2008.08.016 ↗
8. Hydrogen-assisted quasi-cleavage fracture in a single cystalline type 316 austenitic stainless steel10.1016/j.corsci.2013.06.018 ↗
9. Stress corrosion cracking susceptibility of thermally-aged Type 310S stainless steels in supercritical water10.1016/j.corsci.2018.01.023 ↗
10. Effect of microstructure on hydrogen embrittlement of various stainless steels10.1016/j.msea.2013.07.004 ↗
11. Effects of dissolved hydrogen and surface condition on the intergranular stress corrosion cracking initiation and short crack growth behavior of non-sensitized 316 stainless steel in simulated PWR primary water10.1016/j.corsci.2017.02.003 ↗
12. On the role of phase transitions in the hydrogen embrittlement of stainless steels10.1016/0036-9748(80)90194-5 ↗
13. Deformation-induced phase transformation and strain hardening in type 304 austenitic stainless steel10.1007/s11661-006-0130-y ↗
14. Strain hardening and transformation mechanism of deformation-induced martensite transformation in metastable austenitic stainless steels10.1016/0921-5093(91)90769-J ↗
15. Effect of deformation-induced martensite transformation on the plastic behaviour of metastable austenitic stainless steel10.2320/matertrans1989.30.33 ↗
16. Deformation twinning in high-nitrogen austenitic stainless steel10.1016/j.actamat.2007.02.023 ↗
17. Twinning and martensite in a 304 austenitic stainless steel10.1016/j.msea.2012.05.080 ↗
18. Hydrogen embrittlement of sensitized SUS 316 steel10.2472/jsms.45.1078 ↗
19. Hydrogen embrittlement of the Ni-base alloy 600 correlated with hydrogen transport by dislocations10.1016/S0921-5093(98)01006-5 ↗
20. The effect of pre-deformation on moisture-induced embrittlement of Ni3Al alloys10.1016/S0966-9795(96)00077-5 ↗
21. Effect of prestraining on hydrogen absorption and delayed fracture behaviour of a medium-carbon TRIP steel
22. Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: effect of plastic pre-strain10.1016/j.ijhydene.2014.04.122 ↗
23. Effects of hydrogen on metal fatigue
24. Influence of machining-induced martensite on hydrogen-assisted fracture of AISI type 304 austenitic stainless steel10.1016/j.ijhydene.2011.05.133 ↗
25. Effects of hydrogen on fatigue crack growth behavior of austenitic stainless steels10.1016/j.ijhydene.2008.02.067 ↗
26. Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures10.1016/S1359-6454(98)00136-0 ↗
27. Comparison of hydrogen gas embrittlement of austenitic and ferritic stainless steels10.1007/BF02646229 ↗
28. Internal reversible hydrogen embrittlement of austenitic stainless steels based on type 316 at low temperatures
29. Influence of macro segregation on hydrogen environment embrittlement of SUS 316L stainless steel10.1016/j.ijhydene.2009.02.015 ↗
30. Influence of hydrogen content on the tensile properties and fracture of austenitic stainless steel welds10.1016/j.ijhydene.2012.11.016 ↗
31. Toughness and hydrogen compatibility of austenitic stainless steel welds at cryogenic temperatures10.1016/j.ijhydene.2007.03.009 ↗
32. Hydrogen-assisted crack propagation in 304L/308L and 21Cr-6Ni-9Mn/308L austenitic stainless steel fusion welds10.1016/j.corsci.2012.03.046 ↗
33. Hydrogen environment embrittlement of orbital welded austenitic stainless steels at -50°C10.1016/j.ijhydene.2009.05.081 ↗
34. Hydrogen diffusion and hydrogen influenced critical stress intensity in an API X70 pipeline steel welded joint-experiments and FE simulations10.1016/j.ijhydene.2012.05.005 ↗
35. Keyhole welding with CF-TIG (cathode focussed GTA)10.1007/s40194-013-0074-y ↗
36. Effect of strain-induced martensite on hydrogen embrittlement of austenitic stainless steels investigated by combined tension and hydrogen release methods10.1016/j.ijhydene.2013.01.198 ↗
37. Effect of grain size on transformation-induced plasticity in an ultrafine-grained metastable austenitic steel10.1016/j.scriptamat.2008.02.024 ↗
38. Kinetics of strain-induced martensite nucleation10.1007/BF02672301 ↗
39. Influence of chemical composition on martensitic transformation in Fe-Cr-Ni stainless steel10.2320/jinstmet1952.34.5_507 ↗
40. Effect of nickel equivalent on hydrogen gas embrittlement of austenitic stainless steels based on type 316 at low temperatures10.1016/j.actamat.2008.03.022 ↗
41. Deformation induced defects in iron revealed by thermal desorption spectroscopy of tritium10.1016/S1359-6462(98)00436-9 ↗
42. Nature of hydrogen trapping sites in steels induced by plastic deformation10.1016/S0925-8388(99)00322-9 ↗
43. Hydrogen effects on tensile property of pure iron with deformed surface10.1016/j.msea.2012.09.075 ↗
44. Fractography of hydrogen-embrittled iron-chromium-nickel alloys
45. Hydrogen-induced equilibrium vacancies in fcc iron-base alloys10.1016/1359-6462(95)00580-3 ↗
46. Effects of hydrogen on dislocation morphology in spheroidized steel, Acta Metall
47. Dieter · 1986
48. Hydrogen transport in solution-treated and pre-strained austenitic stainless steels and its role in hydrogen-enhanced fatigue crack growth10.1016/j.ijhydene.2008.11.018 ↗
49. Effects of deformation on hydrogen permeation in austenitic stainless steels10.1016/0001-6160(86)90123-9 ↗
50. Effect of pre-strain on hydrogen embrittlement of high strength steels10.1016/j.msea.2014.07.085 ↗
51. First-principles study on the grain boundary embrittlement of metals by solute segregation: part II. Metal (Fe, Al, Cu)-hydrogen (H) systems10.1007/s11661-010-0380-6 ↗
52. The effect of pre-strain on hydrogen embrittlement in 310S stainless steel10.1016/j.jallcom.2014.02.038 ↗
53. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation II. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗
54. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
55. Effect of hydrogen on martensite formation in austenitic stainless steels in high-pressure torsion10.1016/j.actamat.2009.03.006 ↗
56. First-principles study on the interaction of H interstitials with grain boundaries in alpha- and gamma-Fe10.1103/PhysRevB.84.144121 ↗
57. Effects of hydrogen on the fracture toughness of a X70 pipeline steel10.1016/j.corsci.2009.07.013 ↗
58. Study of correlation between hydrogen-induced stress and hydrogen embrittlement10.1016/S0921-5093(02)00600-7 ↗