Effect of hydrogen charging time on hydrogen blister and hydrogen-induced cracking of pure iron

Xinfeng Li, Weihong Huang, Xubin Wu, Jin Zhang, Yao Wang, Eiji Akiyama, Dewen Hou

Corrosion Science· Volume 181
Publisher page

Abstract

Abstract Hydrogen blister (HB) and hydrogen-induced cracking (HIC) of pure iron at various charging times were investigated. The results show that an increase in charging time leads to the increased HB height/width and HIC length/depth, and a change in hydrogen damage morphology. Subsurface HIC initiates and propagates along the grain boundaries, which makes the surface bend outwards to form blister on blister features, suggesting grain boundary cracking-induced blister-blister interaction mechanism. Crystallographic analysis demonstrates that adjacent grain boundary oriented-{100}//ND and {110}//ND exhibits the highest susceptibility to HIC, which offers a pathway to design hydrogen-resistant structural steels through the control of grain boundary.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. On some remarkable changes produced in Iron and steel by the action of hydrogen and acids10.1038/011393a0 ↗
2. Effects of Cu addition on resistance to hydrogen embrittlement in 1 GPa-grade duplex lightweight steels10.1016/j.actamat.2020.06.051 ↗
3. Hydrogen trapping and desorption of dual precipitates in tempered low-carbon martensitic steel10.1016/j.actamat.2020.06.046 ↗
4. The combined effects of hydrogen and aging condition on the deformation and fracture behavior of a precipitation-hardened nickel-base superalloy10.1016/j.actamat.2020.01.033 ↗
5. Hydrogen-assisted fatigue crack-propagation in a Ni-based superalloy 718, revealed via crack-path crystallography and deformation microstructures10.1016/j.corsci.2020.108814 ↗
6. A comparative study of microstructure and hydrogen embrittlement of selective laser melted and wrought 17–4 PH stainless steel10.1016/j.msea.2020.139363 ↗
7. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
8. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
9. Hydrogen-induced intergranular failure of iron
10. Hydrogen related failure of steels – a new aspect
11. Review of hydrogen embrittlement in metals: hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention10.1007/s40195-020-01039-7 ↗
12. Synchrotron X-ray Laue diffraction study of hydrogen-induced blisters on iron grain boundaries10.1016/j.scriptamat.2019.05.009 ↗
13. The effects of inclusions and second phase particles on hydrogen-induced blistering in iron10.1016/j.matchemphys.2007.07.004 ↗
14. Investigation of hydrogen concentration and hydrogen damage on API X80 steel surface under cathodic overprotection10.1016/j.ijhydene.2017.10.116 ↗
15. Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel10.1016/j.ijhydene.2010.05.089 ↗
16. Hydrogen induced blister cracking and mechanical failure in X65 pipeline steels10.1016/j.ijhydene.2019.06.098 ↗
17. Understanding the effect of niobium on hydrogen-induced blistering in pipeline steel: a combined experimental and theoretical study10.1016/j.corsci.2019.108142 ↗
18. Effect of deformation and charging conditions on crack and blister formation during electrochemical hydrogen charging10.1016/j.actamat.2017.01.013 ↗
19. Effect of hydrogen charging conditions on hydrogen blisters and pitting susceptibility of 445J1M ferritic stainless steel10.1149/2.0711816jes ↗
20. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
21. Suppression of hydrogen-induced blisters in SK4 carbon steel alloy by friction stir processing10.1007/s10853-013-7246-4 ↗
22. Suppression of hydrogen-induced damage in friction stir welded low carbon steel joints10.1016/j.corsci.2015.01.046 ↗
23. Influence of sulphur content and inclusion distribution on the hydrogen induced blister cracking in pressure vessel and pipeline steels10.1016/S0010-938X(00)00084-6 ↗
24. Effect of environmental and metallurgical factors on hydrogen induced cracking of HSLA steels10.1016/j.corsci.2008.09.030 ↗
25. Degradation of the pipe-steel structure upon long-term operation in contact with a hydrogen sulfide-containing medium10.1134/S0031918X11020128 ↗
26. Effects of alloying elements and microstructure on the susceptibility of the welded HSLA steel to hydrogen-induced cracking and sulfide stress cracking10.1016/j.msea.2008.11.064 ↗
27. Effect of loading mode on blistering in iron submitted to plastic prestrain before hydrogen cathodic charging10.1016/j.ijhydene.2017.02.048 ↗
28. Crack and blister initiation and growth in purified iron due to hydrogen loading10.1016/j.actamat.2016.05.034 ↗
29. Towards suppressing H blistering by investigating the physical origin of the H-He interaction in W10.1088/0029-5515/50/11/115010 ↗
30. Three-dimensional imaging of hydrogen blister in iron with neutron tomography10.1016/j.actamat.2014.06.034 ↗
31. Nucleation mechanism of intra-granular blisters in tungsten exposed to hydrogen plasma10.1016/j.scriptamat.2020.06.024 ↗
32. Influence of sulphur content and inclusion distribution on the hydrogen induced blister cracking in pressure vessel and pipeline steels10.1016/S0010-938X(00)00084-6 ↗
33. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
34. Role of crystallographic texture in hydrogen-induced cracking of low carbon steels for sour service piping10.1007/s11661-007-9130-9 ↗
35. The mechanism of failure by hydrogen induced cracking in an acidic environment for API 5L X70 pipeline steel10.1016/j.ijhydene.2014.11.057 ↗
36. Hydrogen embrittlement controlled by reaction of dislocation with grain boundary in alpha-iron
37. A focus on different factors affecting hydrogen induced cracking in oil and natural gas pipeline steel10.1016/j.engfailanal.2017.05.022 ↗
38. Zapffe · 1941
39. A nucleation mechanism of hydrogen blister in metals and alloys10.1007/s11661-007-9391-3 ↗
40. Dual role of nanosized NbC precipitates in hydrogen embrittlement susceptibility of lath martensitic steel10.1016/j.corsci.2019.108345 ↗
41. The dual role of shot peening in hydrogen-assisted cracking of PSB1080 high strength steel10.1016/j.matdes.2016.07.121 ↗
42. Y. Li, Research on flake’s generation mechanism by macro-meso cross scale methods in heavy forgings, Dissertation, Yanshan University.
43. Friction stir modification of GTA 7075-T6 Al alloy weld joints: EBSD study and microstructural evolutions10.1016/j.acme.2017.01.002 ↗
44. Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking10.1016/j.msea.2014.10.009 ↗
45. The structure of high-angle grain boundaries10.1016/0001-6160(66)90168-4 ↗
46. The effect of lattice defects induced by cathodic hydrogen charging on the apparent diffusivity of hydrogen in pure iron10.1007/BF01133343 ↗
47. Effect of microstructures and inclusions on hydrogen-induced cracking and blistering of A537 steel10.1016/j.msea.2015.06.085 ↗
48. Hydrogen-induced cracking and healing behaviour of X70 steel10.1016/j.jallcom.2009.05.085 ↗
49. A study of hydrogen blistering mechanism for Molybdenum by Tritium radio-luminography10.1016/j.jnucmat.2009.01.275 ↗
50. Vacancy trapping mechanism for hydrogen bubble formation in metal10.1103/PhysRevB.79.172103 ↗
51. Predictive model of hydrogen trapping and bubbling in nanovoids in bcc metals10.1038/s41563-019-0422-4 ↗
52. Review of hydrogen embrittlement in metals: hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention10.1007/s40195-020-01039-7 ↗
53. A decohesion model of hydrogen assisted cracking10.1016/0013-7944(88)90107-5 ↗
54. A comparative study of hydrogen embrittlement of 20SiMn2CrNiMo, PSB1080 and PH13-8Mo high strength steels10.1016/j.msea.2018.03.076 ↗
55. Role of lattice strain and texture in hydrogen embrittlement of 18Ni (300) maraging steel10.1016/j.ijhydene.2017.03.209 ↗
56. Texture and grain boundary study in high strength Fe–18Ni–Co steel related to hydrogen embrittlement10.1016/j.matdes.2015.11.093 ↗
57. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
58. Microstructural and crystallographic features of hydrogen-related fracture in lath martensitic steels10.1080/02670836.2017.1312210 ↗
59. The effect of hydrogen on the evolution of intergranular cracking: a cross-scale study using first-principles and cohesive finite element methods10.1039/C5RA26061B ↗
60. EBSD characterization of hydrogen induced blisters and internal cracks in TRIP-assisted steel
61. T.D. Silva Botelho, Effect of loading mode on blistering in iron submitted to plastic prestrain before hydrogen cathodic charging10.1016/j.ijhydene.2017.02.048 ↗
62. In situ study of the initiation of hydrogen bubbles at the aluminium metal/oxide interface10.1038/nmat4336 ↗
63. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗