journal article·2024-03Open access

Effect of heat treatment on the microstructure and pitting corrosion behavior of 316L stainless steel fabricated by different additive manufacturing methods (L-PBF versus L-DED): Comparative investigation exploring the role of microstructural features on passivity

Reynier I. Revilla, Guichuan Li, Romain Pion, Kristof Marcoen, Francesco Andreatta, Lorenzo Fedrizzi, Kim Vanmeensel, Iris De Graeve

Corrosion Science· Volume 228

Abstract

This work explores the relation between microstructural features and pitting corrosion resistance of additively manufactured 316 L stainless steel. Specimens fabricated using two different laser-based manufacturing processes (L-PBF and L-DED) were studied in as-built and heat-treated conditions following a comparative approach. Potentiodynamic polarization tests and corrosion morphology analysis served to evaluate their corrosion resistance and passive behavior. This work shows that, contrary to previous reports, the absence of MnS inclusions or presence of the microsegregation structure are not the main factors enhancing passivity of these materials. Instead, dislocation density was the only microstructural feature matching the trend in their passivity behavior.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Hardened austenite steel with columnar sub-grain structure formed by laser melting10.1016/j.msea.2014.12.018 ↗
2. Correlation between process parameters, microstructure and properties of 316L stainless steel processed by selective laser melting10.1016/j.msea.2018.01.103 ↗
3. Intragranular cellular segregation network structure strengthening 316L stainless steel prepared by selective laser melting10.1016/j.jnucmat.2015.12.034 ↗
4. Quantitative multiscale correlative microstructure analysis of additive manufacturing of stainless steel 316L processed by selective laser melting10.1016/j.matchar.2019.110074 ↗
5. On the origin of the high tensile strength and ductility of additively manufactured 316L stainless steel: multiscale investigation10.1016/j.jmst.2019.09.017 ↗
6. An investigation on the effect of powder recycling on the microstructure and mechanical properties of AISI 316L produced by Directed Energy Deposition10.1016/j.msea.2019.138360 ↗
7. Microstructure evolution of 316L produced by HP-SLM (high power selective laser melting)
8. Effect of heat treatment on microstructure and mechanical properties of 316L steel synthesized by selective laser melting10.1016/j.msea.2019.01.110 ↗
9. Dislocation network in additive manufactured steel breaks strength-ductility trade-off10.1016/j.mattod.2017.11.004 ↗
10. Corrosion behaviour of 316L stainless steel manufactured by selective laser melting
11. Additively manufactured 316L stainless steel with improved corrosion resistance and biological response for biomedical applications
12. EIS comparative study and critical Equivalent Electrical Circuit (EEC) analysis of the native oxide layer of additive manufactured and wrought 316L stainless steel10.1016/j.corsci.2020.108480 ↗
13. Microstructure and corrosion behavior of 316L stainless steel prepared using different additive manufacturing methods: a comparative study bringing insights into the impact of microstructure on their passivity10.1016/j.corsci.2020.108914 ↗
14. In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing10.1016/j.matdes.2017.09.044 ↗
15. Melt pool temperature and cooling rates in laser powder bed fusion
16. Real-time detection of cooling rate using pyrometers in tandem in laser material processing and directed energy deposition10.1016/j.matlet.2020.128330 ↗
17. In situ measurements of melt-pool length and cooling rate during 3D builds of the metal AM-bench artifacts10.1007/s40192-020-00170-8 ↗
18. Laser metal deposition as repair technology for 316L stainless steel: influence of feeding powder compositions on microstructure and mechanical properties10.1016/j.optlastec.2018.07.051 ↗
19. Application of directed energy deposition-based additive manufacturing in repair10.3390/app9163316 ↗
20. Corrosion behavior of additively manufactured 316L stainless steel in acidic media10.1016/j.mtla.2018.06.015 ↗
21. The enhancement of microstructure on the passive and pitting behaviors of selective laser melting 316L SS in simulated body fluid10.1016/j.apsusc.2018.10.150 ↗
22. The passivity of selective laser melted 316L stainless steel10.1016/j.apsusc.2019.144495 ↗
23. Pitting corrosion in 316L stainless steel fabricated by laser powder bed fusion additive manufacturing: a review and perspective10.1007/s11837-022-05206-2 ↗
24. The microstructure, mechanical properties and corrosion resistance of 316L stainless steel fabricated using laser engineered net shaping10.1016/j.msea.2016.09.028 ↗
25. Studies on pitting corrosion and sensitization in laser rapid manufactured specimens of type 316L stainless steel10.1016/j.matdes.2012.03.011 ↗
26. Mechanical and electro-chemical properties of multiple-layer diode laser cladding of 316L stainless steel10.1016/j.apsusc.2005.01.131 ↗
27. Interstitial elements created via metal 3D printing10.1016/j.mattod.2023.04.020 ↗
28. Transformation of austenite to duplex austenite-ferrite assembly in annealed stainless steel 316L consolidated by laser melting10.1016/j.jallcom.2015.01.249 ↗
29. Microstructure and corrosion resistance of laser additively manufactured 316L stainless steel
30. About metastable cellular structure in additively manufactured austenitic stainless steels
31. Effect of real-time cooling rate on microstructure in Laser Additive Manufacturing10.1016/j.jmatprotec.2016.01.017 ↗
32. On the enhanced corrosion resistance of a selective laser melted austenitic stainless steel10.1016/j.scriptamat.2017.07.037 ↗
33. On the corrosion and metastable pitting characteristics of 316L stainless steel produced by selective laser melting10.1149/2.0551706jes ↗
34. Critical features in the microstructural analysis of AISI 316L produced by metal additive manufacturing10.1007/s13632-019-00604-6 ↗
35. Microstructure and mechanical properties of AISI 316L produced by directed energy deposition-based additive manufacturing: a review10.3390/app10093310 ↗
36. Microstructural features, defects, and corrosion behaviour of 316L stainless steel clads deposited on wrought material by powder- and laser-based direct energy deposition with relevance to repair applications10.3390/ma15207181 ↗
37. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
38. Heat treatment effect on the microstructure and corrosion behavior of 316L stainless steel fabricated by selective laser melting for proton exchange membrane fuel cells10.1016/j.electacta.2018.04.188 ↗
39. Mechanical properties and corrosion behavior of selective laser melted 316L stainless steel after different heat treatment processes10.1016/j.jmst.2019.03.003 ↗
40. Enhanced corrosion resistance of additively manufactured 316L stainless steel after heat treatment10.1149/1945-7111/abc10e ↗
41. Pitting corrosion of type 316L stainless steel elaborated by the selective laser melting method: influence of microstructure10.1007/s11665-021-05621-7 ↗
42. Effect of heat treatment on microstructure, mechanical and corrosion properties of austenitic stainless steel 316L using arc additive manufacturing10.1016/j.msea.2017.10.002 ↗
43. Unanticipated drastic decline in pitting corrosion resistance of additively manufactured 316L stainless steel after high-temperature post-processing10.1016/j.corsci.2019.108412 ↗
44. Electrochemical studies on the effect of residual stress on the corrosion of 316L manufactured by selective laser melting10.1016/j.corsci.2019.108314 ↗
45. Effect of thermal treatment on corrosion behavior of AISI 316L stainless steel manufactured by laser powder bed fusion10.3390/ma15196768 ↗
46. Effect of heat-treatment on the microstructure, mechanical properties and corrosion behaviour of SS 316 structures built by laser directed energy based additive manufacturing10.1007/s12540-020-00838-y ↗
47. Enhanced pitting resistance of directed energy deposition 316L stainless steel by post-manufacturing heat treatment
48. Corrosion challenges towards a sustainable society10.1002/maco.202213140 ↗
49. Characterization of nano-scale oxides in austenitic stainless steel processed by powder bed fusion10.1016/j.scriptamat.2018.06.011 ↗
50. On the effect of build orientation and residual stress on the corrosion of 316L stainless steel prepared by selective laser melting10.1016/j.corsci.2020.109149 ↗
51. MiCLAD as a platform for real-time monitoring and machine learning in laser metal deposition10.1016/j.procir.2020.09.164 ↗
52. Recrystallization-based grain boundary engineering of 316L stainless steel produced via selective laser melting10.1016/j.actamat.2020.09.015 ↗
53. The effect of post-processing heat treatment on the microstructure, residual stress and mechanical properties of selective laser melted 316L stainless steel10.1016/j.msea.2021.141611 ↗
54. Effect of powder recycling on inclusion content and distribution in ASI 316L produced by L-PBF technique10.1016/j.jmrt.2023.02.017 ↗
55. Why stainless steel corrodes10.1038/415770a ↗
56. Intragranular irradiation-assisted stress corrosion cracking (IASCC) of 316L stainless steel made by laser direct energy deposition additive manufacturing: delta ferrite-dislocation channel interaction10.1016/j.jnucmat.2023.154305 ↗
57. Microstructural studies of direct-laser-deposited stainless steel 316L-Si on 316L base material10.1007/s42452-020-03530-3 ↗
58. Thermal stability and microstructural evolution of additively manufactured 316L stainless steel by laser powder bed fusion at 500–800 °C
59. 1978
60. Origin of dislocation structure in an additively manufactured austenitic stainless steel 316L10.1016/j.actamat.2020.07.063 ↗
61. On the unusual intergranular corrosion resistance of 316L stainless steel additively manufactured by selective laser melting10.1016/j.corsci.2019.108189 ↗
62. The effect of sub-grain structure on intergranular corrosion of 316L stainless steel fabricated via selective laser melting10.1016/j.matlet.2019.02.047 ↗
63. Atom-probe tomography characterization of the oxidation of stainless steel10.1016/j.scriptamat.2010.02.021 ↗
64. Corrosion mechanism of additively manufactured 316L stainless steel in 3.5 wt% NaCl solution